journal article·2001-07

Current luting cements: marginal gap formation of composite inlay and their mechanical properties

M. Irie, K. Suzuki

Dental Materials· Volume 17· Issue 4
Publisher page

Abstract

Objective The aims of this investigation were to investigate the effect of thermocycling on the marginal gap formation of composite inlays using three types of luting cements (Compolute, PermaCem, Fuji Plus, Panavia 21: as a control) and on mechanical properties of four luting cements. Methods The maximum marginal gap in the dentin cavity of each of ten resin inlay specimens in each group, was measured by a microscope before and after 10,000 thermocycles. The dimensional change, shear bond strength to dentin, and material and conditions for flexural strength and modulus testing were examined. Results Compolute and Panavia 21 showed marginal gaps of approximately 10 microm before thermocycling. In contrast, the gap widths after thermocycling was significantly wider. Although the gap widths of PermaCem and Fuji Plus were approximately 60-110 microm prior to thermocycling, they were significantly smaller in width after thermocycling. Statistical differences in the shear bond strength to dentin were not observed before or after thermocycling for all materials. The flexural strength and modulus were significantly increased after thermocycling compared with three products and with all four products, respectively. Significance The mechanical properties of all four luting cements were closely related to their marginal gap formations and these mechanical factors have important roles in determining their marginal gap formations.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Clinical evaluation of a heat-treated resin composite inlay: 3-year results
2. Scanning electron microscopic and clinical examination of composite resin inlays/onlays up to 12 months in situ
3. Direct and indirect evaluation of posterior composite restorations at three years10.1016/0109-5641(92)90055-H ↗
4. Clinical and semiquantitative marginal analysis of four tooth-coloured inlay systems at 3 years10.1016/0300-5712(95)98768-X ↗
5. Marginal breakdown of 5-year-old direct composite inlays10.1016/0300-5712(95)00098-4 ↗
6. One-year clinical evaluation of composite and ceramic inlays in posterior teeth10.1016/S0022-3913(98)70004-6 ↗
7. Wear and marginal adaptation of composite resin inlays10.1016/0022-3913(94)90335-2 ↗
8. The competition between the composite-dentin bond strength and the polymerization contraction stress10.1177/00220345840630121101 ↗
9. Setting stress in composite resin in relation to configuration of the restoration10.1177/00220345870660110601 ↗
10. Curing contraction of composites and glass-ionomer cements10.1016/0022-3913(88)90176-X ↗
11. Setting stresses in composites for two different curing modes10.1016/0109-5641(93)90095-8 ↗
12. Marginal gap formation of light-activated base/liner materials: effect of setting shrinkage and bond strength10.1016/S0109-5641(99)00064-0 ↗
13. Water storage effect on the marginal seal of resin-modified glass-ionomer restorations
14. Destructive stresses in adhesive luting cements10.1177/00220345910700050301 ↗
15. Dentin bond strength and marginal adaptation: direct composite resins vs ceramic inlays
16. Relative gap formation of resin-cemented ceramic inlays and dentin bonding agents10.1016/S0022-3913(96)90541-7 ↗
17. Relative gap formation adjacent to ceramic inlays with combinations of resin cements and dentin bonding agents10.1016/S0022-3913(96)90003-7 ↗
18. The initial gap around large composite restorations in vitro: the effect of etching enamel walls10.1177/00220345840630051501 ↗
19. Bonding to enamel and dentin: a brief history and state of the art
20. Fluid exchange at the margins of dental restoratios10.1016/S0002-8177(52)43006-8 ↗
21. Marginal seal of resin-modified glass-ionomers and compomers: effect of polishing after one-day storage
22. Flexural properties and swelling after storage in water of polyacid-modified composite resin (Compomer)10.4012/dmj.17.77 ↗
23. In vitro study of fracture incidence and compressive fracture load of all-ceramic crowns cemented with resin-modified glass ionomer and other luting agents10.1016/S0022-3913(98)70058-7 ↗
24. Early strength of glass ionomer cements10.1016/0109-5641(93)90107-2 ↗
25. Mechanical properties of dental luting cements10.1016/S0022-3913(99)70216-7 ↗
26. Dentin-polymer bond promoted by Gluma and various resins10.1177/00220345850640121801 ↗
27. Rank transformations as a bridge between parametric and nonparametric statistics10.2307/2683975 ↗
28. Craig RG, ed. Restorative dental materials, 10th edn, St. Louis, Mosby-Year Book, 1997. p. 56-103.
29. Dental luting agents: a review of the current literature10.1016/S0022-3913(98)70128-3 ↗
30. Dimensional changes of resin/ionomer restoratives in aqueous and neutral media10.1016/S0109-5641(99)00098-6 ↗
31. The influence of water sorption on the development of setting shrinkage stress in traditional and resin-modified glass ionomer cement10.1016/0109-5641(95)80016-6 ↗
32. Current status of luting agents for fixed prosthodontics10.1016/S0022-3913(99)70240-4 ↗
33. Resin-modified glass-ionomer cement