Slow cooling protocol improves fatigue life of zirconia crowns
Source abstract
Abstract
Objective To compare the fatigue life and damage modes of zirconia crowns fabricated with and without framework design modification when porcelain veneered using a fast or slow cooling protocol. Methods Composite resin replicas of a first molar full crown preparation were fabricated. Zirconia copings were milled as conventional (0.5mm even thickness, Zr-C, n=20,) or modified (lingual margin of 1.0mm thickness, 2.0mm height connected to two proximal struts of 3.5mm height, Zr-M, n=20). These groups were subdivided (n=10 each) according to the veneer cooling protocol employed: fast cooling (Zr-CFast and Zr-MFast) and slow cooling (Zr-CSlow and Zr-MSlow). Crowns were cemented and fatigued for 10(6) cycles in water. The number of cycles to failure was recorded and used to determine the interval databased 2-parameter probability Weibull distribution parameter Beta (β) and characteristic life value Eta (η). Results 2-parameter Weibull calculation presented β=5.53 and β=4.38 for Zr-MFast and Zr-CFast, respectively. Slow cooled crowns did not fail by completion of 10(6) cycles, thereby Weibayes calculation was applied. Increased fatigue life was observed for slow cooled crowns compared to fast cooled ones. Groups Zr-MFast and Zr-MSlow presented no statistical difference. Porcelain cohesive fractures were mainly observed in fast cooled groups. Slow cooled crowns presented in some instances inner cone cracks not reaching the zirconia/veneer interface. Significance Improved fatigue life in tandem with the absence of porcelain fractures were observed in slow cooled crowns, regardless of framework design. Crowns fast cooled chiefly failed by porcelain cohesive fractures.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Erosion and Treatment
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Thermal/mechanical simulation and laboratory fatigue testing of an alternative yttria tetragonal zirconia polycrystal core-veneer all-ceramic layered crown design10.1111/j.1600-0722.2010.00724.x ↗
2. Fatigue testing of two porcelain-zirconia all-ceramic crown systems10.1016/j.dental.2009.03.009 ↗
3. Fatigue life and failure modes of crowns systems with a modified framework design10.1016/j.jdent.2010.04.011 ↗
4. Modified Y-TZP core design improves all-ceramic crown reliability10.1177/0022034510384617 ↗
5. Reliability of metalloceramic and zirconia-based ceramic crowns10.1177/0022034510375826 ↗
6. Clinical trials in zirconia: a systematic review
7. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures
8. From porcelain-fused-to-metal to zirconia: clinical and experimental considerations10.1016/j.dental.2010.10.024 ↗
9. Influence of thickness and cooling rate on development of spontaneous cracks in porcelain/zirconia structures10.1111/j.1834-7819.2010.01239.x ↗
10. Effect of firing protocols on cohesive failure of all-ceramic crowns10.1016/j.jdent.2010.08.014 ↗
11. Transient and residual stress in a porcelain-metal strip10.1177/00220345900690020901 ↗
12. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures10.1016/j.actbio.2008.12.016 ↗
13. Effect of framework design on crown failure10.1111/j.1600-0722.2008.00608.x ↗
14. Customization of milled zirconia copings for all-ceramic crowns: a clinical report10.1016/S0022-3913(08)00028-0 ↗
15. Clinical behavior of zirconia-based fixed partial dentures made of DC-Zirkon: 3-year results
16. Pressed ceramics onto zirconia, Part 2: Indentation fracture and influence of cooling rate on residual stresses10.1016/j.dental.2011.08.003 ↗
17. Influence of cooling rate on zirconia/veneer interfacial adhesion10.1016/j.actbio.2010.06.026 ↗
18. Effect of thermal misfit between different veneering ceramics and zirconia frameworks on in vitro fracture load of single crowns10.4012/dmj.26.766 ↗
19. Glass transition temperatures of dental porcelain10.1177/00220345810600061601 ↗
20. Residual stresses in porcelain-veneered zirconia prostheses10.1016/j.dental.2012.04.019 ↗
21. O’Brien · 2008
22. Strength, fracture toughness and microstructure of a selection of all-ceramic materials, Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
23. Thermal gradients and residual stresses in veneered Y-TZP frameworks10.1016/j.dental.2011.08.001 ↗
24. Effect of cooling rate on shear bond strength of veneering porcelain to a zirconia ceramic material10.2334/josnusd.52.647 ↗
25. The use of slow heating and slow cooling regimens to strengthen porcelain fused to zirconia10.1016/S0022-3913(12)60050-X ↗
26. Influence of cooling rate on residual stress profile in veneering ceramic: measurement by hole-drilling10.1016/j.dental.2011.05.005 ↗
27. Ivoclar · 2009
28. Ivoclar · 2010
29. Effect of core design and veneering technique on damage and reliability of Y-TZP-supported crowns10.1016/j.dental.2012.11.012 ↗
30. Fractographic ceramic failure analysis using the replica technique10.1016/j.dental.2006.12.002 ↗
31. Preparation an the design of metal substructures
32. Five-year clinical prospective evaluation of zirconia-based Denzir 3-unit FPDs
33. Clinical performance of extended zirconia frameworks for fixed dental prostheses: two-year results10.1111/j.1365-2842.2009.01969.x ↗
34. Modeling of water absorption induced cracks in resin-based composite supported ceramic layer structures10.1002/jbm.b.30852 ↗
35. Okeson · 2012 · 58
36. Abernethy · 2007
37. Weibayes testing: what is the impact if assumed beta is incorrect?
38. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
39. Effect of veneering techniques on damage and reliability of Y-TZP trilayers
40. Can material properties predict survival of all-ceramic posterior crowns?
41. XRD2 micro-diffraction analysis of the interface between Y-TZP and veneering porcelain: role of application methods10.1016/j.dental.2010.02.002 ↗
42. SEM observations of porcelain Y-TZP interface10.1016/j.dental.2009.01.006 ↗
43. Clinical risk factors related to failures with zirconia-based restorations: an up to 9-year retrospective study10.1016/j.jdent.2013.10.009 ↗
44. Thermal-induced residual stresses affect the lifetime of zirconia-veneer crowns10.1016/j.dental.2012.11.015 ↗
45. Laboratory simulation of Y-TZP all-ceramic crown clinical failures10.1177/0022034509333968 ↗
46. Residual stress measurement in veneering ceramic by hole-drilling10.1016/j.dental.2010.12.002 ↗
47. Quinn · 2007
48. Damage maps for layered ceramics under simulated mastication10.1177/154405910808700706 ↗
49. Near-surface damage-a persistent problem in crowns obtained by computer-aided design and manufacturing10.1243/095441105X9363 ↗
50. Engineering long term clinical success of advanced ceramic prostheses10.1007/s10856-006-0661-1 ↗
51. Stress fatigue: basic principles and prosthodontic implications
52. Role of indenter material and size in veneer failure of brittle layer structures10.1002/jbm.b.30728 ↗
53. Chipping resistance of graded zirconia ceramics for dental crowns10.1177/0022034511434356 ↗
54. A rationale for a simplified occlusal design in restorative dentistry: historical review and clinical guidelines10.1016/S0022-3913(05)80159-3 ↗
55. Nature of contacts in centric occlusion in 32 adults10.1177/00220345710500013201 ↗