A critical evaluation of bond strength tests for the assessment of bonding to Y-TZP
Source abstract
Abstract
Objectives To compare three different designs for measuring the bond strength between Y-TZP ceramic and a composite material, before and after ceramic surface treatment, evaluating the influence of the size of the adhesive interface for each design. Methods 'Macro' tensile, microtensile, 'macro' shear, microshear, 'macro' push-out, and micropush-out tests were carried out. Two Y-TZP surface treatments were evaluated: silanization (sil) and tribochemical silica coating (30μm silica-modified Al2O3 particles+silanization) (TBS). Failure mode analysis of tested samples was also performed. Results Both the surface treatment and the size of the bonded interface significantly affected the results (p=0.00). Regardless of the type of surface treatment, the microtensile and microshear tests had higher values than their equivalent "macro" tests. However, the push-out test showed the highest values for the "macro" test. The tensile tests showed the greatest variability in results. The tribochemical silica coating method significantly increased bond strength for all tests. Significance Different test designs can change the outcome for Y-TZP/cement interfaces, in terms of mean values and reliability (variability). The 'micro' tests expressed higher bond strengths than their equivalent 'macro' tests, with the exception of the push-out test (macro>micro).
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
2. Effect of fatigue on fracture toughness and phase transformation of Y-TZP ceramics by X-ray diffraction and Raman spectroscopy10.1002/jbm.b.31964 ↗
3. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
4. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
5. Mechanical properties of alumina–zirconia composites for ceramic abutments10.1590/S1516-14392004000400021 ↗
6. Comparison of resin cement adhesion to Y-TZP ceramic following manufacturer's instructions of the cements only10.1007/s00784-007-0151-y ↗
7. Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging10.4012/dmj.27.99 ↗
8. Variables related to materials and preparing for bond strength testing irrespective of the test protocol10.1016/j.dental.2009.11.154 ↗
9. Effect of silica coating combined to a MDP-based primer on the resin bond to Y-TZP ceramic
10. Adhesive quality of self-adhesive and conventional adhesive resin cement to Y-TZP ceramic before and after long-term storage and thermal cycling10.2341/10-157-L ↗
11. Evaluation of resin adhesion to zirconia ceramic using some organosilanes10.1016/j.dental.2005.11.035 ↗
12. Early bond strength of two resin cements to Y-TZP ceramic using MPS or MPS/4-META silanes10.1007/s10266-010-0144-1 ↗
13. A critique of bond strength measurements10.1016/0300-5712(89)90131-0 ↗
14. Three-dimensional finite element analysis of the shear bond test10.1016/0109-5641(95)80047-6 ↗
15. Do dentin bond strength tests serve a useful purpose?
16. Clinical relevance of tests on bond strength, microleakage and marginal adaptation10.1016/j.dental.2012.07.158 ↗
17. Relationship between bond-strength tests and clinical outcomes10.1016/j.dental.2009.11.148 ↗
18. Bond strength – what does it mean?
19. Effect of cross-sectional area on resin-enamel tensile bond strength10.1016/S0109-5641(97)80098-X ↗
20. Regional measurement of resin-dentin bonding as an array10.1177/00220345990780021001 ↗
21. Adhesion to tooth structure: a critical review of “micro” bond strength test methods10.1016/j.dental.2009.11.155 ↗
22. Adhesion to tooth structure: a critical review of “macro” test methods10.1016/j.dental.2009.11.150 ↗
23. Adhesion testing of dentin bonding agents: a review10.1016/0109-5641(95)80046-8 ↗
24. Why do shear bond tests pull out dentin?10.1177/00220345970760061001 ↗
25. Relationship between surface area for adhesion and tensile bond strength – evaluation of a micro-tensile bond test10.1016/0109-5641(94)90067-1 ↗
26. Effect of cross-sectional surface area on bond strengths between resin and dentin10.1016/S0109-5641(98)00018-9 ↗
27. Microtensile testing of dentin adhesives10.1016/S0109-5641(98)00030-X ↗
28. A microshear test to measure bond strengths of dentin–polymer interfaces10.1016/S0142-9612(02)00089-3 ↗
29. Does the bonded cross-sectional surface area affect the microtensile bond strength of resin cement to glass-ceramic?
30. Direct comparison of the bond strength results of the different test methods: a critical literature review10.1016/j.dental.2009.12.002 ↗
31. The phenomena of rupture and flow in solids
32. Analysis of interfacial behavior in MMCs and IMCs by the use of thin-slice push-out tests10.1016/0266-3538(95)00040-2 ↗
33. Effect of mechanical cycling on the push-out bond strength of fiber posts adhesively bonded to human root dentin10.2341/06-165 ↗
34. The disk-specimen height does not influence the push-out bond strength results between fiber post and root dentin10.1080/00218464.2012.655174 ↗
35. Fiber post cementation strategies: effect of mechanical cycling on push-out bond strength and cement polymerization stress evaluation
36. Shear vs. tensile bond strength of resin composite bonded to ceramic10.1177/00220345950740091401 ↗
37. The adhesion between fiber posts and root canal walls: comparison between microtensile and push-out bond strength measurements10.1111/j.1600-0722.2004.00146.x ↗
38. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
39. Strength and reliability of treated Y-TZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
40. Mechanical strength and subcritical crack growth under wet cyclic loading of glass-infiltrated dental ceramics10.1016/j.dental.2010.01.007 ↗
41. The effect of local interfacial geometry on the measurement of the tensile bond strength to dentin10.1177/00220345910700050501 ↗
42. Association of different primers and resin cements for adhesive bonding to zirconia ceramics
43. Comparison of shear test methods for evaluating the bond strength of resin cement to zirconia ceramic10.3109/00016357.2014.903516 ↗
44. Simulation of fiber debonding with friction in a model composite push-out test10.1016/S0020-7683(01)00085-3 ↗
45. A finite element analysis of the push-out test. Influence of test conditions10.1002/jbm.820260111 ↗
46. Interfacial mechanics of push-out tests: theory and experiments
47. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
48. Bond strength of luting cements to zirconium oxide ceramics
49. Influence of surface conditioning and cleaning methods on resin bonding to zirconia ceramic10.1016/j.dental.2010.10.004 ↗
50. Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning10.1016/j.dental.2005.04.021 ↗
51. Bond strength of a resin cement to high-alumina and zirconia-reinforced ceramics: the effect of surface conditioning
52. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic10.1016/j.jdent.2005.06.006 ↗
53. Interfacial characteristics of adhesive luting resins and composites with dentine10.1016/j.dental.2006.06.023 ↗