Residual compressive surface stress increases the bending strength of dental zirconia
Source abstract
Abstract
Objective To assess the influence of surface treatment and thermal annealing on the four-point bending strength of two ground dental zirconia grades. Methods Fully-sintered zirconia specimens (4.0×3.0×45.0mm3) of Y-TZP zirconia (LAVA Plus, 3M ESPE) and Y-TZP/Al2O3 zirconia (ZirTough, Kuraray Noritake) were subjected to four surface treatments: (1) 'GROUND': all surfaces were ground with a diamond-coated grinding wheel on a grinding machine; (2) 'GROUND+HEAT': (1) followed by annealing at 1100°C for 30min; (3) 'GROUND+Al2O3 SANDBLASTED': (1) followed by sandblasting using Al2O3; (4) 'GROUND+CoJet SANDBLASTED': (1) followed by tribochemical silica (CoJet) sandblasting. Micro-Raman spectroscopy was used to assess the zirconia-phase composition and potentially induced residual stress. The four-point bending strength was measured using a universal material-testing machine. Results Weibull analysis revealed a substantially higher Weibull modulus and slightly higher characteristic strength for ZirTough (Kuraray Noritake) than for LAVA Plus (3M ESPE). For both zirconia grades, the 'GROUND' zirconia had the lowest Weibull modulus in combination with a high characteristic strength. Sandblasting hardly changed the bending strength but substantially increased the Weibull modulus of the ground zirconia, whereas a thermal treatment increased the Weibull modulus of both zirconia grades but resulted in a significantly lower bending strength. Micro-Raman analysis revealed a higher residual compressive surface stress that correlated with an increased bending strength. Significance Residual compressive surface stress increased the bending strength of dental zirconia. Thermal annealing substantially reduced the bending strength but increased the consistency (reliability) of 'GROUND' zirconia.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Building materials and conservation · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Ageing of dental zirconia ceramics10.1016/j.jeurceramsoc.2012.02.024 ↗
2. Current status of zirconia restoration10.1016/j.jpor.2013.09.001 ↗
3. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
4. Meta-analysis of bonding effectiveness to zirconia ceramics10.1177/0022034514524228 ↗
5. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?10.1016/j.dental.2010.10.022 ↗
6. Effect of sandblasting and heat treatment on biaxial flexure strength of the zirconia/alumina nanocomposite10.4028/www.scientific.net/KEM.330-332.353 ↗
7. Biaxial flexure strength and low temperature degradation of Ce-TZP/Al2O3 nanocomposite and Y-TZP as dental restoratives10.1002/jbm.b.31131 ↗
8. Effect of sintering condition, sandblasting and heat treatment on biaxial flexure strength of zirconia
9. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
10. Effect of abrasive grinding on the strength of Y-TZP10.1016/j.jeurceramsoc.2009.02.011 ↗
11. Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of Y-TZP ceramics10.1002/jbm.b.31477 ↗
12. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
13. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics10.1016/j.prosdent.2006.08.004 ↗
14. Effect of grinding, sandblasting and heat treatment on the phase transformation of zirconia surface10.4028/www.scientific.net/KEM.330-332.1263 ↗
15. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
16. Post-hot isostatic pressing: a healing treatment for process related defects and laboratory grinding damage of dental zirconia?10.1016/j.dental.2013.04.014 ↗
17. Air-particle abrasion on zirconia ceramic using different protocols: effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography10.1016/j.jmbbm.2013.04.018 ↗
18. Influence of different surface treatments on computer-aided design and manufacturing (CAD-CAM) zirconia frameworks
19. Raman spectroscopic analysis of phase-transformation and stress patterns in zirconia hip joints10.1117/1.1647547 ↗
20. Quantitative analysis of monoclinic phase in 3Y-TZP by Raman spectroscopy10.1111/j.1551-2916.2010.03635.x ↗
21. Fityk: a general-purpose peak fitting program10.1107/S0021889810030499 ↗
22. Monte Carlo pivotal confidence bounds for Weibull analysis, with implementations in R
23. Effect of sandblasting on the mechanical properties of Y-TZP zirconia
24. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment10.4012/dmj.27.408 ↗
25. Raman piezo-spectroscopic analysis of natural and synthetic biomaterials10.1007/s00216-004-2780-1 ↗
26. Raman spectroscopy evaluation of subsurface hydrothermal degradation of zirconia10.1111/j.1551-2916.2012.05237.x ↗
27. Is Weibull distribution the most appropriate statistical strength distribution for brittle materials?10.1016/j.ceramint.2007.10.003 ↗
28. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
29. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
30. Strength and reliability of surface treated Y-TZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
31. Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30μm silica-coated alumina particles10.1016/j.dental.2010.10.003 ↗
32. Phase transformation and subsurface damage in 3Y-TZP after sandblasting10.1016/j.dental.2013.03.005 ↗
33. Microstructural changes in ground 3Y-TZP and their effect on mechanical properties10.1016/j.actamat.2011.07.024 ↗
34. Mechanical property and microstructure of TZP and TZP/Al2O3 composites
35. Strength and fracture-toughness of isostatically hot-pressed composites of Al2O3 and Y2O3-partially-stabilized ZrO2