Sealing performance of resin cements before and after thermal cycling: Evaluation by optical coherence tomography
Source abstract
Abstract
Objectives Self-adhesive resin cements have been recently introduced; however, there is little data available on their long-term performance. In this in vitro study, swept-source optical coherence tomography (OCT) at 1310 nm center wavelength was used for monitoring adaptation of indirect resin restorations after thermal cycling. Methods Resin inlays were luted to class-I cavities of extracted human teeth using three resin cements; Clearfil SA Luting (SA; Kuraray), Bistite II DC or Multibond II (Tokuyama Dental). Each cement was applied with or without pre-coating of dentin by a self-etch adhesive (Clearfil SE Bond) and a low-viscosity microfilled resin. OCT imaging was performed after 24 h, after 2000 and after 10,000 thermocycles (n=5). Selected samples were sectioned for interfacial observation by confocal laser scanning microscope (CLSM). Floor adaptation (percentage) was analyzed by software on 20 B-scans throughout each specimen, and subjected to statistical analysis by three-way ANOVA test at a significance level of 0.05. Results Resin cement type, resin coating and thermal aging all significantly affected adaptation (p<0.05). Initially, SA showed the highest adaptation; however, thermal aging significantly affected its sealing. The best results for all the cements were consistently achieved when the resin coating technique was applied where no deterioration of interfacial integrity was observed in the coated groups. CLSM closely confirmed OCT findings in all groups. Significance OCT could be used for monitoring of composite inlays with several interfacial resin layers. The application of a direct bonding agent in the resin-coating technique improved interfacial sealing and durability of all resin cements.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Optical Coherence Tomography Applications · Endodontics and Root Canal Treatments · Dental materials and restorations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Direct composite inlays versus conventional composite restorations: three-year clinical results10.1038/sj.bdj.4808919 ↗
2. Longevity of restorations in posterior teeth and reasons for failure
3. The resin-coating technique. Effect of a single-step bonding system on dentin bond strengths
4. The effects of luting resin bond to dentin on the strength of dentin supported by indirect resin composite10.1016/S0109-5641(01)00032-X ↗
5. Early bonding of resin cements to dentin—effect of bonding environment
6. Sealing ability of dentin coating using adhesive resin systems
7. The effect of a resin coating on the interfacial adaptation of composite inlays
8. Effect of resin coating on dentin bond durability of a resin cement over 1 year
9. Effect of resin-coating technique on dentin tensile bond strengths over 3 years10.1111/j.1708-8240.2002.tb00160.x ↗
10. Microleakage of porcelain veneer restorations bonded to enamel and dentin with a new self-adhesive resin-based dental cement10.1016/j.dental.2006.01.013 ↗
11. Self-adhesive resin cements – chemistry, properties and clinical considerations10.1111/j.1365-2842.2010.02148.x ↗
12. Concurrent evaluation of composite internal adaptation and bond strength in a class-I cavity10.1016/j.jdent.2012.10.003 ↗
13. Nondestructive assessment of current one-step self-etch dental adhesives using optical coherence tomography10.1117/1.JBO.18.7.076020 ↗
14. 3D mapping of polymerization shrinkage using X-ray micro-computed tomography to predict microleakage10.1016/j.dental.2008.07.010 ↗
15. A 3D analysis of mechanically stressed dentin-adhesive-composite interfaces using X-ray micro-CT10.1016/j.biomaterials.2004.02.024 ↗
16. Sadr A, Shimada Y, Mayoral JR, Hariri I, Bakhsh TA, Sumi Y, et al. Swept source optical coherence tomography for quantitative and qualitative assessment of dental composite restorations. Proc. SPIE 2011;7884:78840C.10.1117/12.877351 ↗
17. 3D assessment of void and gap formation in flowable resin composites using optical coherence tomography
18. Non-destructive 3D imaging of composite restorations using optical coherence tomography: marginal adaptation of self-etch adhesives10.1016/j.jdent.2011.01.011 ↗
19. Quality assessment of dental treatments using en-face optical coherence tomography10.1117/1.2992593 ↗
20. Estimation of the enamel and dentin mineral content from the refractive index10.1159/000342416 ↗
21. Non-invasive quantification of resin-dentin interfacial gaps using optical coherence tomography: validation against confocal microscopy10.1016/j.dental.2011.05.003 ↗
22. Effect of hydration on assessment of early enamel lesion using swept-source optical coherence tomography10.1002/jbio.201200012 ↗
23. Validation of swept source optical coherence tomography (SS-OCT) for the diagnosis of smooth surface caries in vitro10.1016/j.jdent.2012.10.007 ↗
24. Noninvasive cross-sectional visualization of enamel cracks by optical coherence tomography in vitro10.1016/j.joen.2012.05.008 ↗
25. Evaluation of enamel dental restoration interface by optical coherence tomography10.1117/1.2141617 ↗
26. Thermal cycling procedures for laboratory testing of dental restorations10.1016/S0300-5712(98)00037-2 ↗
27. In situ gold nanoparticles formation: contrast agent for dental optical coherence tomography10.1117/1.JBO.17.6.066003 ↗
28. Influence of dental resin material composition on cross-polarization-optical coherence tomography imaging10.1117/1.JBO.17.10.106002 ↗
29. Stickiness prior to setting of some light cured resin-composites10.1016/S0109-5641(02)00097-0 ↗
30. Signal degradation by multiple scattering in optical coherence tomography of dense tissue: a Monte Carlo study towards optical clearing of biotissues10.1088/0031-9155/47/13/307 ↗
31. Non-destructive characterization of voids in six flowable composites using swept-source optical coherence tomography10.1016/j.dental.2012.11.004 ↗
32. Efficacy of a resin coating on bond strengths of resin cement to dentin10.1111/j.1708-8240.2003.tb00325.x ↗
33. Microtensile bond strengths of composite cores to pulpal floor dentin with resin coating10.4012/dmj.27.400 ↗
34. Nikaido T, Cho E, Nakajima M, Tashiro H, Toba S, Burrow MF, et al. Tensile bond strengths of resin cements to bovine dentin using resin coating. Am J Dent 2003;16(Spec No):41A–6A.
35. The effect of additional enamel etching and a flowable composite to the interfacial integrity of Class II adhesive composite restorations
36. Hydrolytic stability of self-etch adhesives bonded to dentin10.1177/154405910508401213 ↗
37. Comparative study on adhesive performance of functional monomers10.1177/154405910408300604 ↗
38. Influence of the chemical structure of functional monomers on their adhesive performance10.1177/154405910808700804 ↗
39. Long-term bond between dual-polymerizing cementing agents and human hard dental tissue10.1016/j.dental.2006.01.012 ↗
40. Dentin bonding performance and ability of four MMA-based adhesive resins to prevent demineralization along the hybrid layer
41. Long-term regional bond strength of three MMA-based adhesive resins in simulated vertical root fracture10.4012/dmj.2011-066 ↗
42. Effects of luting agent and thermocycling on bond strengths to root canal dentine10.1111/j.1365-2591.2006.01155.x ↗
43. Long-term evaluation of water sorption and ultimate tensile strength of HEMA-containing/-free one-step self-etch adhesives10.1016/j.jdent.2011.04.008 ↗
44. Increased wall-to-wall curing contraction in thin bonded resin layers10.1177/00220345890680010701 ↗