Machining variability impacts on the strength of a ‘chair-side’ CAD–CAM ceramic
Source abstract
Abstract
Objectives To develop a novel methodology to generate specimens for bi-axial flexure strength (BFS) determination from a 'chair-side' CAD-CAM feldspathic ceramic with surface defect integrals analogous to the clinical state. The hypotheses tested were: BFS and surface roughness (R(a)) are independent of machining variability introduced by the renewal or deterioration of form-grinding tools and that a post-machining annealing cycle would significantly modify BFS. Methods Nominally identical disc-shaped specimens (11 mm diameter, 1.1mm thickness) were machined with identical design and operative parameters from Vita Mark II feldspathic ceramic. Six individual bur sets (Groups A-F) generated 14 specimens each. Three groups were annealed between glass transition and softening temperatures. 3D contact profilometry determined surface roughness before and following annealing and prior to BFS determination. Scanning electron microscopy was undertaken to examine machining tools and perform fractographic analyses of ceramic fracture fragments. Statistical analysis included independent and pairwise analyses of R(a)-values (P<0.05), Weibull analysis of BFS data and Pearsons correlations. Results Mean R(a) differed significantly between groups (P<0.01) but was unaffected by annealing (P = 0.42). Mean BFS was significantly altered by bur-set (P<0.01). Annealing resulted in no significant modification of the Weibull parameters as the 95% confidence intervals overlapped. No significant correlations between machining order and BFS or R(a) were observed (P>0.05). Significance Surface roughness and the nature of strength limiting defects appear to be probabilistic with flaw generation dependent on a random selection of a bur and a random machining sequence. The variability in BFS with machining could account for premature clinical failures.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. The evolution of the CEREC system10.14219/jada.archive.2006.0398 ↗
2. Computer-aided design and manufacturing in dentistry: a review of the state of the art10.1016/0022-3913(87)90285-X ↗
3. Zhang GM, Satish KG, Ko WK. The mechanics of material removal mechanisms in machining ceramics. Technical Report TR 94-22rl. Institute for Systems Research (NIST), Maryland; 1994.
4. Surface integrity in electro-discharge machining, ultrasonic machining, and diamond saw cutting of ceramic composites10.1016/S0272-8842(00)00024-9 ↗
5. Laser machining of structural ceramics—a review10.1016/j.jeurceramsoc.2008.11.010 ↗
6. A review of abrasive jet machining10.1016/0924-0136(93)90005-Q ↗
7. Chemical-assisted ultrasonic machining of glass10.1016/j.jmatprotec.2007.03.017 ↗
8. A fracture mechanics approach to modelling strength degradation in ceramic grinding processes10.1115/1.2901642 ↗
9. Precision machining of advanced ceramics
10. Lawn · 1993
11. Evaluation of subsurface damage in CAD/CAM machined dental ceramics10.1023/A:1008812929476 ↗
12. Kingery · 1976
13. The phenomena of rupture and flow in solids
14. Influence of contraction mismatch and cooling rate on flexural failure of PFM systems10.1177/00220345880670011201 ↗
15. Near-surface damage—a persistent problem in crowns obtained by computer-aided design and manufacturing10.1243/095441105X9363 ↗
16. Marginal and internal fit of Cerec 3 CAD/CAM all-ceramic crowns
17. Marginal and internal fit of all-ceramic crowns fabricated with two different CAD/CAM systems10.4012/dmj.27.422 ↗
18. Machining accuracy of CAD/CAM ceramic crowns fabricated with repeated machining using the same diamond bur10.4012/dmj.24.123 ↗
19. Effect of heat treatment on microcrack healing behavior of a machinable dental ceramic10.1002/(SICI)1097-4636(1999)48:6<791::AID-JBM5>3.0.CO;2-P ↗
20. Symmetrical bending of circular plates
21. Evaluation of mechanical properties of dental ceramic materials in combination with porcelain
22. Fracture statistics of ceramics—Weibull statistics and deviations from Weibull statistics10.1016/j.engfracmech.2006.05.028 ↗
23. Quinn · 2007
24. Effects of surface finish and fatigue testing on the fracture strength of CAD–CAM and pressed-ceramic crowns10.1016/S0022-3913(99)70036-3 ↗
25. Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns10.1016/j.dental.2005.02.007 ↗
26. Fracture strength and fatigue resistance of all-ceramic molar crowns manufactured with CAD/CAM technology10.1111/j.1532-849X.2008.00305.x ↗
27. Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crowns10.1016/j.prosdent.2005.11.014 ↗
28. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
29. Fracture-surface analysis of dental ceramics10.1016/0022-3913(89)90075-9 ↗
30. Occlusal forces during chewing and swallowing as measured by sound transmission10.1016/0022-3913(81)90455-8 ↗
31. The association among occlusal contacts, clenching effort, and bite force distribution in man10.1177/00220345970760061201 ↗
32. Transient and residual stresses induced during the sintering of two dentin ceramics10.1016/j.dental.2010.11.018 ↗
33. The strength characteristics of CEREC
34. Biaxial flexural strength of CAD/CAM ceramics
35. Measurement of the tensile strength of brittle materials10.1088/0508-3443/10/6/307 ↗
36. Clinical performance of chairside CAD/CAM restorations10.14219/jada.archive.2006.0395 ↗
37. Clinical performance of CEREC ceramic inlays: a systematic review10.1016/S0109-5641(99)00014-7 ↗
38. Long-term clinical results of chairside Cerec CAD/CAM inlays and onlays: a case series
39. A 10-year prospective evaluation of CAD/CAM-manufactured (Cerec) ceramic inlays cemented with a chemically cured or dual-cured resin composite
40. Controlled, prospective clinical split-mouth study of cast gold vs. ceramic partial crowns: 5.5 year results
41. Cerec3D endocrowns—two-year clinical examination of CAD/CAM crowns for restoring endodontically treated molars
42. The deformation and strength of a dental ceramic following resin-cement coating10.1016/j.jdent.2010.10.015 ↗
43. Influence of annealing temperature on the strength of dental glass ceramic materials10.1016/j.dental.2004.09.004 ↗