journal article·2008-08

Influence of leucite content on slow crack growth of dental porcelains

Paulo F. Cesar, Fabiana N. Soki, Humberto N. Yoshimura, Carla C. Gonzaga, Victor Styopkin

Dental Materials· Volume 24· Issue 8
Publisher page

Abstract

Objectives To determine the stress corrosion susceptibility coefficient, n, of seven dental porcelains (A: Ceramco I; B: Ceramco-II; C: Ceramco-III; D: d.Sign; E: Cerabien; F: Vitadur-Alpha; and G: Ultropaline) after aging in air or artificial saliva, and correlate results with leucite content (LC). Methods Bars were fired according to manufacturers' instructions and polished before induction of cracks by a Vickers indenter (19.6N, 20s). Four specimens were stored in air/room temperature, and three in saliva/37 degrees C. Five indentations were made per specimen and crack lengths measured at the following times: approximately 0; 1; 3; 10; 30; 100; 300; 1000 and 3000 h. The stress corrosion coefficient n was calculated by linear regression analysis after plotting crack length as a function of time, considering that the slope of the curve was [2/(3n+2)]. Microstructural analysis was performed to determine LC. Results LC of the porcelains were 22% (A and B); 6% (C); 15% (D); 0% (E and F); and 13% (G). Except for porcelains A and D, all materials showed a decrease in their n values when stored in artificial saliva. However, the decrease was more pronounced for porcelains B, F, and G. Ranking of materials varied according to storage media (in air, porcelain G showed higher n compared to A, while in saliva both showed similar coefficients). No correlation was found between n values and LC in air or saliva. Significance Storage media influenced the n value obtained for most of the materials. LC did not affect resistance to slow crack growth regardless of the test environment.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Clinical assessment of high-strength all-ceramic crowns10.1016/S0022-3913(00)70033-3 ↗
2. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling10.1177/00220345950740060301 ↗
3. Survival of in-ceram crowns in a private practice: a prospective clinical trial10.1016/S0022-3913(00)80015-3 ↗
4. Fracture surface characterization of clinically failed all-ceramic crowns10.1177/00220345940730120601 ↗
5. Fatigue failure parameters of IPS-empress porcelain
6. Predicting lifetimes of materials and material structures10.1016/0109-5641(95)80050-6 ↗
7. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses10.1016/S0142-9612(01)00206-X ↗
8. Fatigue of dental ceramics in a simulated oral environment10.1177/00220345860650071901 ↗
9. Watchman · 1996
10. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics10.1016/j.dental.2003.05.003 ↗
11. Green · 1998
12. Wiederhorn · 1974
13. Post-indentation slow growth of radial cracks in glasses10.1111/j.1151-2916.1981.tb09909.x ↗
14. Correlation between fracture toughness and leucite content in dental porcelains10.1016/j.jdent.2005.02.001 ↗
15. Fracture toughness of dental porcelains evaluated by IF, SCF, and SEPB methods10.1111/j.1551-2916.2005.00334.x ↗
16. ASTM C. Flexural strength of advanced ceramics at ambient temperature; 2002.
17. Cracking and the indentation size effect for Knoop hardness of glasses10.1111/j.1151-2916.2003.tb03319.x ↗
18. Variables that affect the indentation fracture testing (IF) of a dental porcelain10.4028/www.scientific.net/MSF.416-418.663 ↗
19. Elastic–plastic indentation damage in ceramics—the median-radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
20. A critical-evaluation of indentation techniques for measuring fracture-toughness. Part 1. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
21. Influence of test methods on fracture toughness of a dental porcelain and a soda lime glass10.1111/j.1551-2916.2005.00515.x ↗
22. Dynamic fatigue of feldspathic porcelain10.1016/0109-5641(93)90073-Y ↗
23. Prediction of the service life of dental porcelains by the measurements of post-indentation slow crack growth10.4012/dmj.12.45 ↗
24. Effect of cubic leucite stabilization on the flexural strength of feldspathic dental porcelain10.1177/00220345960750120301 ↗
25. Slow fracture model based on strained silicate structures10.1063/1.333789 ↗
26. Doremus · 1994
27. Crack velocity functions and tresholds in brittle solids10.1016/0955-2219(90)90053-I ↗
28. Influence of water vapor on crack propagation in soda-lime glass10.1111/j.1151-2916.1967.tb15145.x ↗
29. Chemical interpretation of static fatigue10.1111/j.1151-2916.1972.tb11215.x ↗
30. Transverse strength of aluminous and feldspathic porcelain10.1177/00220345740530032801 ↗
31. The endurance limit of dental porcelain10.1111/j.1834-7819.1974.tb05012.x ↗
32. Analysis of tempering stresses in metal ceramic disks10.1177/00220345960750020301 ↗
33. Fractographic analyses of three ceramic whole crown restoration failures10.1016/j.dental.2005.01.006 ↗
34. Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics
35. Flexural strength of a layered zirconia and porcelain dental all-ceramic system10.1016/j.prosdent.2005.05.007 ↗
36. Mechanical fatigue of a feldspathic dental procelain10.1016/0109-5641(93)90071-W ↗
37. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗