Fracture strength of machined ceramic crowns as a function of tooth preparation design and the elastic modulus of the cement
Source abstract
Abstract
Objectives To determine, by means of static fracture testing the effect of the tooth preparation design and the elastic modulus of the cement on the structural integrity of the cemented machined ceramic crown-tooth complex. Methods Human maxillary extracted premolar teeth were prepared for all-ceramic crowns using two preparation designs; a standard preparation in accordance with established protocols and a novel design with a flat occlusal design. All-ceramic feldspathic (Vita MK II) crowns were milled for all the preparations using a CAD/CAM system (CEREC-3). The machined all-ceramic crowns were resin bonded to the tooth structure using one of three cements with different elastic moduli: Super-Bond C&B, Rely X Unicem and Panavia F 2.0. The specimens were subjected to compressive force through a 4mm diameter steel ball at a crosshead speed of 1mm/min using a universal test machine (Loyds Instrument Model LRX.). The load at the fracture point was recorded for each specimen in Newtons (N). These values were compared to a control group of unprepared/unrestored teeth. Results There was a significant difference between the control group, with higher fracture strength, and the cemented samples regardless of the occlusal design and the type of resin cement. There was no significant difference in mean fracture load between the two designs of occlusal preparation using Super-Bond C&B. For the Rely X Unicem and Panavia F 2.0 cements, the proposed preparation design with a flat occlusal morphology provides a system with increased fracture strength. Significance The proposed novel flat design showed less dependency on the resin cement selection in relation to the fracture strength of the restored tooth. The choice of the cement resin, with respect to its modulus of elasticity, is more important in the anatomic design than in the flat design.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling10.1111/j.1365-2842.2005.01604.x ↗
2. Callister · 2002
3. The effect of luting media on the fracture resistance of a flame sprayed all-ceramic crown10.1016/S0300-5712(01)00040-9 ↗
4. Structural reliability of alumina-: feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
5. Direct resin composite inlays/onlays: an 11 year follow-up10.1016/S0300-5712(00)00010-5 ↗
6. Maximal bite forces in healthy young adults as predicted by surface electromyography10.1016/j.jdent.2004.02.009 ↗
7. Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crowns10.1016/j.prosdent.2005.11.014 ↗
8. ZrO2 three-unit fixed partial dentures: comparison of failure load before and after exposure to a mastication simulator10.1111/j.1365-2842.2006.01705.x ↗
9. CEREC: science, research, and clinical application
10. Shillinburg · 2012 · 149
11. Rosenstiel · 2006 · 258
12. Photoelasticity as a research technique for analyzing stresses in dental structures10.1177/00220345550340060601 ↗
13. The effects of enamel anisotropy on the distribution of stress in a tooth10.1177/00220345930720111101 ↗
14. Zentner · 2003
15. In vitro study of fracture incidence and compressive fracture load of all-ceramic crowns cemented with resin-modified glass ionomer and other luting agents10.1016/S0022-3913(98)70058-7 ↗
16. The all-porcelain: resin-bonded bridge
17. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
18. Destructive stresses in adhesive luting cements10.1177/00220345910700050301 ↗
19. Effect of cement film thickness on the fracture resistance of a machinable glass-ceramic10.1016/0109-5641(94)90028-0 ↗
20. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli
21. Dynamic viscoelastic behavior of resin cements measured by torsional resonance10.1016/S0109-5641(02)00098-2 ↗
22. Effect of the crown design and interface lute parameters on the stress-state of a machined crown-tooth system: a finite element analysis10.1016/j.dental.2013.04.002 ↗
23. Marginal and internal fit of CEREC 3 CAD/CAM all-ceramic crowns
24. Three-dimensional finite element analysis of weakened roots restored with different cements in combination with titanium alloy posts10.1097/00029330-200602020-00007 ↗
25. Laboratory simulation of Y-TZP all-ceramic crown clinical failures10.1177/0022034509333968 ↗
26. Evaluation of the marginal fit of three margin designs of resin composite crowns using CAD/CAM10.1016/j.jdent.2006.04.008 ↗
27. Maximising the fracture resistance of dentine-bonded all-ceramic crowns10.1016/S0300-5712(98)00050-5 ↗
28. Effect of a crown ferrule on the fracture strength of endodontically treated canines restored with fiber posts and metal-ceramic or all-ceramic crowns10.11607/ijp.3409 ↗
29. Effect of thickness of zirconia-ceramic crown frameworks on strength and fracture pattern10.4012/dmj.2012-255 ↗
30. Shahrbaf · 2011
31. Effect of structural change of collagen fibrils on the durability of dentin bonding10.1016/j.biomaterials.2005.01.024 ↗
32. Influence of different adhesive resin cements on the fracture strength of aluminum oxide ceramic posterior crowns10.1016/j.prosdent.2004.07.018 ↗
33. Fracture strength of all-ceramic crowns luted using two bonding methods10.1016/j.prosdent.2003.12.005 ↗
34. Craig · 2006
35. Fracture strength and fatigue resistance of all-ceramic molar crowns manufactured with CAD/CAM technology10.1111/j.1532-849X.2008.00305.x ↗
36. A new method to test the fracture probability of all-ceramic crowns with a dual-axis chewing simulator10.1016/j.dental.2010.09.004 ↗