journal article·2015-12

Comparison of the microstructure and phase stability of as-cast, CAD/CAM and powder metallurgy manufactured Co–Cr dental alloys

Kai Chun Li, David J. Prior, J. Neil Waddell, Michael V. Swain

Dental Materials· Volume 31· Issue 12
Publisher page

Abstract

Objective The objective of this study was to identify the different microstructures produced by CC, PM and as-cast techniques for Co-Cr alloys and their phase stability following porcelain firings. Methods Three bi-layer porcelain veneered Co-Cr specimens and one monolithic Co-Cr specimen of each alloy group [cast, powder metallurgy (PM), CAD/CAM (CC)] were manufactured and analyzed using electron backscatter diffraction (EBSD), energy dispersive spectrometry (EDS) and X-ray diffraction (XRD). Specimens were treated to incremental numbers of porcelain firings (control 0, 5, 15) with crystallographic data, grain size and chemical composition subsequently obtained and analyzed. Results EBSD datasets of the cast alloy indicated large grains >200 μm whereas PM and CC alloy consisted of mean arithmetic grain sizes of 29.6 μm and 19.2 μm respectively. XRD and EBSD results both indicated the highest increase in hcp content (>13vol%) for cast Co-Cr alloy after treatment with porcelain firing while PM and CC indicated <2vol% hcp content. A fine grain interfacial layer developed on all surfaces of the alloy after porcelain firing. The depth of this layer increased with porcelain firings for as-cast and PM but no significant increase (p>.05) was observed in CC. EDS line scans indicated an increase in Cr content at the alloy surface after porcelain firing treatment for all three alloys. Significance PM and CC produced alloy had superior fcc phase stability after porcelain firings compared to a traditional cast alloy. It is recommended that PM and CC alloys be used for porcelain-fused-to-metal restorations.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Nanoarchitectured Co–Cr–Mo orthopedic implant alloys: nitrogen-enhanced nanostructural evolution and its effect on phase stability10.1016/j.actbio.2012.12.013 ↗
2. The Co–Cr (cobalt–chromium) system
3. Direct evidence of magnetically induced phase separation in the fcc phase and thermodynamic calculations of phase equilibria of the Co–Cr system10.1016/S1359-6454(01)00433-5 ↗
4. Co–Cr (cobalt–chromium)10.1361/105497103770330460 ↗
5. Effects of Ni and Mo on the microstructure and some other properties of Co–Cr dental alloys10.1016/j.jallcom.2003.07.004 ↗
6. Martensitic transformation in a cast Co–Cr–Mo–C alloy10.1007/s11661-007-9370-8 ↗
7. Davis · 2000
8. Significant improvement in mechanical properties of biomedical Co–Cr–Mo alloys with combination of N addition and Cr-enrichment10.2320/matertrans.MRA2007220 ↗
9. Effects of nitrogen addition on microstructure and mechanical behavior of biomedical Co–Cr–Mo alloys10.1016/j.jmbbm.2013.10.006 ↗
10. Effects of grain size, texture and twinning on mechanical properties and work-hardening behavior of AZ31 magnesium alloys10.1016/j.msea.2011.07.076 ↗
11. Effect of interfacial variables on metal–porcelain bonding10.1002/jbm.820270414 ↗
12. Effect of oxidation on ceramometal bond strength10.1016/0022-3913(82)90243-8 ↗
13. Interactive effects of etching and pre-oxidation on porcelain adherence to non-precious alloys: a guided planar shear test study10.1016/S0109-5641(05)80001-6 ↗
14. The effect of oxidation heat treatment on porcelain bond strength in selected base metal alloys10.1016/0022-3913(91)90502-N ↗
15. The effect of heat treatment on hardness of a chromium–cobalt alloy10.1016/0022-3913(65)90127-7 ↗
16. Metallurgical, surface, and corrosion analysis of Ni–Cr dental casting alloys before and after porcelain firing10.1016/j.dental.2007.06.010 ↗
17. Veterans Administration Cooperative Studies Project No. 147/242. Part VII: the mechanical properties of metal ceramic alloys as cast and after simulated porcelain firing10.1016/0022-3913(89)90366-1 ↗
18. Properties of cobalt–chromium metal ceramic alloys after heat treatment10.1016/0022-3913(90)90232-2 ↗
19. Effects of the porcelain-fused-to-metal firing process on the surface and corrosion of two Co–Cr dental alloys10.1007/s10853-010-4927-0 ↗
20. Surface characteristics and corrosion properties of selective laser melted Co–Cr dental alloy after porcelain firing10.1016/j.dental.2013.11.013 ↗
21. EBSD in the Earth sciences: applications, common practice, and challenges
22. First combined electron backscatter diffraction and transmission electron microscopy study of grain boundary structure of deformed quartzite10.1111/j.1365-2818.2006.01697.x ↗
23. Nishiyama · 2012
24. FCC to HCP transformation kinetics in a Co–27Cr–5Mo–0.23C alloy10.1007/s10853-010-4969-3 ↗
25. Grain size effect on the martensite formation in a high-manganese TWIP steel by the Rietveld method10.1016/S1005-0302(10)60030-8 ↗
26. Gupta · 2002
27. Adherence controlling elements in ceramic–metal systems, II. Nonprecious alloys10.1177/00220345770560090401 ↗
28. Microprobe analyses of gold–porcelain bonding10.1177/00220345690480061901 ↗
29. Effect of four different surface treatments on shear bond strength of three porcelain repair systems: an in vitro study10.4103/0972-0707.111315 ↗
30. Influence of surface treatment on the shear bond strength of ceramics fused to cobalt–chromium10.1111/j.1532-849X.2009.00546.x ↗
31. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
32. Ceramic bonding to a dental gold–titanium alloy10.1016/S0142-9612(01)00248-4 ↗
33. Surface analysis of porcelain fused to metal systems10.1016/j.dental.2005.05.003 ↗
34. Tensile strength determination of the interface between porcelain fused to gold10.1002/jbm.820030302 ↗
35. Grain boundary diffusion of Fe in ultrafine-grained nanocluster-strengthened ferritic steel10.1016/j.actamat.2010.10.067 ↗
36. Smith · 2003