Zirconia-reinforced lithium silicate crowns: Effect of thickness on survival and failure mode

Edmara T.P. Bergamo, Dimorvan Bordin, Ilana S. Ramalho, Adolfo C.O. Lopes, Rafael S. Gomes, Marina Kaizer, Lukasz Witek, Estevam A. Bonfante, Paulo G. Coelho, Altair A. Del Bel Cury

Dental Materials· Volume 35· Issue 7
Publisher page

Abstract

Objective To evaluate the reliability and failure mode of zirconia-reinforced lithium silicate (ZLS) molar crowns of different thicknesses. Methods Monolithic ZLS molar crowns (0.5mm, 1.0mm, and 1.5 mm thickness) were modeled and milled using a CAD/CAM system (n = 21/group). Crowns were cemented on dentin-like epoxy resin replicas with a resin cement. The specimens were subjected to single load-to-failure test for step-stress profiles designing. Mouth-motion step-stress accelerated-life test was performed under water by sliding an indenter 0.7 mm lingually down on the distobuccal cusp until specimen fracture or suspension. Use level probability Weibull curves and reliability were calculated and plotted. Polarized-light optical microscope and scanning electron microscope (SEM) were used to characterize fracture patterns. Results Irrespective of crown thickness, beta (β) values were higher than 1 and fatigue accelerated failures. While 0.5 mm ZLS crowns exhibited a significant reduction in the probability of survival at 200N, 300N and 400 N mission loads (69%, 41% and 19%, respectively), no significant difference was observed between 1.0 mm and 1.5 mm crowns. Both thicknesses have maintained the survivability at approximately 90%. Failure primarily comprised bulk fracture where radial cracks originated from the cementation surface beneath the indenter loading trail and propagated towards the cervical margin. Significance 1.5 mm- and 1.0 mm-thickness monolithic ZLS crowns presented higher probability of survival compared to 0.5 mm crowns. Bulk fracture was the chief failure mode, regardless of thickness.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. All-ceramic systems: laboratory and clinical performance10.1016/j.cden.2011.01.005 ↗
2. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part II: multiple-unit FDPs10.1016/j.dental.2015.02.013 ↗
3. Clinical evaluation of zirconia-based all-ceramic single crowns: an up to 12-year retrospective cohort study10.1007/s00784-017-2142-y ↗
4. Survival and chipping of zirconia-based and metal-ceramic implant-supported single crowns
5. Dental ceramics: a review of new materials and processing methods10.1590/1807-3107bor-2017.vol31.0058 ↗
6. Residual stresses in porcelain-veneered zirconia prostheses10.1016/j.dental.2012.04.019 ↗
7. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part I: single crowns (SCs)10.1016/j.dental.2015.02.011 ↗
8. Fracture-resistant monolithic dental crowns10.1016/j.dental.2015.12.010 ↗
9. Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue
10. Reliability of reduced-thickness and thinly veneered lithium disilicate crowns10.1177/0022034511433504 ↗
11. Fatigue behavior of ultrafine tabletop ceramic restorations10.1016/j.dental.2018.06.017 ↗
12. Influence of cyclic loading and luting agents on the fracture load of two all-ceramic crown systems10.1016/j.prosdent.2004.09.002 ↗
13. Adhesive cementation promotes higher fatigue resistance to zirconia crowns10.2341/16-002-L ↗
14. Influence of cementation on in vitro performance, marginal adaptation and fracture resistance of CAD/CAM-fabricated ZLS molar crowns10.1016/j.dental.2015.08.154 ↗
15. Cementation of glass-ceramic posterior restorations: a systematic review10.1155/2015/148954 ↗
16. Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: effect of ceramic thickness10.1016/j.dental.2018.03.004 ↗
17. Approximate relative fatigue life estimation methods for thin-walled monolithic ceramic crowns10.1016/j.dental.2018.01.020 ↗
18. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics10.1002/1097-4636(2000)53:4<297::AID-JBM3>3.0.CO;2-G ↗
19. Mechanical and optical properties of monolithic CAD-CAM restorative materials10.1016/j.prosdent.2017.06.012 ↗
20. Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: a systematic review10.1016/j.prosdent.2014.01.005 ↗
21. Clinical survival of chair-side generated monolithic lithium disilicate crowns: 10-year results10.1007/s00784-017-2271-3 ↗
22. Clinical results of lithium-disilicate crowns after up to 9 years of service10.1007/s00784-012-0700-x ↗
23. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
24. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
25. Microstructural and mechanical characterization of CAD/CAM materials for monolithic dental restorations10.1111/jopr.12964 ↗
26. Fracture toughness of chairside CAD/CAM materials - Alternative loading approach for compact tension test10.1016/j.dental.2016.03.003 ↗
27. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
28. Wear, strength, modulus and hardness of CAD/CAM restorative materials10.1016/j.dental.2016.08.222 ↗
29. Fracture resistance of monolithic glass-ceramics versus bilayered zirconia-based restorations
30. Damage maps for layered ceramics under simulated mastication10.1177/154405910808700706 ↗
31. Performance of dental ceramics: challenges for improvements10.1177/0022034510391795 ↗
32. Stress fatigue: basic principles and prosthodontic implications
33. Competing fracture modes in brittle materials subject to concentrated cyclic loading in liquid environments: monoliths10.1557/JMR.2005.0276 ↗
34. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗
35. Sliding contact fatigue damage in layered ceramic structures10.1177/154405910708601105 ↗
36. A critical perspective on mechanical testing of implants and prostheses10.1177/0022034515624445 ↗
37. Fatigue anddamage accumulation of veneer porcelain pressed on Y-TZP10.1016/j.jdent.2009.12.004 ↗
38. Failure modes of Y-TZP crowns at different cusp inclines10.1016/j.jdent.2010.04.001 ↗
39. Laboratory simulation of Y-TZP all-ceramic crown clinical failures10.1177/0022034509333968 ↗
40. Fatigue testing of two porcelain-zirconia all-ceramic crown systems10.1016/j.dental.2009.03.009 ↗
41. Polymer infiltrated ceramic network structures for resistance to fatigue fracture and wear10.1016/j.dental.2016.08.216 ↗
42. Fatigue resistance of CAD/CAM resin composite molar crowns10.1016/j.dental.2015.12.005 ↗
43. Modified Y-TZP core design improves all-ceramic crown reliability10.1177/0022034510384617 ↗
44. Reliability of metalloceramic and zirconia-based ceramic crowns10.1177/0022034510375826 ↗
45. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
46. Load-bearing capacity of lithium disilicate and ultra-translucent zirconias10.1016/j.jmbbm.2018.08.023 ↗
47. Effects of surface treatments on the bond strength between resin cement and a new zirconia-reinforced Lithium silicate ceramic10.2341/14-357-L ↗
48. A general accelerated life model for step-stress testing10.1080/07408170500232396 ↗
49. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
50. Nelson · 2004
51. Occlusal forces during chewing--influences of biting strength and food consistency10.1016/0022-3913(81)90247-X ↗
52. Bite forces and their resultants during forceful intercuspal clenching in humans10.1016/j.jbiomech.2009.03.040 ↗
53. Relative flexural strength of dental restorative ceramics10.1016/0109-5641(90)90026-B ↗
54. Strength of CAD/CAM-generated esthetic ceramic molar implant crowns
55. Effect of acid etching on tridimensional microstructure of etchable CAD/CAM materials10.1016/j.dental.2018.03.013 ↗
56. Self-etching ceramic primer versus hydrofluoric acid etching: etching efficacy and bonding performance10.1016/j.jpor.2017.06.002 ↗
57. New single-bottle ceramic primer: 6-month case report and laboratory performance10.5005/jp-journals-10024-1977 ↗
58. Fractographic analyses of all-ceramic crowns: a study of 27 clinically fractured crowns10.1016/j.dental.2013.03.018 ↗
59. Fractographic features of glass-ceramic and zirconia-based dental restorations fractured during clinical function10.1111/eos.12127 ↗
60. Three- to nine-year survival estimates and fracture mechanisms of zirconia- and alumina-based restorations using standardized criteria to distinguish the severity of ceramic fractures10.1007/s00784-015-1455-y ↗