journal article·2018-02

Light irradiance through novel CAD–CAM block materials and degree of conversion of composite cements

Diogo Pedrollo Lise, Annelies Van Ende, Jan De Munck, Kumiko Yoshihara, Noriyuki Nagaoka, Luiz Clovis Cardoso Vieira, Bart Van Meerbeek

Dental Materials· Volume 34· Issue 2
Publisher page

Abstract

Objective To assess light irradiance (LI) delivered by two light-curing units (LCU's) and to measure the degree of conversion (DC) of three composite cements, when cured through different thicknesses of two novel CAD-CAM block materials. Methods 100-μm-thick films of a dual-curable composite cement (G-CEM LinkAce, GC), a light-curable flowable resin-based composite (RBC) (G-ænial Universal Flo, GC) and a micro-hybrid RBC (G-ænial Posterior, GC) were investigated as luting agents. Two 'polymer-ceramic' CAD-CAM blocks (Cerasmart, GC; Enamic, Vita Zahnfabrik) were sectioned in slabs with different thicknesses (1, 3 and 5mm). LI at the bottom of the specimens was measured using a calibrated spectrometer, while being light-cured through the CAD-CAM block slabs for 40s with a low- (±500mW/cm2) or high- (±1,600mW/cm2) irradiance LCU (n=5). After light-curing, micro-Raman spectra of the composite films were acquired to determine DC at 5min, 10min, 1h and 24h. LI data were statistically analyzed by Kruskal-Wallis followed by post-hoc comparisons, while a linear mixed-effect model was applied for the DC analysis. In addition, the CAD-CAM blocks ultrastructure was characterized upon argon-ion slicing using scanning transmission electron microscopy (STEM). Finally, light transmission (LT) through each CAD-CAM block material was assessed using a spectrophotometer. Results Curing-light attenuation and DC were significantly influenced by thickness and type of the overlying material. LCU only had a significant effect on DC of the micro-hybrid RBC. DC significantly increased over time for all composite cements. CAD-CAM block structural analysis revealed a relatively small and homogenous filler configuration (mean filler size of 0.2-0.5μm) for Cerasmart, while Enamic contained ceramic grains varying in shape and size (1-10μm), which were interconnected by the polymer-based network. LT was much higher at a wavelength range of 300-800nm for Cerasmart than for Enamic. Significance Light-curable composite cements can be cured through a restoration up to 2.7-mm thickness, depending on the kind of CAD-CAM material. A high-irradiance LCU only has a limited effect on the maximum thickness of the polymer-ceramic CAD-CAM material that can be cured through.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Anatomy and Medical Technology · Photopolymerization techniques and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Mechanical properties of luting cements after water storage
2. Marginal discrepancies and leakage of all-ceramic crowns: influence of luting agents and aging conditions
3. Influence of ceramic thickness on mechanical properties and polymer structure of dual-cured resin luting agents10.1016/j.dental.2007.06.014 ↗
4. Influence of radiant exposure on contraction stress, degree of conversion and mechanical properties of resin composites10.1016/j.dental.2005.11.008 ↗
5. Correlation between clinical performance and degree of conversion of resin cements: a literature review10.1590/1678-775720140524 ↗
6. Longevity of ceramic inlays and onlays luted with a solely light-curing composite resin10.1016/j.jdent.2004.10.026 ↗
7. Indirect composite restorations luted with two different procedures: a ten years follow up clinical trial10.4317/jced.51640 ↗
8. Clinical evaluation on porcelain laminate veneers bonded with light-cured composite: results up to 7 years10.1007/s00784-011-0593-0 ↗
9. Five-year retrospective clinical study of indirect composite restorations luted with a light-cured composite in posterior teeth10.1007/s00784-013-1001-8 ↗
10. Long-term bond between dual-polymerizing cementing agents and human hard dental tissue10.1016/j.dental.2006.01.012 ↗
11. Effect of curing mode on the micro-mechanical properties of dual-cured self-adhesive resin cements10.1007/s00784-011-0527-x ↗
12. Curing-light attenuation in filled-resin restorative materials10.1016/j.dental.2005.11.009 ↗
13. Correlation between ceramics translucency and polymerization efficiency through ceramics10.1016/j.dental.2007.11.006 ↗
14. Mechanical properties of resin-ceramic CAD/CAM restorative materials10.1016/j.prosdent.2015.04.016 ↗
15. Light transmission of novel CAD/CAM materials and their influence on the degree of conversion of a dual-curing resin cement
16. Mechanical properties of composite resin blocks for CAD/CAM10.4012/dmj.2014-208 ↗
17. Characterization of a polymer-infiltrated ceramic-network material10.1016/j.dental.2014.02.019 ↗
18. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
19. Determination of VITA classical shades with the 3D-master shade guide10.3109/00016357.2012.715197 ↗
20. Evaluation of mechanical and optical behavior of current esthetic dental restorative CAD/CAM composites10.1016/j.jmbbm.2015.10.004 ↗
21. Refractive index mismatch and monomer reactivity influence composite curing depth10.1177/154405910808700115 ↗
22. The effect of nanofiller on the opacity of experimental composites
23. Spectral characteristics of light-curing units and dental adhesives10.2494/photopolymer.24.411 ↗
24. Effect of different photoinitiators and reducing agents on cure efficiency and color stability of resin-based composites using different LED wavelengths10.1016/j.jdent.2015.08.015 ↗
25. UV–vis spectrophotometric direct transmittance analysis of composite resins10.1016/j.dental.2006.06.020 ↗
26. Optical properties of composites of selected shades in white light10.1111/j.1365-2842.1983.tb00126.x ↗
27. Color of selected shades of composites by reflection spetrophotometry10.1177/00220345820610101401 ↗
28. High irradiance curing and anomalies of exposure reciprocity law in resin-based materials10.1016/j.jdent.2011.05.007 ↗
29. Polymerization efficiency of different photocuring units through ceramic discs10.2341/04-188 ↗
30. The effect of ceramic restoration shade and thickness on the polymerization of light- and dual-cure resin cements10.2341/10-206-L ↗
31. Effects of ceramic thickness and curing unit on light transmission through leucite-reiforced material and polymerization of dual-cured luting agent10.2334/josnusd.50.131 ↗
32. Post-irradiation polymerization of different anterior and posterior visible light-activated resin composites10.1016/0109-5641(92)90104-K ↗
33. Influence of pulse-delay curing on softening of polymer structures10.1177/00220345010800061801 ↗
34. Oxygen inhibition in dental resins10.1177/154405910508400808 ↗
35. Marginal adaptation of ceramic crowns: a systematic review10.1016/j.prosdent.2013.08.003 ↗
36. Effect of ceramic shade on the degree of conversion of a dual-cure resin cement analyzed by FTIR10.1016/j.dental.2012.11.014 ↗
37. Degree of conversion of a resin cement light-cured through ceramic veneers of different thicknesses and types10.1590/0103-6440201302200 ↗
38. Influence of the curing mode on the degree of conversion of a dual-cured self-adhesive resin luting cement beneath ceramic10.3109/00016357.2012.690571 ↗
39. Degree of conversion of luting resins around ceramic inlays in natural deep cavities: a micro-Raman spectroscopy analysis10.2341/10-012-L ↗
40. Degree of conversion of three composite materials employed in the adhesive cementation of indirect restorations: a micro-Raman analysis10.1016/j.jdent.2009.04.001 ↗
41. The micro-Raman spectroscopy, a useful tool to determine the degree of conversion of light-activated composite resins10.1002/(SICI)1097-4636(1999)48:5<675::AID-JBM11>3.0.CO;2-P ↗
42. Effect of temperature on the degree of conversion and working time of dual-cured resin cements exposed to different curing conditions10.2341/11-198-L ↗