Abstract

OBJECTIVE: A major limiting factor for the widespread use of zirconia in prosthetic dentistry is its poor resin-cement bonding capabilities. We show that this deficiency can be overcome by infiltrating the zirconia cementation surface with glass. Current methods for assessing the fracture resistance of resin-ceramic bonds are marred by uneven stress distribution at the interface, which may result in erroneous interfacial fracture resistance values. We have applied a wedge-loaded double-cantilever-beam testing approach to accurately measure the interfacial fracture resistance of adhesively bonded zirconia-based restorative materials. METHODS: The interfacial fracture energy GC was determined for adhesively bonded zirconia, graded zirconia and feldspathic ceramic bars. The bonding surfaces were subjected to sandblasting or acid etching treatments. Baseline GC was measured for bonded specimens subjected to 7 days hydration at 37°C. Long-term GC was determined for specimens exposed to 20,000 thermal cycles between 5 and 55°C followed by 2-month aging at 37°C in water. The test data were interpreted with the aid of a 2D finite element fracture analysis. RESULTS: The baseline and long-term GC for graded zirconia was 2-3 and 8 times greater than that for zirconia, respectively. More significantly, both the baseline and long-term GC of graded zirconia were similar to those for feldspathic ceramic. SIGNIFICANCE: The interfacial fracture energy of feldspathic ceramic and graded zirconia was controlled by the fracture energy of the resin cement while that of zirconia by the interface. GC for the graded zirconia was as large as for feldspathic ceramic, making it an attractive material for use in dentistry.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
2. Damage accumulation and fatigue life of particle-abraded ceramics
3. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
4. The effect of nano-structured alumina coating on resin-bond strength to zirconia ceramics10.1016/j.dental.2010.03.013 ↗
5. Superhydrophobic nanostructured boehmite coatings prepared by AlN powder hydrolysis10.1111/j.1744-7402.2010.02516.x ↗
6. Effects of cementation surface modifications on fracture resistance of zirconia10.1016/j.dental.2015.01.013 ↗
7. Surface modification for enhanced silanation of zirconia ceramics10.1016/j.dental.2009.03.008 ↗
8. Silica-based nano-coating on zirconia surfaces using reactive magnetron sputtering: Effect on chemical adhesion of resin cements
9. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
10. Methacrylate bonding to zirconia by in situ silica nanoparticle surface deposition10.1016/j.dental.2014.11.011 ↗
11. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
12. Graded structures for all-ceramic restorations10.1177/0022034510363245 ↗
13. Graded structures for damage resistant and aesthetic all-ceramic restorations10.1016/j.dental.2009.01.002 ↗
14. Sliding contact fatigue of graded zirconia with external esthetic glass10.1177/0022034511412075 ↗
15. Overview: Damage resistance of graded ceramic restorative materials10.1016/j.jeurceramsoc.2012.02.020 ↗
16. Optimization of ceramic strength using elastic gradients10.1016/j.actamat.2009.02.037 ↗
17. Designing functionally graded materials with superior load-bearing properties10.1016/j.actbio.2011.11.033 ↗
18. On the interfacial fracture of porcelain/zirconia and graded zirconia dental structures10.1016/j.actbio.2014.04.016 ↗
19. Graded zirconia glass for resistance to veneer fracture10.1177/0022034510375289 ↗
20. Chipping resistance of graded zirconia ceramics for dental crowns10.1177/0022034511434356 ↗
21. Edge chipping and flexural resistance of monolithic ceramics10.1016/j.dental.2013.09.004 ↗
22. Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling10.1016/j.dental.2008.03.028 ↗
23. Relationship between surface area for adhesion and tensile bond strength – evaluation of a micro-tensile bond test10.1016/0109-5641(94)90067-1 ↗
24. The effect of surface modification on the retention strength of polyetheretherketone crowns adhesively bonded to dentin abutments10.1016/j.prosdent.2014.05.010 ↗
25. Microtensile bond strength and impact energy of fracture of cad-veneered zirconia restorations10.1111/j.1532-849X.2008.00412.x ↗
26. Comparison of two bond strength testing methodologies for bilayered all-ceramics10.1016/j.dental.2006.05.004 ↗
27. A fluid filtration and clearing technique to assess microleakage associated with three dentine bonding systems10.1016/S0300-5712(98)00048-7 ↗
28. Shear vs. Tensile bond strength of resin composite bonded to ceramic10.1177/00220345950740091401 ↗
29. A critique of bond strength measurements10.1016/0300-5712(89)90131-0 ↗
30. Shear fracture10.1007/BF00041716 ↗
31. On the correlation between the mode i failure of adhesive joints and laminated composites10.1016/0013-7944(86)90071-8 ↗
32. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods10.1016/j.dental.2005.11.040 ↗
33. Surface conditioning influences zirconia ceramic bonding10.1177/0022034509340881 ↗
34. Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers’ instructions of the cements only10.1007/s00784-007-0151-y ↗
35. Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain10.1016/0022-3913(94)90553-3 ↗
36. Della Bona · 2009
37. Modeling of water absorption induced cracks in resin-based composite supported ceramic layer structures10.1002/jbm.b.30852 ↗
38. Effect of water storage time and composite cement thickness on fatigue of a glass-ceramic trilayer system10.1002/jbm.b.30851 ↗
39. Thermal cycling procedures for laboratory testing of dental restorations10.1016/S0300-5712(98)00037-2 ↗
40. Verification of theoretical modeling of heat transmission in teeth by in vivo experiments10.1177/00220345870660080901 ↗
41. Transverse fracture in multilayers from tension and line-wedge indentation10.1007/s10704-007-9129-7 ↗
42. Bond thickness effect in adhesive joints and its significance for mode i interlaminar fracture of composites
43. An experimental study of the fracture resistance of bimaterial interfaces10.1016/0167-6636(89)90020-3 ↗
44. Asymmetric shielding mechanisms in the mixed-mode fracture of a glass/epoxy interface10.1115/1.2789035 ↗
45. Experimental-determination of interfacial toughness curves using brazil-nut-sandwiches10.1016/0956-7151(90)90200-Z ↗
46. The fracture of epoxy- and elastomer-modified epoxy polymers in bulk and as adhesives10.1002/app.1975.070190917 ↗
47. The fracture resistance of a toughened epoxy adhesive10.1080/00218468108071189 ↗
48. Influence of cooling rate on zirconia/veneer interfacial adhesion10.1016/j.actbio.2010.06.026 ↗
49. Le Thanh · 2009
50. Bond durability of the resin-bonded and silane treated ceramic surface10.1016/S0109-5641(01)00047-1 ↗