Influence of thermal and mechanical cycling on the flexural strength of ceramics with titanium or gold alloy frameworks
Source abstract
Abstract
Objectives The aim of this study was to evaluate the effect of thermal and mechanical cycling alone or in combination, on the flexural strength of ceramic and metallic frameworks cast in gold alloy or titanium. Methods Metallic frameworks (25 mm x 3 mm x 0.5 mm) (N=96) cast in gold alloy or commercial pure titanium (Ti cp) were obtained using acrylic templates. They were airborne particle-abraded with 150 microm aluminum oxide at the central area of the frameworks (8 mm x 3 mm). Bonding agent and opaque were applied on the particle-abraded surfaces and the corresponding ceramic for each metal was fired onto them. The thickness of the ceramic layer was standardized by positioning the frameworks in a metallic template (height: 1 mm). The specimens from each ceramic-metal combination (N=96, n=12 per group) were randomly assigned into four experimental fatigue conditions, namely water storage at 37 degrees C for 24h (control group), thermal cycling (3000 cycles, between 4 and 55 degrees C, dwell time: 10s), mechanical cycling (20,000 cycles under 10 N load, immersion in distilled water at 37 degrees C) and, thermal and mechanical cycling. A flexural strength test was performed in a universal testing machine (crosshead speed: 1.5 mm/min). Data were statistically analyzed using two-way ANOVA and Tukey's test (alpha=0.05). Results The mean flexural strength values for the ceramic-gold alloy combination (55+/-7.2MPa) were significantly higher than those of the ceramic-Ti cp combination (32+/-6.7 MPa) regardless of the fatigue conditions performed (p<0.05). Mechanical and thermo-mechanical fatigue decreased the flexural strength results significantly for both ceramic-gold alloy (52+/-6.6 and 53+/-5.6 MPa, respectively) and ceramic-Ti cp combinations (29+/-6.8 and 29+/-6.8 MPa, respectively) compared to the control group (58+/-7.8 and 39+/-5.1 MPa, for gold and Ti cp, respectively) (p<0.05) (Tukey's test). While ceramic-Ti cp combinations failed adhesively at the metal-opaque interface, gold alloy frameworks exhibited a residue of ceramic material on the surface in all experimental groups. Significance Mechanical and thermo-mechanical fatigue conditions decreased the flexural strength values for both ceramic-gold alloy and ceramic-Ti cp combinations with the results being significantly lower for the latter in all experimental conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Clinical study on the reasons and location of the failures of metal–ceramic restorations and survival of repairs
2. Studies of Ti alloys for dental castings10.1016/0109-5641(89)90093-6 ↗
3. Layered structure of cast titanium surface10.4012/dmj.8.175 ↗
4. Oxidation effects on porcelain–titanium interface reactions and bond strength10.4012/dmj.9.91 ↗
5. Properties of test metal ceramic titanium alloys10.1016/0022-3913(92)90411-3 ↗
6. Titanium for prosthodontic applications: a review of the literature
7. Titanium and titanium alloys as dental materials
8. New approach for evaluating metal–porcelain interfacial bonding
9. Fatigue of dental ceramics in a simulated oral environment10.1177/00220345860650071901 ↗
10. Stress fatigue: basic principles and prosthodontic implications
11. Three-point bending strength of ceramics fused to cast titanium10.1111/j.1600-0722.1996.tb00083.x ↗
12. Effect of mechanical cycling on the flexural strength of reinforced ceramics10.1016/j.dental.2005.11.025 ↗
13. International Organization for Standardization. Metal–ceramic dental restorative systems: ISO 9693. ISO, 1999.
14. Longevity of repaired composite and metal–ceramic restorations: 3.5 year clinical study
15. Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium–copper alloy10.1016/S0022-3913(05)80267-7 ↗
16. Castability, opaque masking, and porcelain bonding of 17 porcelain-fused-to-metal alloys10.1016/S0022-3913(96)90027-X ↗
17. Effects of interfacial variables on ceramic adherence to cast and machined commercially pure titanium10.1016/S0022-3913(03)00263-4 ↗
18. Effect of magnesia investments in the dental casting of pure titanium or titanium alloys10.4012/dmj.1.8 ↗
19. Pure titanium casting into zirconia-modified magnesia-based investment molds10.1016/j.dental.2003.10.016 ↗
20. Evaluation of shear bond strength at the interface of two porcelains and pure titanium injected into the casting mold at three different temperatures10.1016/j.prosdent.2004.03.033 ↗
21. Ceramic bonding to a dental gold–titanium alloy10.1016/S0142-9612(01)00248-4 ↗
22. Bond strength of porcelain on cast vs. wrought titanium
23. The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium–aluminium–vanadium alloy10.1016/S0109-5641(03)00027-7 ↗
24. Fracture toughness and flexural strength of dental ceramics for titanium10.1016/0142-9612(95)91099-K ↗
25. Monotonic flexure and fatigue strength of composites for provisional and definitive restorations10.1016/S0022-3913(03)00174-4 ↗
26. Fatigue of biomaterials: a review10.1016/S0142-1123(00)00052-9 ↗
27. A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry
28. The fatigue strength of the interface between Ag–Pd alloy and hydrothermal ceramic10.1016/S0109-5641(99)00068-8 ↗
29. Effect of laboratory procedures and thermocycling on the shear bond strength of resin-metal bonding systems10.1016/S0022-3913(03)00261-0 ↗
30. Comparative strength of metal–ceramic and metal-composite bonds after extended thermocycling10.1111/j.1365-2842.2004.01391.x ↗
31. Fracture strength of four different types of anterior 3-unit bridges after thermo-mechanical fatigue in the dual-axis chewing simulator10.1046/j.1365-2842.2001.00742.x ↗
32. Prospective clinical 5-year study of ceramic-veneered titanium restorations with the Procera system10.1067/mpr.2000.110137 ↗