Optimizing mechanical properties of laser-welded gold alloy through heat treatment
Source abstract
Abstract
Objective The goal of this work was to improve the mechanical strength of laser-welded gold alloy with age-hardenability at intraoral temperature. Methods The gold alloy was cast conventionally in plate patterns (0.5 mm x 3.0 mm x 20 mm). After bench-cooling the mold to room temperature (as-cast state), transverse sections of the plate were made at mid-span. They were butted against one another and welded using Nd:YAG laser (current: 320 A; time: 10 ms; spot diameter: 1 mm). Three laser pulses were applied from both sides to cover the joint width (3.0 mm) of the specimens before or after solution heat treatment at 700 degrees C/5 min. Uncut control specimens (non-welded) were also prepared. After solution treatment, two different heat treatments were given the laser-welded specimens: high-temperature aging at 250 degrees C/15 min, or intraoral aging at 37 degrees C/3 days. Control specimens underwent all of the heat treatments after solution treatment. Tensile testing was conducted at a crosshead speed of 2 mm/min and a gauge length of 10 mm. Results Solution treatment of the gold alloy before laser-welding did not improve the mechanical strength of laser-welded gold alloy after high-temperature aging or intraoral aging. The joint strengths of laser-welded gold alloy were improved only by solution heat treatments after laser-welding and subsequent aging treatment at high or intraoral temperatures. Significance The results of this study indicated that laser-welded cast gold alloy prostheses aged at high or intraoral temperatures produce high strength when they are solution-treated after laser-welding.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Hardening of dental gold–copper alloys10.1177/00220345720510042901 ↗
2. Determination of the Au–Cu superlattice formation region in gold–copper–silver ternary system10.1177/00220345810600050501 ↗
3. Correlation between microstructure of Ag–Pd–Au–Cu alloy and changes in shape10.1002/jbm.820180611 ↗
4. Difference in age-hardening mechanism in dental gold alloys10.1177/00220345820610030601 ↗
5. A low-gold dental alloy: structure and segregations10.1177/00220345820610111601 ↗
6. High-resolution electron microscopic study of age-hardening in a commercial dental gold alloy10.1177/00220345860650091301 ↗
7. Dental gold alloys with age-hardenability at intraoral temperature10.1007/BF01154683 ↗
8. Dimensional changes related to ordering in an AuCu–3wt%Ga alloy at intraoral temperature10.1016/0109-5641(94)90061-2 ↗
9. New gold alloy with age-hardenability in oral cavity
10. Mechanical properties of laser-welded cast and wrought titanium10.1016/S0022-3913(05)80131-3 ↗
11. Mechanical properties of laser welding of titanium in dentistry by pulsed Nd:YAG laser apparatus10.1016/0022-3913(93)90063-T ↗
12. Effects of heat treatments on mechanical strength of laser-welded equi-atomic AuCu–6at%Ga alloy10.1177/00220345010800090801 ↗
13. Effects of Au/Cu ratio and gallium content on the low-temperature age-hardening in Au–Cu–Ga alloys10.1007/BF01153947 ↗
14. Effects of variable Au/Cu ratio and Ga content on the ordering in Au–Cu and Au–Cu–Ga alloys10.1016/S0925-8388(99)00491-0 ↗
15. Phillips · 1991