journal article·2016-05Open access

Behavior of failed bonded interfaces under in vitro cariogenic challenge

Anelise F. Montagner, Niek J.M. Opdam, Jan L. Ruben, Ewald M. Bronkhorst, Maximiliano S. Cenci, Marie-Charlotte D.N.J.M. Huysmans

Dental Materials· Volume 32· Issue 5

Abstract

Objective This in vitro study aimed to compare dentin wall caries development at different composite-dentin interfaces. Methods Dentin samples (10.4 mm(2)) were restored with composite resin using two adhesive systems (etch-and-rinse and self-etch techniques). Different composite-dentin interfaces with gaps were produced: (a) failed bonded, which were fractured at interface after being submitted to aging protocols (no aging, mechanical loading or water storage); (b) non-bonded interfaces, both without any adhesive material or with adhesive material applied only on the dentin. Adhesively fractured and non-bonded samples were subjected to a lactic acid gel (pH=5) caries model with a continuous opening/closing movement of the interfacial gap for 10 days. Transverse wavelength-independent microradiographs were taken, and lesion depth and mineral loss were measured. Data were analyzed with linear mixed-effects regression models. Results Caries development differed among the composite-dentin interfaces (p<0.001). The non-bonded interface with adhesive material on the dentin showed less lesion depth than the failed bonded groups, while the non-bonded interface without adhesive on dentin showed the deepest wall lesions. Difference between the adhesive systems was observed only in the non-bonded groups (p=0.003), with the self-etch adhesive applied on the dentin showing more severe lesions. Samples broken after mechanical loading aging showed deeper lesions than those broken after water storage (p<0.001). Significance Composite-dentin interfaces failed after aging presented different demineralization from interfaces that were never bonded, indicating that the restorative treatment changes the tissue in a way relevant to secondary caries development.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Health and Care Utilization · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. 22-Year clinical evaluation of the performance of two posterior composites with different filler characteristics10.1016/j.dental.2011.06.001 ↗
2. Patient risk factors’ influence on survival of posterior composites10.1177/0022034513484337 ↗
3. What constitutes dental caries? Histopathology of carious enamel and dentin related to the action of cariogenic biofilms10.1177/154405910408301s07 ↗
4. Histopathology of natural caries around silver amalgam fillings10.1159/000260123 ↗
5. Adhesive/dentin interface: the weak link in the composite restoration10.1007/s10439-010-9969-6 ↗
6. Ten-years degradation of resin-dentin bonds10.1111/j.1600-0722.2010.00744.x ↗
7. Effect of water on bonding of one-bottle self-etching adhesives10.4012/dmj.27.172 ↗
8. Cariogenic bacteria degrade dental resin composites and adhesives10.1177/0022034513504436 ↗
9. Hydrodynamic flow through loading and in vitro secondary caries development10.1177/0022034513481040 ↗
10. Restoration materials and secondary caries using an in vitro biofilm model10.1177/0022034514553245 ↗
11. Wall lesion development in gaps: the role of the adhesive bonding material10.1016/j.jdent.2015.04.007 ↗
12. A multifunctional device to simulate oral ageing: the Rub&Roll10.1016/j.jmbbm.2013.10.019 ↗
13. A critical review of the durability of adhesion to tooth tissue: methods and results10.1177/154405910508400204 ↗
14. Dental adhesion review: aging and stability of the bonded interface10.1016/j.dental.2007.02.009 ↗
15. In vitro longevity of bonding properties of universal adhesives to dentin10.2341/14-055-L ↗
16. State of the art of self-etch adhesives10.1016/j.dental.2010.10.023 ↗
17. Permeability of dental adhesives – a SEM assessment10.1055/s-0039-1697863 ↗
18. A prospective, randomized clinical trial of a two-step self-etching vs. two-step etch-and-rinse adhesive and SEM margin analysis: four-year results
19. Effect of gap geometry on secondary caries wall lesion development10.1159/000329384 ↗
20. Isolated development of inner (wall) caries like lesions in a bacterial-based in vitro model10.1007/s00784-009-0250-z ↗
21. Adhesive analysis of voids in class II composite resin restorations at the axial and gingival cavity walls restored under in vivo versus in vitro conditions10.1016/j.dental.2006.07.001 ↗
22. Effect of cariogenic challenge on the stability of dentin bonds10.1590/1678-775720130011 ↗
23. Degradation in the dentin-composite interface subjected to multi-species biofilm challenges10.1016/j.actbio.2013.08.034 ↗