journal article·2014

Mechanical properties of model composite resin containing nanosilver filler

L.S. Gonçalves, C. Gouveia, R.F. Bonan, F.G. Carvalho, H.L. Carlo, P.R.F. Bonan, J.E. Oliveira, A.C. Lancellotti

Dental Materials· Volume 30
Publisher page

Abstract

Purpose: Previous studies have successfully added nanosilver particles in commercial restorative composites to inhibit the growth of Streptococcus mutans and Lactobacillus. The aim of the present study was to evaluate the flexural strength (FS), flexuralmodulus (E), Knoop hardness (KH) and changes in surface roughness (Ra) and gloss after simulated toothbrushing of model composites resins containing nanosilver filler. Methods and materials: A co-monomer blend of bis-GMA diluted in a 80:20 ratio with TEGDMA was used as model resin matrix. The photoinitiator system was composed by 1mol% of camphorquinone, 2mol% of ethyl-4-dimethylamino benzoate and 0.5mol% of diphenyliodonium hexafluorphosphate. Hydroxy butyl toluene (0.1mol%) was used as inhibitor. The composite resins were loaded according to the following groups: Control – 60wt% of silanated Ba-Al-Si glass fillers; G1 – 59.94wt% Ba-Al-Si glass fillers + 0.06wt% of nanosilver fillers; G2 – 59.875wt% Ba-Al-Si glass fillers + 0.125wt% nanosilver fillers; G3 – 59.75wt% Ba-Al-Si glass fillers + 0.25wt% nanosilver fillers; G4 – 59.5wt% Ba-Al-Si glass fillers + 0.5wt% nanosilver fillers; G5 – 59.0wt%Ba-Al-Si glass fillers + 1wt%nanosilver fillers; and G6 – 58.0wt% Ba-Al-Si glass fillers + 2wt% nanosilver fillers. The FS and E tests were performed in a universal testing machine with a crosshead speed of 0.5mm/min (n=10); KH was performed with a load of 25 gf during 15 s (n=8). Ra was measured with contact profilometer and the Gloss (n=8) with a glossmeter before and after simulated toothbrushing with toothpaste slurry, load of 150 g and frequency of 4Hzduring 2h. Thedata of E andKHwere submitted to one-wayANOVA; FS datawere compared by Kruskal–Wallis. The data of Ra and Gloss were analyzed by repeated-measure two-way ANOVA and t-test for paired specimens. Results: Significant differences were not found among the groups for FS (p=0.377), E (p=0.660) and KH (p=0.542). However, toothbrushing had a negative influence on the Ra and Gloss results of all tested groups (p<0.05). Conclusion: The incorporation of nanosilver fillers had no influence on the mechanical properties of the tested model composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Scientific and Engineering Research Topics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.