journal article·2012

Evaluation of hardness and fracture toughness, coupled with microstructural analysis, of zirconia ceramics stored in environments with different pH values

Volkan TURP, Betul TUNCELLI, Deniz SEN, Gultekin GOLLER

Dental Materials Journal· Volume 31· Issue 6
Publisher page

Abstract

The aim of this study was to evaluate the effects of pH changes in the oral cavity on the mechanical properties of zirconia and feldspathic ceramics. Bilayered zirconia-feldspathic samples were prepared from three different commercial brands of Y-TZP blocks: Zirkonzahn, Cercon, and Everest. Samples were stored in artificial saliva with different pH values (3.5, 7.0, and 10.0) for 10 days at 37°C. Flexural strength, Vickers hardness, and fracture toughness were calculated after samples were subjected to biaxial flexure test. Microstructural analysis of the materials was also performed.Data were analyzed by one-way analysis of variance (ANOVA), and multiple comparisons were performed using Tukey's test (α=0.05). Acidic and alkaline environments adversely affected the mechanical properties of zirconia, resulting in material degradation, loss of stabilizer content, and increase in tetragonal-monoclinic phase transformation. Commercial dental zirconia blocks have varied mechanical properties, but they are generally susceptible to degradation when exposed to corrosive environments.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. 1) Denry I, Kelly JR. State of the art of zirconia for dental applications. Dent Mater 2008; 24: 299-307.10.1016/j.dental.2007.05.007 ↗
2. 2) Anusavice KJ. Recent developments in restorative dental ceramics. J Am Dent Assoc 1993; 124: 72-84.10.14219/jada.archive.1993.0031 ↗
3. 3) Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered allceramic restorations. Part II: Zirconia veneering ceramics. Dent Mater 2006; 22: 857-863.10.1016/j.dental.2005.11.014 ↗
4. 4) Ardlin BI. Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure. Dent Mater 2002; 18: 590-595.10.1016/S0109-5641(01)00095-1 ↗
5. 5) Deville S, Chevalier J, Fantozzi G, Bartolome JF, Requena J, Moya JS, Torrecillas R, Dı́LA. Low-temperature ageing of zirconia-toughened alumina ceramics and its implication in biomedical implants. J Eur Ceram Soc 2003; 23: 2975-2982.10.1016/S0955-2219(03)00313-3 ↗
6. 6) Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 1999; 20: 1-25.10.1016/S0142-9612(98)00010-6 ↗
7. 7) Claussen N, Ruhle M, Heuer AH, editors. Advances in ceramics. Ohio: American Ceramic Society; 1984. p. 391-398.
8. 8) Chevalier J, Olagnon C, Fantozzi G. Subcritical crack growth in 3Y-TZP ceramics: static and cyclic fatigue. J Am Ceram Soc 1999; 82: 3129-3138.10.1111/j.1151-2916.1999.tb02213.x ↗
9. 9) Chevalier J, Cales B, Drouin JM. Low temperature aging of Y-TZP ceramics. J Am Ceram Soc 1999; 82: 2150-2154.10.1111/j.1151-2916.1999.tb02055.x ↗
10. 10) Swab JJ. Low temperature degradation of Y-TZP materials. J Mater Sci 1991; 26: 6706-6714.10.1007/BF02402664 ↗
11. 11) Kelly JR, Denry I. Stabilized zirconia as a structural ceramic: an overview. Dent Mater 2008; 24: 289-298.10.1016/j.dental.2007.05.005 ↗
12. 12) Guazzato M, Albakry M, Swain MV, Ironside J. Mechanical properties of In-Ceram Alumina and In-Ceram Zirconia. Int J Prosthodont 2002; 15: 339-346.
13. 13) Wang H, Aboushelib MN, Feilzer AJ. Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 2008; 24: 633-638.10.1016/j.dental.2007.06.030 ↗
14. 14) Pinto MM, Cesar PF, Rosa V, Yoshimura HN. Influence of pH on slow crack growth of dental porcelains. Dent Mater 2008; 24: 814-823.10.1016/j.dental.2007.10.001 ↗
15. 15) Studart AR, Filser F, Kocher P, Gauckler LJ. In vitro lifetime of dental ceramics under cyclic loading in water. Biomaterials 2007; 28: 2695-2705.10.1016/j.biomaterials.2006.12.033 ↗
16. 16) ten Cate JM, Duijsters PP. Alternating demineralization and remineralization of artificial enamel lesions. Caries Res 1982; 16: 201-210.10.1159/000260599 ↗
17. 17) Thompson GA. Influence of relative layer height and testing method on the failure mode and origin in a bilayered dental ceramic composite. Dent Mater 2000; 16: 235-243.10.1016/S0109-5641(00)00005-1 ↗
18. 18) Garvie RC, Nicholson PS. Phase analysis in zirconia systems. J Am Ceram Soc 1972; 55: 303-305.10.1111/j.1151-2916.1972.tb11290.x ↗
19. 19) Toraya H, Yoshimura M, Sōmiya S. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-ray diffraction. J Am Ceram Soc 1984; 67: 119- 121.10.1111/j.1151-2916.1984.tb19614.x ↗
20. 20) Heffernan MJ, Aquilino SA, Diaz-Arnold AM, Haselton DR, Stanford CM, Vargas MA. Relative translucency of six allceramic systems. Part I: core materials. J Prosthet Dent 2002; 88: 4-9.10.1067/mpr.2002.126794 ↗
21. 21) Heffernan MJ, Aquilino SA, Diaz-Arnold AM, Haselton DR, Stanford CM, Vargas MA. Relative translucency of six all-ceramic systems. Part II: core and veneer materials. J Prosthet Dent 2002; 88: 10-15.10.1067/mpr.2002.126795 ↗
22. 22) Lin JD, Duh JG. Fracture toughness and hardness of ceria- and yttria-doped tetragonal zirconia ceramics. Mater Chem Phys 2002; 78: 253-261.
23. 23) McLaren EA. All-ceramic alternatives to conventional metalceramic restorations. Compend Contin Educ Dent 1998; 19: 307-325.
24. 24) Koutayas SO, Vagkopoulou T, Pelekanos S, Koidis P, Strub JR. Zirconia in dentistry: part 2. Evidence-based clinical breakthrough. Eur J Esthet Dent 2009; 4: 348-380.
25. 25) Featherstone JD. Modeling the caries-inhibitory effects of dental materials. Dent Mater 1996; 12: 194-197.10.1016/S0109-5641(96)80021-2 ↗
26. 26) Itthagarun A, Wei SH, Wefel JS. Morphology of initial lesions of enamel treated with different commercial dentifrices using a pH cycling model: scanning electron microscopy observations. Int Dent J 1999; 49: 352-360.10.1111/j.1875-595X.1999.tb00537.x ↗
27. 27) Thylstrup A, Fejerskov O. Textbook of clinical cariology. 2nd ed. Copenhagen: Munksgaard; 1994. p. 17-43
28. 28) Beuer F, Edelhoff D, Gernet W, Naumann M. Parameters affecting retentive force of electroformed double-crown systems. Clin Oral Investig 2010; 14: 129-135.10.1007/s00784-009-0271-7 ↗
29. 29) Pellecchia R, Kang KH, Hirayama H. Fixed partial denture supported by all-ceramic copings: a clinical report. J Prosthet Dent 2004; 92: 220-223.10.1016/j.prosdent.2004.06.006 ↗
30. 30) Rösch R, Mericske-Stern R. Zirkoniumdioxid in der abnehmbaren Prothetik. Schweiz Monatsschr Zahnmed 2008; 118: 959-966.
31. 31) Stamouli K, Smeekens S. Rehabilitation of a periodontally compromised case using the conical crown system. Part II. Eur J Esthet Dent 2009; 4: 164-176.
32. 32) Guazzato M, Proos K, Quach L, Swain MV. Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics. Biomaterials 2004; 25: 5045-5052.10.1016/j.biomaterials.2004.02.036 ↗
33. 33) Guazzato M, Proos K, Sara G, Swain MV. Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics. Int J Prosthodont 2004; 17: 142-149.
34. 34) Chevalier J. What future for zirconia as a biomaterial? Biomaterials 2006; 27: 535-543.10.1016/j.biomaterials.2005.07.034 ↗
35. 35) Roy ME, Whiteside LA, Katerberg BJ, Steiger JA, Nayfeh T. Not all zirconia femoral heads degrade in vivo. Clin Orthop Relat Res 2007; 465: 220-226.10.1097/BLO.0b013e318158b4d3 ↗
36. 36) Lawson S. Environmental degradation of zirconia ceramics. J Eur Ceram Soc 1995; 15: 485-502.10.1016/0955-2219(95)00035-S ↗
37. 37) Sato T, Shimada M. Transformation of yttria-doped tetragonal ZrO2 polycrystals by annealing in water. J Am Ceram Soc 1985; 68: 356-359.10.1111/j.1151-2916.1985.tb15239.x ↗
38. 38) Sato T, Shimada M. Crystalline phase change in yttriapartially-stabilized zirconia by low-temperature annealing. J Am Ceram Soc 1984; 67: 212-213.10.1111/j.1151-2916.1984.tb19668.x ↗
39. 39) Lilley E. Review of low temperature degradation in Y-TZPs. In: Tressler RE, McNallan M, editors. Ceramic transaction: corrosion and corrosive degradation of ceramics. Westerville: American Ceramics Society; 1990. p. 387-407.
40. 40) Fang Q, Sidky PS, Hocking MG. Erosion and corrosion of PSZ-zirconia and the t–m phase transformation. Wear 1999; 233-235: 615-622.10.1016/S0043-1648(99)00239-2 ↗
41. 41) Novak S, Kalin M. The effect of pH on the wear of waterlubricated alumina and zirconia ceramics. Tribol Lett 2004; 17: 727-732.10.1007/s11249-004-8080-2 ↗
42. 42) Papanagiotou HP, Morgano SM, Giordano RA, Pober R. In vitroevaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics. J Prosthet Dent 2006; 96: 154-164.10.1016/j.prosdent.2006.08.004 ↗
43. 43) Bona AD, Anusavice KJ, DeHoff PH. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures. Dent Mater 2003; 19: 662-669.10.1016/S0109-5641(03)00010-1 ↗