Influence of surface treatment on bond strength of veneering ceramics fused to zirconia

Kouki TADA, Toru SATO, Masao YOSHINARI

Dental Materials Journal· Volume 31· Issue 2

Abstract

In all-ceramic restorations involving a zirconia framework, surface treatment of the zirconia surface is required to enhance bonding strength with the veneering ceramics and thus prevent chipping. The purpose of the present study was to investigate the influence of surface roughness and heat treatment of the zirconia and use of liner porcelain on bond strength between veneering ceramics and a zirconia framework. Debonding/crack-initiation strength (τb) was determined according to ISO 9693. No significant difference was observed among conditions, except with use of a liner under heat treatment, which yielded a τb of 26.0±2.9-28.9±1.7 MPa. Electron probe microanalysis revealed that components of the veneering ceramics remained on the zirconia surface after debonding, suggesting that fractures occur in the veneering ceramics and that improving the strength of the veneering ceramics themselves might increase bond strength.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Building materials and conservation · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Division of Oral Implants Research, Oral Health Science Center, Tokyo Dental Collage

Department of Crown & Bridge Prosthodontics, Tokyo Dental Collage

References (31)

Show source-provided references
1. 1) Sturzenegger B, Fehér A, Lüthy H, Schärer P, Gauckler LJ. Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM). Int J Comp Dent 2001; 4: 89-106.
2. 2) Lüthy H, Filser F, Loeffel O, Schuhmacher M, Gauckler LJ, Hämmerle CHF. Strength and reliability of four unit all-ceramic posterior bridges. Dent Mater 2005; 21: 930-937.10.1016/j.dental.2004.11.012 ↗
3. 3) Sailer I, Fehér A, Filser F, Lüthy H, Gauckler LJ, Schärer P, Hämmerle CHF. Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up. Quintessence Int 2006; 37: 41-49.
4. 4) Sailer I, Fehér A, Filser F, Gauckler LJ, Lüthy H, Hämmerle CHF. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont 2007; 20: 383-388.
5. 5) Scurria MS, Bader JD, Shugars DA. Meta-analysis of fixed partial denture survival: Protheses and abutments. J Prosthet Dent 1998; 79: 459-464.10.1016/S0022-3913(98)70162-3 ↗
6. 6) Creugers NHJ, Kayser AF, van’t Hof MA. A meta analysis of durability data on conventional fixed bridges. Community Dent Oral Epidemiol 1994; 22: 448-452.10.1111/j.1600-0528.1994.tb00795.x ↗
7. 7) Shehri S, Mohammed H, Wilson CA. Influence of lamination on the flexure strength of dental castable ceramic. J Prosthet Dent 1996; 76: 23-28.10.1016/S0022-3913(96)90341-8 ↗
8. 8) Isgro G, Pallav P, Jef M, Feilzer AJ. The influence of the veneering porcelain and different surface treatments on the biaxial flexure strength of a heat-pressed ceramic. J Prosthet Dent 2003; 90: 465-473.10.1016/j.prosdent.2003.08.003 ↗
9. 9) De Jager N, Pallav P, Feilzer AJ. The influence of design parameters on the FEA-determined stress distribution in CAD-CAM produced all-ceramic crowns. Dent Mater 2005; 21: 242-251.10.1016/j.dental.2004.03.013 ↗
10. 10) Fischer J, Grohmann P, Stawarczyk B. Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composite. Dent Mater J 2008; 27: 448-454.10.4012/dmj.27.448 ↗
11. 11) Ban S, Sato H, Yamashita D. Bonding strength of zirconia to veneering porcelains. J J Dent Mater 2006 Oct 28-29; Nagoya, Japan. Tokyo: JSDMD; 2006. p.387.
12. 12) Yoshida K, Doi M, Atsuta M. Influence of surface treatments on properties of zirconia core. IADR 86th; 2008 July 2-8; Toronto, Ontario. Exhibition 2315.
13. 13) Luthardt RG, Sandkuhl O, Reitz B. Zirconia-TZP and Alumina-advanced technologies for the manufacturing of single crowns. Eur J Prosthodont Rest Dent 1999; 7: 113-119.
14. 14) Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering ceramics. Dent Mater 2006; 22: 857-863.10.1016/j.dental.2005.11.014 ↗
15. 15) Nakamura T, Wakabayashi K, Zaima C, Nishida H, Kinuta S, Yatani H. Tensile bond strength between colored-porcelain and sandblasted zirconia framework. J Prosthodont Res 2009; 53: 116-119.10.1016/j.jpor.2009.02.007 ↗
16. 16) Kosmac T, Oblack C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramics. Dent Mater 1999; 15: 116-119.10.1016/S0109-5641(99)00070-6 ↗
17. 17) Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 2005; 33: 9-18.10.1016/j.jdent.2004.07.001 ↗
18. 18) Fischer J, Stawarczyk B. Compatibility of machined Ce-TZP/Al2O3 nanocomposite and a veneering ceramic. Dent Mater 2007; 23: 1500-1505.10.1016/j.dental.2007.01.005 ↗
19. 19) Shofu veneering material VintageZR manuals, Shofu, Kyoto, Japan.
20. 20) Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Effect of zirconia type on its bond strength with different veneer ceramics. J Prosthodont 2008; 17: 401-408.10.1111/j.1532-849X.2008.00306.x ↗
21. 21) ISO9693; Metal-ceramic dental restorative systems, 1999.
22. 22) Garvie RC, Nicholson PS. Phase Analysis in zirconia systems. J Am Ceram Soc 1972; 55: 303-305.10.1111/j.1151-2916.1972.tb11290.x ↗
23. 23) Lenz J, Schwarz S, Schwickerath H, Sperner F, Schafer A. Bond strength of metal-ceramic system in three point flexure bond test. J Appl Biomater 1995; 6: 55-64.10.1002/jab.770060108 ↗
24. 24) Kizuki Y, Fukui Y, Ogura R, Kumagae N, Komada W, Kawashima K. Bond strength of porcelain to Ce-TZP/Al2O3 Nanocomposite framework. IADR 87th; 2009 Apr 1-4; Miami, Florida. Exhibition 1868.
25. 25) Guess PC, Kulis A, Witkowski S, Wolkewitz M, Zhang Y, Strub JR. Shear bond strength between deferent zirconia cores and veneering ceramics and their susceptibility to thermocycling. Dent Mater 2008; 24: 1556-1567.10.1016/j.dental.2008.03.028 ↗
26. 26) Fischer J, Stawarzcyk B, Trottmann A, Hammerle CHF. Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites. Dent Mater 2009; 25: 419-423.10.1016/j.dental.2008.09.003 ↗
27. 27) Kim ST, Cho HJ, Lee YK, Choi SH, Moon HS. Bond strength of Y-TZP-zirconia ceramics subjected various surface roughening methods and layering porcelain. Surf Interface Anal 2010; 42: 576-580.10.1002/sia.3209 ↗
28. 28) Ban S, Sato H, Nawa M, Suehiro Y, Nakanishi H. Effect of sandblasting and heat treatment on biaxial flexure strength of zirconia/alumina nanocomposite. Key Eng Mater 2007; 353-356.10.4028/www.scientific.net/KEM.330-332.353 ↗
29. 29) Sato H, Ban S, Nawa M, Suehiro Y, Nakanishi H. Effect of grinding, sandblasting and heat treatment on the phase transformation of zirconia surface. Key Eng Mater 2007; 1263-1266.10.4028/www.scientific.net/KEM.330-332.1263 ↗
30. 30) Fisher J, Grohmann P, Stawarczyk B. Effect of zirconia surface treatment on the shear strength of zirconia/veneering ceramic composites. Dent Mater J 2008; 27: 448-454.10.4012/dmj.27.448 ↗
31. 31) Denry IL, Peacock JJ, Holloway JA. Effect of heat treatment after accelerated aging on phase transformation in 3Y-TZP. J Biomed Mater Res 2010; 93B: 238-243.10.1002/jbm.b.31580 ↗