Corrosion Behavior of Dental Alloys in Various Types of Electrolyzed Water
Source abstract
Abstract
The corrosion behavior of dental alloys was examined in electrolyzed strong acid water, weak acid water and neutral water using a 7-day immersion test. The precious metal alloys, gold alloy. Au-Ag-Pd alloy and silver alloy showed the greatest surface color change and dissolution of constituents in the strong acid water and the smallest in the neutral water. The release of Au from gold alloy was especially marked in the strong acid water. Co-Cr alloy showed greater corrosion and tarnish resistance in the strong acid water rather than in the weak acid water and the neutral water. X-ray microanalysis revealed that the corrosion products on the precious metal alloys were silver chloride crystals and the thin brown products on Co-Cr alloy were cobalt and chromium oxides. Ti was sound in all three types of electrolyzed water. The neutral water appeared the least corrosive to metals among the three types showing equivalent bactericidal activity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Halal products and consumer behavior · Advanced Chemical Sensor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.