Mechanical properties of dental Ti-Ag alloys with 22.5, 25, 27.5, and 30 mass% Ag
Source abstract
Abstract
The mechanical properties -tensile strength, yield strength, elongation after fracture, Vickers hardness, and Young's modulus-and the phases of Ti-Ag alloys were investigated, as prepared with 22.5, 25, 27.5, and 30 mass% Ag. The tensile strength, yield strength, hardness, and Young's modulus of the alloys increase with their Ag content up to 25 mass%, but their breaking elongation decreases. These changes in the mechanical properties are attributed to solid-solution strengthening of the α-titanium phase, to Ti2Ag precipitation, and to the formation of eutectic structures composed of α+Ti2Ag. The addition of Ag, at 25 mass% in particular, improves the mechanical properties of these alloys, making them suitable for high strength dental prostheses, such as implantretained superstructures and narrow-diameter implants.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Division of Dental Biomaterials, Tohoku University Graduate School of Dentistry
Department of Biomaterials Science, Kagoshima University Graduate School of Medical and Dental Sciences
References (22)
Show source-provided references
1. 1) ASM Committee on titanium and titanium alloys. Introduction to titanium and its alloys, Metals Handbook 9th ed Vol. 3 Properties and selection: Stainless steels, tool materials and special-purpose metals, ASM Int, Metals Park, 1980, p. 353-360.
2. 2) ISO 22674, Dentistry —Metallic materials for fixed and removable restorations and appliances. ISO, Switzerland, 2006, p. 1-22.
3. 3) Takahashi M, Kikuchi M, Takada Y, Okuno O. Mechanical properties and microstructures of dental cast Ti-Ag and Ti Cu alloys. Dent Mater J 2002; 21: 270-280.10.4012/dmj.21.270 ↗
4. 4) Kikuchi M, Takahashi M, Okuno O. Elastic moduli of cast TiAu, Ti-Ag, and Ti-Cu alloys. Dent Mater 2006; 22: 641-646.10.1016/j.dental.2005.05.015 ↗
5. 5) ANSI/ADA Specification No. 5, Dental casting alloys. ADA, Illinois, 1997, p.1-12.
6. 6) Yoda M, Konno T, Takada Y, Iijima K, Griggs J, Okuno O, Kimura K, Okabe T. Bond strength of binary titanium alloys to porcelain. Biomaterials 2001; 22: 1675-1681.10.1016/S0142-9612(00)00329-X ↗
7. 7) Chandler HE. Machining of reactive metals. Metals Handbook 9th ed. Vol.16 Machining, ASM Int, Metals Park, 1989, p. 844-847.10.31399/asm.hb.v16.a0002189 ↗
8. 8) Kikuchi M, Takahashi M, Okabe T, Okuno O. Grindability of dental cast Ti-Ag and Ti-Cu alloys. Dent Mater J 2003; 22: 191-205.10.4012/dmj.22.191 ↗
9. 9) Kasahara H, Sato H, Kameyama Y, Sato H, Oyaizu Y, Shimpo R, Tooe S, Takahashi M. Precision polishing of purity titanium and Ti-Ag alloys for dentistry. J Jpn Soc Abrasive Technol 2014; 58: 777-778.
10. 10) Kikuchi M, Takahashi M, Okuno O. Machinability of experimental Ti-Ag alloys. Dent Mater J 2008; 27: 216-220.10.4012/dmj.27.216 ↗
11. 11) Inagaki R, Yoda M, Kikuchi M, Kimura K, Okuno O. Machinability evaluation of a Ti-Ag alloy using a dental CAD/CAM. J Dent Res 2008; 87B: 1830.
12. 12) Nakajo K, Takahashi M, Kikuchi M, Takada Y, Okuno O, Sasaki K, Takahashi N. Inhibitory effect of Ti-Ag alloy on artificial biofilm formation. Dent Mater J 2014; 33: 389-393.10.4012/dmj.2013-334 ↗
13. 13) Takahashi M, Kikuchi M, Hatori K, Orii Y, Sasaki K, Takada Y. Calcium phosphate formation on Ti-Ag alloys in simulated body fluid. J Biomech Sci Eng 2009; 4: 318-325.10.1299/jbse.4.318 ↗
14. 14) Takahashi M, Kikuchi M, Takada Y, Okabe T, Okuno O. Electrochemical behavior of cast Ti-Ag alloys. Dent Mater J 2006; 25: 516-523.10.4012/dmj.25.516 ↗
15. 15) Takahashi M, Kikuchi M, Takada Y, Okuno O. Corrosion resistance of dental Ti-Ag alloys in NaCl solution. Mater Trans 2010; 51: 762-766.10.2320/matertrans.M2009355 ↗
16. 16) Takahashi M, Kikuchi M, Takada Y. Corrosion behavior of Ti-Ag alloys used in dentistry in lactic acid solution. Met Mater Int 2011; 17: 175-179.10.1007/s12540-011-0224-y ↗
17. 17) Han MK, Hwang MJ, Won DH, Kim YS, Song HJ, Park YJ. Massive transformation in titanium-silver alloys and its effect on their mechanical properties and corrosion behavior. Materials 2014; 7: 6194-6206.10.3390/ma7096194 ↗
18. 18) Murray JL, Bhansali KJ. The Ag-Ti system, Phase diagrams of binary titanium alloys, ASM Int, Materials Park, 1987, p. 6-11.
19. 19) Kikuchi M, Takada Y, Kiyosue S, Yoda M, Woldu M, Cai Z, Okuno O, Okabe T. Mechanical properties and microstructures of cast Ti-Cu alloys. Dent Mater 2003; 19: 174-181.10.1016/S0109-5641(02)00027-1 ↗
20. 20) Takahashi M, Kikuchi M, Takada Y, Okuno O, Okabe T. Corrosion behavior and microstructures of experimental cast Ti-Au alloys. Dent Mater J 2004; 23: 109-116.10.4012/dmj.23.109 ↗
21. 21) Takahashi M, Kikuchi M, Okuno O. Mechanical properties and grindability of experimental Ti-Au alloys. Dent Mater J 2004; 23: 203-210.10.4012/dmj.23.203 ↗
22. 22) O’Brien WJ. Tabulated values of physical and mechanical properties, Dental materials and their selection 3rd ed, Quintessence, Illinois, 2002, p. 309-385.