journal article·2023-11-25Open access

Effect of translucency and absorbance of composite on temperature change during photopolymerization

Chang-Ha LEE, In-Bog LEE

Dental Materials Journal· Volume 42· Issue 6

Abstract

This study investigated the effect of translucency and absorbance of conventional (FiltekTM-Z350-XT) and bulk-fill (Tetric®-N-Ceram) composites on temperature change during photopolymerization, using a non-contact infrared sensor. Three shades from each composite were selected to prepare disk-shaped specimens (n=3), which then photopolymerized with LED-light for 20 s. A second light exposure was performed on the photopolymerized specimens. The first peak temperature rise during composite photopolymerization (ΔTtotal), second peak temperature rise by the light (ΔTlight), and net peak temperature rise by composite curing heat (ΔTcomposite) were obtained from the temperature change vs. time curve. The changes in ΔTtotal and ΔTlight with varying the composite shade were greater than those in ΔTcomposite. The conventional composite showed higher ΔTtotal and ΔTlight than bulk-fill composite. ΔTtotal and ΔTlight increased as translucency parameter decreased, and absorbance increased. The potential risk for heat-induced pulpal damage should be considered when selecting a composite shade, especially for deep cavities.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Building materials and conservation · 3D Surveying and Cultural Heritage

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Conservative Dentistry, School of Dentistry and Dental Research Institute, Seoul National University

References (30)

Show source-provided references
1. 1) McCabe JF. Cure performance of light-activated composites by differential thermal analysis (DTA). Dent Mater 1985; 1: 231-234.10.1016/S0109-5641(85)80048-8 ↗
2. 2) Al-Qudah AA, Mitchell CA, Biagioni PA, Hussey DL. Effect of composite shade, increment thickness and curing light on temperature rise during photocuring. J Dent 2007; 35: 238-245.10.1016/j.jdent.2006.07.012 ↗
3. 3) Ozturk B, Ozturk AN, Usumez A, Usumez S, Ozer F. Temperature rise during adhesive and resin composite polymerization with various light curing sources. Oper Dent 2004; 29: 325-332.
4. 4) Lloyd CH, Joshi A, McGlynn E. Temperature rises produced by light sources and composites during curing. Dent Mater 1986; 2: 170-174.10.1016/S0109-5641(86)80030-6 ↗
5. 5) Zach L, Cohen G. Pulp response to externally applied heat. Oral Surg Oral Med Oral Pathol 1965; 19: 515-530.10.1016/0030-4220(65)90015-0 ↗
6. 6) Stewardson DA, Shortall AC, Harrington E, Lumley PJ. Thermal changes and cure depths associated with a high intensity light activation unit. J Dent 2004; 32: 643-651.10.1016/j.jdent.2004.06.007 ↗
7. 7) Atai M, Motevasselian F. Temperature rise and degree of photopolymerization conversion of nanocomposites and conventional dental composites. Clin Oral Investig 2009; 13: 309-316.10.1007/s00784-008-0236-2 ↗
8. 8) Vaidyanathan J, Vaidyanathan TK, Wang Y, Viswanadhan T.Thermoanalytical characterization of visible light cure dental composites. J Oral Rehabil 1992; 19: 49-64.10.1111/j.1365-2842.1992.tb01590.x ↗
9. 9) Asmussen E, Peutzfeldt A. Temperature rise induced by some light emitting diode and quartz-tungsten-halogen curing units. Eur J Oral Sci 2005; 113: 96-98.10.1111/j.1600-0722.2004.00181.x ↗
10. 10) Al-Qudah AA, Mitchell CA, Biagioni PA, Hussey DL. Thermographic investigation of contemporary resin-containing dental materials. J Dent 2005; 33: 593-602.10.1016/j.jdent.2005.01.010 ↗
11. 11) Kim MJ, Kim RJ, Ferracane J, Lee IB. Thermographic analysis of the effect of composite type, layering method, and curing light on the temperature rise of photo-cured composites in tooth cavities. Dent Mater 2017; 33: e373-e383.10.1016/j.dental.2017.07.007 ↗
12. 12) Jo SA, Lee CH, Kim MJ, Ferracane J, Lee IB. Effect of pulse-width-modulated LED light on the temperature change of composite in tooth cavities. Dent Mater 2019; 35: 554-563.10.1016/j.dental.2019.01.009 ↗
13. 13) Aggarwal N, Garg M, Dwarakanathan V, Gautam N, Kumar SS, Jadon RS, et al. Diagnostic accuracy of non-contact infrared thermometers and thermal scanners: A systematic review and meta-analysis. J Travel Med 2020; 27: 1-17.10.1093/jtm/taaa193 ↗
14. 14) Komori A, Ishikawa H. The effect of delayed light exposure on bond strength: Light-cured resin-reinforced glass ionomer cement vs light-cured resin. Am J Orthod Dentofacial Orthop 1999; 116: 139-145.10.1016/S0889-5406(99)70210-6 ↗
15. 15) Lee CH, Lee IB. Real-time analysis of temperature change in composite photopolymerization using non-contact infrared sensor. Korean J Dent Mater 2022; 49: 131-140.10.14815/kjdm.2022.49.4.131 ↗
16. 16) Hyun HK, Christoferson CK, Pfeifer CS, Felix C, Ferracane JL. Effect of shade, opacity and layer thickness on light transmission through a nano-hybrid dental composite during curing. J Esthet Restor Dent 2017; 29: 362-367.10.1111/jerd.12311 ↗
17. 17) Oh HJ, Lee CH, Lee IB. Real-time measurement of transmittance changes during photo-polymerization of conventional and bulk-fill composites. Dent Mater J 2022; 41: 800-807.10.4012/dmj.2022-009 ↗
18. 18) Johnston WM, Ma T, Kienle BH. Translucency parameter of colorants for maxillofacial prostheses. Int J Prosthodont 1995; 8: 79-86.
19. 19) Johnston WM, Reisbick MH. Color and translucency changes during and after curing of esthetic restorative materials. Dent Mater 1997; 13: 89-97.10.1016/S0109-5641(97)80017-6 ↗
20. 20) Wang Z, Landis FA, Giuseppetti AA, Lin-Gibson S, Chiang MY. Simultaneous measurement of polymerization stress and curing kinetics for photo-polymerized composites with high filler contents. Dent Mater 2014; 30: 1316-1324.10.1016/j.dental.2014.09.006 ↗
21. 21) Fidalgo-Pereira R, Carpio D, Torres O, Carvalho O, Silva F, Henriques B, et al. The influence of inorganic fillers on the light transmission through resin-matrix composites during the light-curing procedure: An integrative review. Clin Oral Investig 2022; 26: 5575-5594.10.1007/s00784-022-04589-5 ↗
22. 22) Arikawa H, Takahashi H, Kanie T, Ban S. Effect of various visible light photoinitiators on the polymerization and color of light-activated resins. Dent Mater J 2009; 28: 454-460.10.4012/dmj.28.454 ↗
23. 23) Bennett CO. Momentum, heat, and mass transfer. 3rd ed. Auckland: McGraw-Hill Book Company; 1983.
24. 24) Vaidyanathan J, Vaidyanathan TK. Computer-controlled differential scanning calorimetry of dental composites. IEEE Trans Biomed Eng 1991; 38: 319-325.10.1109/10.133224 ↗
25. 25) 3M ESPE. FiltekTM Z350 XT Universal Restorative System Technical Product Profile. St. Paul, MN, USA: 3M ESPE; 2010. p. 2.
26. 26) Ivoclar Vivadent AG. Scientific Documentation Tetric® N-Ceram Bulk Fill. Schaan Liechtenstein: Ivoclar Vivadent AG; 2014. p. 11-13.
27. 27) Sang EJ, Kim JY, Lim BS, Choi NS, Lee IB. Effect of initiator and inhibitor concentration on the polymerization shrinkage kinetics of experimental dental composites. Korean J Dent Mater 2014; 41: 29-38.10.14815/kjdm.2014.41.1.29 ↗
28. 28) Atai M, Watts DC, Atai Z. Shrinkage strain-rates of dental resin-monomer and composite systems. Biomaterials 2005; 26: 5015-5020.10.1016/j.biomaterials.2005.01.022 ↗
29. 29) Xu T, Li X, Wang H, Zheng G, Yu G, Wang H, et al. Polymerization shrinkage kinetics and degree of conversion of resin composites. J Oral Sci 2020; 62: 275-280.10.2334/josnusd.19-0157 ↗
30. 30) Moszner N, Fischer UK, Ganster B, Liska R, Rheinberger V. Benzoyl germanium derivatives as novel visible light photoinitiators for dental materials. Dent Mater 2008; 24: 901-907.10.1016/j.dental.2007.11.004 ↗