journal article·2019-11-26Open access

Effect of different pH environments on the durability of bonds between zirconia and Ti-6Al-4V

Xin TAN, Shanshan GAO, Beilei LIU, Jie MIN, Qianqian ZHANG, Yuwei ZHAO, Haiyang YU

Dental Materials Journal· Volume 38· Issue 6

Abstract

This study investigated the role played by different pH environments in the deterioration of bonds between Y-TZP and Ti-6Al-4V. One hundred and thirty-five specimens were randomly assigned to one of the following storage media at 37°C: (1) distilled water, pH 6.9, DW; (2) acidic solution, pH 1-2, CS; and (3) alkaline solution, pH 10-11, KS. Shear bond strength (SBS) tests were carried out at the 4-, 14-, and 30-day storage time intervals. The morphology characteristics and elements distribution of the fracture surfaces were analyzed. CS-30 showed the lowest mean SBS and the least amount of residual cement on the Ti-6Al-4V surface after the SBS tests. Bond strength tended to decrease with increasing storage time for the acidic group. Alkaline and neutral media showed little influence on the SBS of Y-TZP to Ti-6Al-4V in 30 days. Acidic environments should be properly avoided to obtain reliable long-term bonding strength between Ti-6Al-4V and Y-TZP.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Orthopaedic implants and arthroplasty · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Prosthodontics, State Key Laboratory of Oral Diseases & National Clinical Research Center for Oral Diseases, West China Hospital of Stomatology, Sichuan University

References (38)

Show source-provided references
1. 1) Revathi A, Borras AD, Munoz AI, Richard C, Manivasagam G.Degradation mechanisms and future challenges of titanium and its alloys for dental implant applications in oral environment Materials. Mater Sci Eng C Mater Biol Appl 2017; 76: 1354-1368.10.1016/j.msec.2017.02.159 ↗
2. 2) Cordeiro JM, Barão VA. Is there scientific evidence favoring the substitution of commercially pure titanium with titanium alloys for the manufacture of dental implants? Mater Sci Eng C Mater Biol Appl 2016; 71: 1201-1215.10.1016/j.msec.2016.10.025 ↗
3. 3) Yan M, Kao CT, Ye JS, Huang TH, Ding SJ. Effect of preoxidation of titanium on the titanium–ceramic bonding. Surf Coat Technol 2007; 202: 288-293.10.1016/j.surfcoat.2007.05.056 ↗
4. 4) Brägger U, Karoussis I, Persson R, Pjetursson B, Salvi G, Lang N. Technical and biological complications and failures with single crowns and fixed partial dentures on implant of the ITI® Dental Implant System. Clin Oral Implants Re 2005; 16: 326-334.10.1111/j.1600-0501.2005.01105.x ↗
5. 5) Grasel R, Santos MJ, Rego HC, Rippe MP, Valandro LF. Effect of resin luting systems and alumina particle air abrasion on bond strength to zirconia. Oper Dent 2018; 43: 282-290.10.2341/15-352-L ↗
6. 6) Llerena-Icochea AE, Costa RM, Borges A, Bombonatti J, Furuse AY. Bonding polycrystalline zirconia with 10-MDP-containing adhesives. Oper Dent 2017; 42: 335-341.10.2341/16-156-L ↗
7. 7) Wandscher VF, Prochnow C, Rippe MP, Dorneles LS, Callegari GL, Baldissara P, et al. Retentive strength of Y-TZP crowns: Comparison of different silica coating methods on the intaglio surfaces. Oper Dent 2017; 42: E121-E33.10.2341/16-090-L ↗
8. 8) Fernandes CA, Ribeiro JC, Larson BS, Bonfante EA, Silva NR, Suzuki M, et al. Microtensile bond strength of resin-based composites to Ti-6Al-4V. Dent Mater 2009; 25: 655-661.10.1016/j.dental.2008.11.012 ↗
9. 9) Xie H, Tay FR, Zhang F, Lu Y, Shen S, Chen C. Coupling of 10-methacryloyloxydecyldihydrogenphosphate to tetragonal zirconia: Effect of pH reaction conditions on coordinate bonding. Dent Mater 2015; 31: 218-225.10.1016/j.dental.2015.06.014 ↗
10. 10) Fonseca RG, de Almeida JG, Haneda IG, Adabo GL. Effect of metal primers on bond strength of resin cements to base metals. J Prosthet Dent 2009; 101: 262-268.10.1016/S0022-3913(09)60050-0 ↗
11. 11) Chen C, Chen Y, Lu Z, Qian M, Xie H, Tay FR. The effects of water on degradation of the zirconia-resin bond. J Dent 2017; 64: 23-29.10.1016/j.jdent.2017.04.004 ↗
12. 12) da Silva EM, Goncalves L, Guimaraes JG, Poskus LT, Fellows CE. The diffusion kinetics of a nanofilled and a midifilled resin composite immersed in distilled water, artificial saliva, and lactic acid. Clin Oral Investig 2011; 15: 393-401.10.1007/s00784-010-0392-z ↗
13. 13) Marghalani HY. Sorption and solubility characteristics of self-adhesive resin cements. Dent Mater 2012; 28: 187-198.10.1016/j.dental.2012.04.037 ↗
14. 14) Sano H, Yoshikawa T, Pereira PN, Kanemura N, Morigami M, Tagami J, et al. Long-term durability of dentin bonds made with a self-etching primer, in vivo. J Dent Res 1999; 78: 906-911.10.1177/00220345990780041101 ↗
15. 15) Cilli R, Pereira JC, Prakki A. Properties of dental resins submitted to pH catalysed hydrolysis. J Dent 2012; 40: 1144-1150.10.1016/j.jdent.2012.09.012 ↗
16. 16) Gopferich A. Mechanisms of polymer degradation and erosion. Biomaterials 1996; 17: 103-114.10.1016/0142-9612(96)85755-3 ↗
17. 17) Ping Y, Zhou X, Arola DD, Jie M, Peng Z, Gao S. Effect of acidic agents on the wear behavior of a polymer infiltrated ceramic network (PICN) material. J Mech Behav Biomed Mater 2017; 74: 154-163.10.1016/j.jmbbm.2017.06.001 ↗
18. 18) Sulaiman TA, Abdulmajeed AA, Shahramian K, Hupa L, Donovan TE, Vallittu P, et al. Impact of gastric acidic challenge on surface topography and optical properties of monolithic zirconia. Dent Mater 2015; 31: 1445-1452.10.1016/j.dental.2015.09.010 ↗
19. 19) de Gee AJ, Wendt SL, Werner A, Davidson CL. Influence of enzymes and plaque acids on in vitro wear of dental composites. Biomaterials 1996; 1317: 1327.10.1016/0142-9612(96)88679-0 ↗
20. 20) Schneider R, de Goes MF, Henriques GE, Chan DC. Tensile bond strength of dual curing resin-based cements to commercially pure titanium. Dent Mater 2007; 23: 81-87.10.1016/j.dental.2005.12.006 ↗
21. 21) Yanagida H, Matsumura H, Taira Y, Atsuta M, Shimoe S. Adhesive bonding of composite material to cast titanium with varying surface preparations. J Oral Rehabil 2002; 29: 121-126.10.1046/j.1365-2842.2002.00811.x ↗
22. 22) Yanagida H, Matsumura H, Atsuta M. Bonding of prosthetic composite material to Ti-6Al-7Nb alloy with eight metal conditioners and a surface modification technique. Am J Dent 2001; 14: 291.
23. 23) Taira Y, Matsumura H, Yoshida K, Tanaka T, Atsuta M. Influence of surface oxidation of titanium on adhesion. J Dent 1998; 26: 69-73.10.1016/S0300-5712(96)00072-3 ↗
24. 24) Ohno H, Endo K, Yamane Y, Kawashima I. Adhesion of adhesive resin to dental precious metal alloys. Part II. The relationship between surface structure of Au-In alloys and adhesive ability with 4-META resin. Dent Mater J 1998; 17: 285-293.10.4012/dmj.17.285 ↗
25. 25) Mertens T, Gammel FJ, Kolb M, Rohr O, Kotte L, Tschöcke S, et al. Investigation of surface pre-treatments for the structural bonding of titanium. Int J Adhes Adhes 2012; 34: 46-54.10.1016/j.ijadhadh.2011.12.007 ↗
26. 26) Hibino Y, Kuramochi K, Hoshino T, Moriyama A, Watanabe Y, Nakajima H. Relationship between the strength of glass ionomers and their adhesive strength to metals. Dent Mater 2002; 18: 552-527.10.1016/S0109-5641(01)00086-0 ↗
27. 27) Ferracane JL. Hygroscopic and hydrolytic effects in dental polymer networks. Dent Mater 2006; 22: 211-222.10.1016/j.dental.2005.05.005 ↗
28. 28) Oyague RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R. Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconiumoxide ceramics. Dent Mater 2009; 25: 392-399.10.1016/j.dental.2008.09.002 ↗
29. 29) Ortengren U, Andersson F, Elgh U, Terselius B, Karlsson S. Influence of pH and storage time on the sorption and solubility behaviour of three composite resin materials. J Dent 2001; 29: 35-41.10.1016/S0300-5712(00)00055-5 ↗
30. 30) Yiu CK, King NM, Pashley DH, Suh BI, Carvalho RM, Carrilho MR, et al. Effect of resin hydrophilicity and water storage on resin strength. Biomaterials 2004; 25: 5789-5796.10.1016/j.biomaterials.2004.01.026 ↗
31. 32) Kuo SW, Chan SC, Hewder Wu A, Chang FC. An unusual, completely miscible, ternary hydrogen-bonded polymer blend of phenoxy, phenolic, and PCL. Macromolecules 2005; 38: 4729-4736.10.1021/ma047371a ↗
32. 33) Kuo SW. Hydrogen-bonding in polymer blends. J Polym Res 2008; 15: 459-486.10.1007/s10965-008-9192-4 ↗
33. 34) Prakki A, Cilli R, Mondelli RF, Kalachandra S, Pereira JC. Influence of pH environment on polymer based dental material properties. J Dent 2005; 33: 91-98.10.1016/j.jdent.2004.08.004 ↗
34. 35) Munchow EA, Ferreira AC, Machado RM, Ramos TS, Rodrigues-Junior SA, Zanchi CH. Effect of acidic solutions on the surface degradation of a micro-hybrid composite resin. Braz Dent J 2014; 25: 321-326.10.1590/0103-6440201300058 ↗
35. 36) Kikuchi T, Yoshida N, Shimakura M, Ohtani M, Nemoto T, Yokobori M. The clinical application of resin facing titanium crown by non-retention method. The influence of heating time on the bond strength. Nihon Hotetsu Shika Gakkai Zasshi 1997; 41: 481-488.10.2186/jjps.41.481 ↗
36. 37) Ban S. Effect of alkaline treatment of pure titanium and its alloys on the bonding strength of dental veneering resins. J Biomed Mater Res A 2003; 66: 138-145.10.1002/jbm.a.10566 ↗
37. 38) Tsuchimoto Y, Yoshida Y, Takeuchi M, Mine A, Yatani H, Tagawa Y, et al. Effect of surface pre-treatment on durability of resin-based cements bonded to titanium. Dent Mater 2006; 22: 545-552.10.1016/j.dental.2005.08.002 ↗
38. 39) Yap AU, Tan SH, Wee SS, Lee CW, Lim EL, Zeng KY. Chemical degradation of composite restoratives. J Oral Rehabil 2001; 28: 1015-1021.10.1046/j.1365-2842.2001.00760.x ↗