The impact of etching time and material on bond strength of self-adhesive resin cement to eroded enamel

Samah SAKER, Mutlu ÖZCAN, Walid AL-ZORDK

Dental Materials Journal· Volume 38· Issue 6

Abstract

The purpose of this study was to assess the effect of pre-etching time and material on shear bond strength (SBS) of self-adhesive resin cements to eroded and sound enamel. Eroded enamel specimens were assigned into 5 groups (n=20 each) based on enamel surface treatment as follow: Group N, eroded enamel (without surface pre-treatment); Group PH15, 35% H3PO4 etching for 15 s; Group PH30, 35% H3PO4 etching for 30 s; Group L30, 20% lactic acid etching for 30 s and Group L60, 20% lactic acid etching for 60 s.Composite blocks were fabricated and cemented to enamel surfaces with one of two self-adhesive cements. Notched-edge SBS was assessed. Bond strength of self-adhesive cement to eroded enamel surface significantly enhanced following application of 20% lactic acid for 30 s.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Fixed Prosthodontics Department, Faculty of Dentistry, Mansoura University

Dental Materials Unit, Center for Dental and Oral Medicine Clinic for Fixed and Removable Prosthodontics and Dental Materials Science

References (45)

Show source-provided references
1. 1) Bartlett DW. The role of erosion in tooth wear: aetiology, prevention and management. Int Dent J 2005; 55: 277-284.10.1111/j.1875-595X.2005.tb00065.x ↗
2. 2) Milosevic A. Tooth wear: an aetiological and diagnostic problem. Eur J Prosthodont Restor Dent 1993; 1: 173-178.
3. 3) Barbour ME, Rees GD. The role of erosion, abrasion and attrition in tooth wear. J Clin Dent 2006; 17: 88-93.
4. 4) Curtis DA, Jayanetti J, Chu R, Staninec M. Decision-making in the management of the patient with dental erosion. J Calif Dent Assoc 2011; 39: 259-265.10.1080/19424396.2011.12221894 ↗
5. 5) Corrêa MC, Lerco MM, Cunha Mde L, Henry MA. Salivary parameters and teeth erosions in patients with gastroesophageal reflux disease. Arq Gastroenterol 2012; 49: 214-218.10.1590/S0004-28032012000300009 ↗
6. 6) Guess Gierthmuehlen PC, Steger E. CAD/CAM solutions for minimally invasive all-ceramic rehabilitation of extended erosive lesions. Compend Contin Educ Dent 2016; 37: 340-345.
7. 7) Trivedi K, Bhaskar V, Ganesh M, Venkataraghavan K, Choudhary P, Shah S, Krishnan R. Erosive potential of commonly used beverages, medicated syrup, and their effects on dental enamel with and without restoration: An in vitro study. J Pharm Bioallied Sci 2015; 7: S474-S480.10.4103/0975-7406.163508 ↗
8. 8) Alghilan MA, Cook NB, Platt JA, Eckert GJ, Hara AT. Susceptibility of restorations and adjacent enamel/dentine to erosion under different salivary flow conditions. J Dent 2015; 43: 1476-1482.10.1016/j.jdent.2015.10.007 ↗
9. 9) Patel M, Seymour D, Chan MF. Contemporary management of generalized erosive tooth surface loss. Dent Update 2013; 40: 222-4, 226-9.10.12968/denu.2013.40.3.222 ↗
10. 10) Briso AL, Caruzo LP, Guedes AP, Catelan A, dos Santos PH. In vitro evaluation of surface roughness and microhardness of restorative materials submitted to erosive challenges. Oper Dent 2011; 36: 397-402.10.2341/10-356-L ↗
11. 11) Schlichting LH, Maia HP, Baratieri LN, Magne P. Novel-design ultra-thin CAD/CAM composite resin and ceramic occlusal veneers for the treatment of severe dental erosion. J Prosthet Dent 2011; 105: 217-226.10.1016/S0022-3913(11)60035-8 ↗
12. 12) Schlichting LH, Resende TH, Reis KR, Magne P. Simplified treatment of severe dental erosion with ultrathin CAD-CAM composite occlusal veneers and anterior bilaminar veneers. J Prosthet Dent 2016; 116: 474-482.10.1016/j.prosdent.2016.02.013 ↗
13. 13) Schepke U, Cune MS. Noninvasive restoration of severe erosion by means of CAD/CAM indirect composite occlusal restorations: a technical note. Int J Prosthodont 2014; 27: 134-136.10.11607/ijp.3768 ↗
14. 14) Dietschi D, Argente A. A comprehensive and conservative approach for the restoration of abrasion and erosion. part II: clinical procedures and case report. Eur J Esthet Dent 2011; 6: 142-159.
15. 15) Moazzez R, Bartlett D, Anggiansah A. Dental erosion, gastro-oesophageal reflux disease and saliva: how are they related? J Dent 2004; 32: 489-494.10.1016/j.jdent.2004.03.004 ↗
16. 16) Eades R. Conservative treatment of tooth wear to improve function and aesthetics. Prim Dent J 2013; 2: 56-60.10.1308/205016814809859581 ↗
17. 17) Eliyas S, Martin N. The management of anterior tooth wear using gold palatal veneers in canine guidance. Br Dent J 2013; 214: 291-297.10.1038/sj.bdj.2013.273 ↗
18. 18) Reston EG, Closs LQ, Busato AL, Broliato GA, Tessarollo FR. Restoration of occlusal vertical dimension in dental erosion caused by gastroesophageal reflux: case report. Oper Dent 2010; 35: 125-129.10.2341/09-110T ↗
19. 19) Dietschi D, Argente A. A comprehensive and conservative approach for therestoration of abrasion and erosion. Part I: concepts and clinical rationale for early intervention using adhesive techniques. Eur J Esthet Dent 2011; 6: 20-33.
20. 20) Gulamali AB, Hemmings KW, Tredwin CJ, Petrie A. Survival analysis of composite Dahl restorations provided to manage localised anterior tooth wear (ten year follow-up). Br Dent J 2011; 211: E9.10.1038/sj.bdj.2011.683 ↗
21. 21) Reis A, Higashi C, Loguercio AD. Re-anatomization of anterior eroded teeth by stratification with direct composite resin. J Esthet Restor Dent 2009; 21: 304-316.10.1111/j.1708-8240.2009.00281.x ↗
22. 22) Vailati F, Belser UC. Classification and treatment of the anterior maxillary dentition affected by dental erosion: the ACE classification. Int J Periodontics Restorative Dent 2010; 30: 559-571.
23. 23) Fradeani M, Barducci G, Bacherini L. Esthetic rehabilitation of a worn dentition with a minimally invasive prosthetic procedure (MIPP). Int J Esthet Dent 2016; 11: 16-35.
24. 24) Vailati F, Carciofo S. CAD/CAM monolithic restorations and full-mouth adhesive rehabilitation to restore a patient with a past history of bulimia: the modified three-step technique. Int J Esthet Dent 2016; 11: 36-56.
25. 25) Vailati F, Belser UC. Palatal and facial veneers to treat severe dental erosion: a case report following the three-step technique and the sandwich approach. Eur J Esthet Dent 2011; 6: 268-278.
26. 26) Manso AP, Carvalho RM. Dental cements for luting and bonding restorations: Self-adhesive resin cements. Dent Clin North Am 2017; 61: 821-83410.1016/j.cden.2017.06.006 ↗
27. 27) Canay S, Kocadereli I, Akca E. The effect of enamel air abrasion on the retention of bonded metallic orthodontic brackets. Am J Orthod Dentofacial Orthop 2000; 117: 15-19.10.1016/S0889-5406(00)70243-5 ↗
28. 28) Chang WG, Lim BS, Yoon TH, Lee YK, Kim CW. Effects of salicylic-lactic acid conditioner on the shear bond strength of brackets and enamel surfaces. J Oral Rehabil 2005; 32: 287-295.10.1111/j.1365-2842.2004.01416.x ↗
29. 29) Sussenberger U, Cacciafesta V, Jost-Brinkmann PG. Light cured glass ionomer cement as a bracket adhesive with different types of enamel conditioners. J Orofac Orthop 1997; 58: 174-180.
30. 30) Urabe H, Rossouw PE, Titley KC, Yamin C. Combinations of etchants, composite resins, and bracket systems: an important choice in orthodontic bonding procedures. Angle Orthod 1999; 69: 267-275.
31. 31) Ayad MF, Rosenstiel SF, Farag AM. A pilot study of lactic acid as an enamel and dentin conditioner for dentin-bonding agent development. J Prosthet Dent 1996; 76: 254-259.10.1016/S0022-3913(96)90168-7 ↗
32. 32) Ayad MF, Farag AM, Garcia-Godoy F. Effect of lactic acid irrigant on shear bond strength of Epiphany adhesive sealer to human dentin surface. Oral Surg Oral Med Oral Pathol Oral Radiol Endod 2010; 109: e100-106.10.1016/j.tripleo.2009.12.050 ↗
33. 33) Chuenarrom C, Benjakul P, Daosodsai P. Effect of indentation load and time on knoop and Vickers microhardness tests for enamel and dentin. Mater Res 2009; 12: 473-476.10.1590/S1516-14392009000400016 ↗
34. 34) Mann C, Ranjitkar S, Lekkas D, Hall C, Kaidonis J, Townsend G, Brook A. Three-dimensional prophilometric assessment of early enamel erosion simulating gastric regurgitation. J Dent 2014; 42: 1411-1421.10.1016/j.jdent.2014.06.011 ↗
35. 35) Zhao X, Pan J, Malmstrom HS, Ren YF. Protective effects of resin sealant and flowable composite coatings against erosive and abrasive wear of dental hard tissues. J Dent 2016; 49: 68-74.10.1016/j.jdent.2016.01.013 ↗
36. 36) Tsujimoto A, Iwasa M, Shimamura Y, Murayama R, Takamizawa T, Miyazaki M. Enamel bonding of single-step self etch adhesives: influence of surface free energy characteristics. J Dent 2010; 38: 123-130.10.1016/j.jdent.2009.09.011 ↗
37. 37) Tsujimoto A, Barkmeier WW, Takamizawa T, Watanabe H, Johnson WW, Latta MA, Miyazaki M. Influence of duration of phosphoric acid pre-etching on bond durability of universal adhesives and surface free-energy characteristics of enamel. Eur J Oral Sci 2016; 124: 377-386.10.1111/eos.12284 ↗
38. 38) Tsujimoto A, Barkmeier WW, Takamizawa T, Latta MA, Miyazaki M. The effect of phosphoric acid pre-etching times on bonding performance and surface free energy with single-step self-etch adhesives. Oper Dent 2016; 41: 441-449.10.2341/15-221-L ↗
39. 39) Nagura Y, Tsujimoto A, Barkmeier WW, Watanabe H, Johnson WW, Takamizawa T, Latta MA, Miyazaki M. Relationship between enamel bond fatigue durability and surface free-energy characteristics with universal adhesives. Eur J Oral Sci 2018; 126: 135-145.10.1111/eos.12398 ↗
40. 40) Lussi A, Jaeggi T. Erosion: diagnosis and risk factors. Clin Oral Investig 2008; 12: S5-13.10.1007/s00784-007-0179-z ↗
41. 41) Ganss C, Lussi A, Schlueter N. The histological features and physical properties of eroded dental hard tissues. Monogr Oral Sci 2014; 25: 99-107.10.1159/000359939 ↗
42. 42) Turssi CP, Messias DF, Corona SM, Serra MC. Viability of using enamel and dentin from bovine origin as a substitute for human counterparts in an intraoral erosion model. Braz Dent J 2010; 21: 332-336.10.1590/S0103-64402010000400008 ↗
43. 43) Lussi A, Schlueter N, Rakhmatullina E, Ganss C. Dental erosion —an overview with emphasis on chemical and histopathological aspects. Caries Res 2011; 45: 2-12.10.1159/000325915 ↗
44. 44) Milosevic A, Dawson LJ. Salivary factors in vomiting bulimics with and without pathological tooth wear. Caries Res 1996; 30: 361-366.10.1159/000262343 ↗
45. 45) Buonocore M. A simple method of increasing the adhesion of acrylic filling materials to enamel surfaces. J Dent Res 1955; 34: 849-853.10.1177/00220345550340060801 ↗