Ultrastructural observation of the acid-base resistant zone of all-in-one adhesives using three different acid-base challenges
Source abstract
Abstract
The aim of this study was to analyze the ultrastructure of the dentin-adhesive interface using two all-in-one adhesive systems (Clearfil Tri-S Bond, TB; Tokuyama Bond Force, BF) after different acid-base challenges. Three solutions were used as acidic solutions for the acid-base challenges: a demineralizing solution (DS), a phosphoric acid solution (PA), and a hydrochloric acid solution (HCl). After the acid-base challenges, the bonded interfaces were examined by scanning electron microscopy. Thickness of the acid-base resistant zone (ABRZ) created in PA and HCl was thinner than in DS for both adhesive systems. For BF adhesive, an eroded area was observed beneath the ABRZ after immersion in PA and HCl, but not in DS. Conversely for TB adhesive, the eroded area was observed only after immersion in PA. In conclusion, although the ABRZ was observed for both all-in-one adhesive systems, its morphological features were influenced by the ingredients of both the adhesive material and acidic solution.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Anxiety and Anesthesia Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. 1) Nakabayashi N. Bonding of restorative materials to dentine. Int Dent J 1985; 35: 145-154.
2. 2) Wang T, Nakabayashi N. Effect of 2-(methacryloxy)ethyl phenyl hydrogen phosphate on adhesion to dentin. J Dent Res 1991; 70: 59-66.10.1177/00220345910700011001 ↗
3. 3) Sano H, Takatsu T, Ciucchi B, Horner JA, Matthews WG, Pashley DH. Nanoleakage: leakage within the hybrid layer. Oper Dent 1995; 20: 18-25.
4. 4) Wefel JS, Heilman JR, Jordan TH. Comparisons of in vitro root caries models. Caries Res 1995; 29: 204-209.10.1159/000262070 ↗
5. 5) Gwinnett AJ, Kanca J. Interfacial morphology of resin composite and shiny erosion lesions. Am J Dent 1992; 5: 315-317.
6. 6) Nakabayashi N. Bonding mechanism of resins and the tooth. Kokubyo Gakkai Zasshi 1982; 49: 410.10.5357/koubyou.49.410 ↗
7. 7) Nakabayashi N, Saimi Y. Bonding to intact dentin. J Dent Res 1996; 75: 1706-1715.10.1177/00220345960750091401 ↗
8. 10.1177/0022034595074010090110.1177/00220345950740100901 ↗
9. 9) Inokoshi S, Hosoda H, Harnirattisai C, Shimada Y. Interfacial structure between dentin and seven dentin bonding systems revealed using argon ion beam etching. Oper Dent 1993; 18: 8-16.
10. 10) Tsuchiya S, Nikaido T, Sonoda H, Foxton RM, Tagami J. Ultrastructure of the dentin-adhesive interface after acid-base challenge. J Adhes Dent 2004; 6: 183-190.
11. 10.4012/dmj.28.18510.4012/dmj.28.185 ↗
12. 10.4012/dmj.28.71710.4012/dmj.28.717 ↗
13. 10.2341/05-6210.2341/05-62 ↗
14. 14) Waidyasekera K, Nikaido T, Weerasinghe DS, Ichinose S, Tagami J. Reinforcement of dentin in self-etch adhesive technology: a new concept. J Dent 2009; 37: 604-609.10.1016/j.jdent.2009.03.021 ↗
15. 15) Nikaido T, Weerasinghe DD, Waidyasekera K, Inoue G, Foxton RM, Tagami J. Assessment of the nanostructure of acid-base resistant zone by the application of all-in-one adhesive systems: Super dentin formation. Biomed Mater Eng 2009; 19: 163-171.10.3233/BME-2009-0576 ↗
16. 10.4012/dmj.25.54510.4012/dmj.25.545 ↗
17. 10.4012/dmj.28.49310.4012/dmj.28.493 ↗
18. 18) Ten Cate JM, Duijsters PP. Alternating demineralization and remineralization of artificial enamel lesions. Caries Res 1982; 16: 201-210.10.1159/000260599 ↗
19. 19) Waidyasekera PG, Nikaido T, Weerasinghe DD, Wettasinghe KA, Tagami J. Caries susceptibility of human fluorosed enamel and dentin. J Dent 2007; 35: 343-349.10.1016/j.jdent.2006.10.008 ↗
20. 20) Wiegand A, Stock A, Attin R, Werner C, Attin T. Impact of the acid flow rate on dentin erosion. J Dent 2007; 35: 21-27.10.1016/j.jdent.2006.04.002 ↗
21. 21) Bakry AS, Sadr A, Inoue G, Otsuki M, Tagami J. Effect of Er:YAG laser treatment on the microstructure of the dentin/adhesive interface after acid-base challenge. J Adhes Dent 2007; 9: 513-520.
22. 22) Hiraishi N, Kitasako Y, Nikaido T, Foxton RM, Tagami J, Nomura S. Detection of acidic diffusion through bovine dentine after adhesive application. Int Endod J 2004; 37: 455-462.10.1111/j.1365-2591.2004.00807.x ↗
23. 10.1177/15440591040830060410.1177/154405910408300604 ↗
24. 24) Attin T, Meyer K, Hellwig E, Buchalla W, Lennon AM. Effect of mineral supplements to citric acid on enamel erosion. Arch Oral Biol 2003; 48: 753-759.10.1016/S0003-9969(03)00156-0 ↗