journal article·2024-03-25Open access

Effect of low-temperature degradation and sintering protocols on the color of monolithic zirconia crowns with different yttria contents

Shoko MIURA, Akikazu SHINYA, Hiroyasu KOIZUMI, Pekka VALLITTU, Lippo LASSILA, Masanori FUJISAWA

Dental Materials Journal· Volume 43· Issue 2

Abstract

This study investigated the effects of low-temperature degradation (LTD) on the L*, a*, and b* values of highly translucent zirconia crowns. Four types of zirconia disks with different yttria contents (IPS e.max ZirCAD LT, IPS e.max ZirCAD MT, IPS e.max ZirCAD MT Multi, IPS e.max ZirCAD Prime, Ivoclar) and two shades (A2 and BL) were used. A crown was manufactured using four types of zirconia and LTD treated. Color measurements were performed, and the color difference (ΔE00) before and after LTD was calculated. The microstructure was determined through X-ray fluorescence and X-ray diffractometry. Highly translucent zirconia crowns showed greater changes in the a* and b* values than in the L* value after LTD, regardless of the shade. The Multi2 crowns exhibited a discernible color change due to the LTD treatment. The X-ray fluorescence results did not reveal any apparent change in the microstructure between sintering programs for all zirconia specimens.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Pigment Synthesis and Properties · Glass properties and applications · Dental materials and restorations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Division of Fixed Prosthodontics, Department of Restorative and Biomaterials Sciences, Meikai University School of Dentistry

Department of Biomaterials Science and Turku Clinical Biomaterials Center-TCBC, Institute of Dentistry, University of Turku

Department of Dental Materials Sciences, School of Life Dentistry at Tokyo, The Nippon Dental University

Department of Prosthetic Dentistry and Biomaterials Science, Institute of Dentistry, University of Turku

Department of Dental Materials, Nihon University School of Tokyo

Welfare District of County of Southwest Finland

References (45)

Show source-provided references
1. 1) Zhang Y, Lawn BR. Novel zirconia materials in dentistry. J Dent Res 2018; 97: 140-147.10.1177/0022034517737483 ↗
2. 2) Abdulmajeed A, Sulaiman T, Abdulmajeed A, Bencharit S, Närhi T. Fracture load of different zirconia types: A mastication simulation study. J Prosthodont 2020; 29: 787-791.10.1111/jopr.13242 ↗
3. 3) Kongkiatkamon S. Effect of speed sintering on low temperature degradation and biaxial flexural strength of 5Y-TZP zirconia. Molecules 2022; 27: 5272.10.3390/molecules27165272 ↗
4. 4) Miura S, Yamauchi S, Kasahara S, Katsuda Y, Fujisawa M, Egusa H. Clinical evaluation of monolithic zirconia crowns: A failure analysis of clinically obtained cases from a 3.5-year study. J Prosthodont Res 2021; 65: 148-154.10.2186/jpr.JPOR_2019_643 ↗
5. 5) Bankoğlu Güngör M, Karakoca Nemli S. Fracture resistance of CAD-CAM monolithic ceramic and veneered zirconia molar crowns after aging in a mastication simulator. J Prosthet Dent 2018; 119: 473-480.10.1016/j.prosdent.2017.05.003 ↗
6. 6) Lawson NC, Janyavula S, Syklawer S, McLaren EA, Burgess JO. Wear of enamel opposing zirconia and lithium disilicate after adjustment, polishing and glazing. J Dent 2014; 42: 1586-1591.10.1016/j.jdent.2014.09.008 ↗
7. 7) Solá-Ruiz MF, Baixauli-López M, Roig-Vanaclocha A, Amengual-Lorenzo J, Agustín-Panadero R. Prospective study of monolithic zirconia crowns: Clinical behavior and survival rate at a 5-year follow-up. J Prosthodont Res 2021; 65: 284-290.10.2186/jpr.JPR_D_20_00034 ↗
8. 8) Miura S, Kasahara S, Yamauchi S, Okuyama Y, Izumida A, Aida J, et al. Clinical evaluation of zirconia-based all-ceramic single crowns: an up to 12-year retrospective cohort study. Clin Oral Investig 2018; 22: 697-706.10.1007/s00784-017-2142-y ↗
9. 9) Kaizer MR, Gierthmuehlen PC, Dos Santos MB, Cava SS, Zhang Y. Speed sintering translucent zirconia for chairside one-visit dental restorations: Optical, mechanical, and wear characteristics. Ceram Int 2017; 43: 10999-11005.10.1016/j.ceramint.2017.05.141 ↗
10. 10) Miura S, Shinya A, Koizumi H, Fujisawa M. Effect of speed sintering of monolithic zirconia with different yttria contents on color and crystal phase. Eur J Oral Sci 2022; 130: e12898.10.1111/eos.12898 ↗
11. 11) Fathy SM, El-fallal AA, El-negoly SA, El Bedawy AB. Translucency of monolithic and core zirconia after hydrothermal aging. Acta Biomater Odontol Scand 2015; 1: 86-92.10.3109/23337931.2015.1102639 ↗
12. 12) Bergamo ETP, Silva WJ, Cesar PF, Cury ADB. Fracture load and phase transformation of monolithic zirconia crowns submitted to different aging protocols. Oper Dent 2016; 41: 118-130.10.2341/15-154-L ↗
13. 13) Lawson S. Environmental degradation of zirconia ceramics. J Eur Ceram Soc 1995; 15: 485-502.10.1016/0955-2219(95)00035-S ↗
14. 14) Hallmann L, Ulmer P, Reusser E, Louvel M, Hämmerle CHF. Effect of dopants and sintering temperature on microstructure and low temperature degradation of dental Y-TZP-zirconia. J Eur Ceram Soc 2012; 32: 4091-4104.10.1016/j.jeurceramsoc.2012.07.032 ↗
15. 15) Zhang Y. Making yttria-stabilized tetragonal zirconia translucent. Dent Mater 2014; 30: 1195-1203.10.1016/j.dental.2014.08.375 ↗
16. 16) Cattani-Lorente M, Scherrer SS, Ammann P, Jobin M, Wiskott A. Low temperature degradation of a Y-TZP dental ceramic. Acta Biomater 2011; 7: 858-865.10.1016/j.actbio.2010.09.020 ↗
17. 17) Harada K, Shinya A, Gomi H, Hatano Y, Shinya A, Raigrodski AJ. Effect of accelerated aging on the fracture toughness of zirconias. J Prosthet Dent 2016; 115: 215-223.10.1016/j.prosdent.2015.08.020 ↗
18. 18) Volpato CAM, Cesar PF, Bottino MA. Influence of accelerated aging on the color stability of dental zirconia. J Esthet Restor Dent 2016; 28: 304-312.10.1111/jerd.12239 ↗
19. 19) Ban S. Chemical durability of high translucent dental zirconia. Dent Mater J 2020; 39: 12-23.10.4012/dmj.2019-109 ↗
20. 20) Hjerppe J, Vallittu PK, Fröberg K, Lassila L. Effect of sintering time on biaxial strength of zirconium dioxide. Dent Mater 2009; 25: 166-171.10.1016/j.dental.2008.05.011 ↗
21. 21) Zhang F, Van Meerbeek B, Vleugels J. Importance of tetragonal phase in high-translucent partially stabilized zirconia for dental restorations. Dent Mater 2020; 36: 491-500.10.1016/j.dental.2020.01.017 ↗
22. 22) Kilinc H, Sanal FA. Effect of sintering and aging processes on the mechanical and optical properties of translucent zirconia. J Prosthet Dent 2021; 126: 129.e1-e7.10.1016/j.prosdent.2021.03.024 ↗
23. 23) Kong MC, Park MG. Effect of sintering condition and low-temperature degradation on the flexural strength and phase transformation of zirconia. J Prosthet Dent 2021; 126: 692. e1-e14.10.1016/j.prosdent.2021.07.027 ↗
24. 24) International Organization for Standardization. Implants for surgery–Ceramic materials based on yttria-stabilized tetragonal zirconia (Y-TZP). ISO standard 3356:2008, 2nd edition. Geneva: 2008.
25. 25) Lee WF, Takahashi H, Iwasaki N, Peng PW. Effect of thickness of externally characterized stains on optical properties of high-translucency zirconia. Clin Oral Investig 2023; 27: 165-171.10.1007/s00784-022-04704-6 ↗
26. 26) Chevalier J, Cales B, Drouin JM. Low temperature aging of Y-TZP ceramics. J Am Ceram Soc 1999; 82: 2150-2154.10.1111/j.1151-2916.1999.tb02055.x ↗
27. 27) Zhang F, Inokoshi M, Vanmeensel K, Van Meerbeek B, Naert I, Vleugels J. Lifetime estimation of zirconia ceramics by linear ageing kinetics. Acta Mater 2015; 92: 290-298.10.1016/j.actamat.2015.04.001 ↗
28. 28) CIE Technical Report: Colorimetry. CIE pub no 15.3. Vienna, Austria: CIE Central Bureau; 2004.
29. 29) Ghinea R, Perez MM, Herrera LJ, Rivas MJ, Yebra A, Paravina RD. Color difference thresholds in dental ceramics. J Dent 2010; 38: e57-64.10.1016/j.jdent.2010.07.008 ↗
30. 30) Perez MM, Ghinea R, Herrera LJ, Ionescu AM, Pomares H, Pulgar R, et al. Dental ceramics: A CIEDE2000 acceptability thresholds for lightness, chroma and hue differences. J Dent 2011; 39: e37-44.10.1016/j.jdent.2011.09.007 ↗
31. 31) Wee AG, Monaghan P, Johnston WM. Variation in color between intended matched shade and fabricated shade of dental porcelain. J Prosthet Dent 2002; 87: 657-666.10.1067/mpr.2002.125727 ↗
32. 32) Paravina RD, Pérez MM, Ghinea R. Acceptability and perceptibility thresholds in dentistry: A comprehensive review of clinical and research applications. J Esthet Restor Dent 2015; 27: S1-S9.
33. 33) Paravina RD, Ghinea R, Herrera LJ, Bona AD, Igiel C, Linninger M, et al. Color difference thresholds in dentistry: A comprehensive review of clinical and research applications. J Esthet Restor Dent 2019; 31: 103-112.10.1111/jerd.12465 ↗
34. 34) Park MG. Effect of low-temperature degradation treatment on hardness, color, and translucency of single layers of multilayered zirconia. J Prosthet Dent 2023; doi.org/10.1016/j. prosdent.2023.01.023. (In press)10.1016/j.prosdent.2023.01.023 ↗
35. 35) Kim HK, Kim SH, Lee JB, Han JS, Yeo IS. Effect of polishing and glazing on the color and spectral distribution of monolithic zirconia. J Adv Prosthodont 2013; 5: 296-304.10.4047/jap.2013.5.3.296 ↗
36. 36) Dikicier S, Ayyildiz S, Ozen J, Sipahi C. Effect of varying core thicknesses and artificial aging on the color difference of different all-ceramic materials. Acta Odontol Scand 2014; 72: 623-629.10.3109/00016357.2013.879997 ↗
37. 37) Kurt M, Bal BT. Effects of accelerated artificial aging on the translucency and color stability of monolithic ceramics with different surface treatments. J Prosthet Dent 2019; 121: 712. e1-e8.10.1016/j.prosdent.2019.01.014 ↗
38. 38) Ertan AA, Sahin E. Colour stability of low fusing porcelains: an in vitro study. J Oral Rehabil 2005; 32: 358-361.10.1111/j.1365-2842.2004.01415.x ↗
39. 39) Pires-de-Souza F, Casemiro LA, Garcia L, Cruvinel DR. Color stability of dental ceramics submitted to artificial accelerated aging after repeated firings. J Prosthet Dent 2009; 101: 13-18.10.1016/S0022-3913(08)60282-6 ↗
40. 40) Shah K, Holloway JA, Denry IL. Effect of coloring with various metal oxides on the microstructure, color and flexural strength of 3Y-TZP. J Biomed Mater Res B 2008; 87: 329-337.10.1002/jbm.b.31107 ↗
41. 41) Čokić SM, Cóndor M, Vleugels J, Meerbeek BV, Oosterwyck HV, Inokoshi M, et al. Mechanical properties-translucency-microstructure relationships in commercial monolayer and multilayer monolithic zirconia ceramics. Dent Mater 2022; 38: 797-810.10.1016/j.dental.2022.04.011 ↗
42. 42) Perdigão J, Pinto AM, Monteiro RC, Braz Fernandes FM, Laranjeira P, Veiga JP. Degradation of dental ZrO2-based materials after hydrothermal fatigue. Part I: XRD, XRF, and FESEM analyses. Dent Mater J 2012; 31: 256-265.10.4012/dmj.2011-216 ↗
43. 43) Cokic SM, Vleugels J, Van Meerbeek B, Camargo B, Willems E, Li M, et al. Mechanical properties, aging stability and translucency of speed-sintered zirconia for chairside restorations. Dent Mater 2020; 36: 959-972.10.1016/j.dental.2020.04.026 ↗
44. 44) Kanpalta B, Burduroğlu D, Kara Ö. Effect of artificial aging on the translucency of monolithic zirconia materials sintered at different temperatures. J Prosthet Dent 2022; 128: 91.e1-91.e6.10.1016/j.prosdent.2022.05.002 ↗
45. 45) Miura S, Tsukada S, Fujita T, Isogai T, Teshigawara D, Saito-Murakami K, et al. Effect of abutment tooth and luting agent colors on final color of high-translucent zirconia crowns. J Prosthodont Res 2022; 66: 243-249.10.2186/jpr.JPR_D_21_00025 ↗