Fluoride release and strength change of self-adhesive filling materials after storage in water
Source abstract
Abstract
The introduction of self-adhesive filling materials has shown advantage in clinical use due to reduced procedure time. The newly developed self-adhesive Surefil One (SO) was compared to other current self-adhesive materials Vertise Flow (VF) and GC Fuji II LC (FJ). Shear bond strength (SBS) to dentin, flexural strength and water sorption were measured at 24 h and 4 weeks. Fluoride release was measured up to 4 weeks. SO showed intermediate fluoride-release that was higher than VF, but lower than FJ. SO demonstrated lower flexural strength than VF at 24 h but maintained that same strength to 4 weeks. SO had SBS comparable to FJ and VF at 24 h but it decreased at 4 weeks. Caution should be exercised when selecting and using SO, as well as the other two self-adhesive materials. Further studies are necessary to evaluate the efficacy for their clinical use in direct restorations.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Midwestern University College of Dental Medicine-Illinois
Midwestern University College of Dental Medicine-Arizona
References (42)
Show source-provided references
1. 1) Yao C, Ahmed MH, Zhang F, Mercelis B, Van Landuyt KL, Huang C, et al. Structural/chemical characterization and bond strength of a new self-adhesive bulk-fill restorative. J Adhes Dent 2020; 22: 85-97.
2. 2) Shimizu S, Kotake H, Takagaki T, Shinno K, Miyata S, Burrow MF, et al. Evaluation of bonding performance and multi-ion release of S-PRG fillercontaining self-adhesive resin composite. Dent Mater J 2021; 40: 1257-1263.10.4012/dmj.2020-142 ↗
3. 3) Burgess JO, Ghuman T, Cakir D. Self-adhesive resin cements. J Esthet Restor Dent 2010; 22: 412-419.10.1111/j.1708-8240.2010.00378.x ↗
4. 4) McLean JW, Wilson AD. The clinical development of the glass-ionomer cements. I. Formulations and properties. Aust Dent J 1977; 22: 31-36.10.1111/j.1834-7819.1977.tb04441.x ↗
5. 5) McLean JW, Wilson AD. The clinical development of the glass-ionomer cement. II. Some clinical applications. Aust Dent J 1977; 22: 120-127.10.1111/j.1834-7819.1977.tb04463.x ↗
6. 6) Sidhu SK, Nicholson JW. A review of glass-ionomer cements for clinical dentistry. J Funct Biomater 2016; 7: 16.10.3390/jfb7030016 ↗
7. 7) Mount GJ. Clinical performance of glass-ionomers. Biomaterials 1998; 19: 573-579.10.1016/S0142-9612(97)00139-7 ↗
8. 8) Francois P, Remadi A, Le Goff S, Abdel-Gawad S, Attal JP, Dursun E. Flexural properties and dentin adhesion in recently developed self-adhesive bulk-fill materials. J Oral Sci 2021; 63: 139-144.10.2334/josnusd.20-0448 ↗
9. 9) Sidhu SK, Watson TF. Resin-modified glass ionomer materials. A status report for the American Journal of Dentistry. Am J Dent 1995; 8: 59-67.
10. 10) Sabbagh J, Dagher S, El Osta N, Souhaid P. Randomized clinical trial of a self-adhering flowable composite for class I restorations: 2-year results. Int J Dent 2017; 2017: 5041529.10.1155/2017/5041529 ↗
11. 11) Jordehi AY, Shahabi MS, Akbari A. Comparison of self-adhering flowable composite microleakage with several types of bonding agent in class V cavity restoration. Dent Res J (Isfahan) 2019; 16: 257-263.10.4103/1735-3327.261129 ↗
12. 12) Rathke A, Pfefferkorn F, McGuire MK, Heard RH, Seemann R. One-year clinical results of restorations using a novel self-adhesive resin-based bulk-fill restorative. Sci Rep 2022; 12: 3934.10.1038/s41598-022-07965-z ↗
13. 13) Omar H, Gao F, Yoo H, Bim O Jr, Garcia C, LePard KJ, et al. Changes to dentin extracellular matrix following treatment with plant-based polyphenols. J Mech Behav Biomed Mater 2022; 126: 105055.10.1016/j.jmbbm.2021.105055 ↗
14. 14) Yeslam HE. Flexural behavior of biocompatible high-performance polymer composites for CAD/CAM dentistry. J Compos Sci 2023; 7: 270.10.3390/jcs7070270 ↗
15. 15) Rodrigues Junior SA, Zanchi CH, Carvalho RV, Demarco FF. Flexural strength and modulus of elasticity of different types of resin-based composites. Braz Oral Res 2007; 21: 16-21.10.1590/S1806-83242007000100003 ↗
16. 16) Malacarne J, Carvalho RM, de Goes MF, Svizero N, Pashley DH, Tay FR, et al. Water sorption/solubility of dental adhesive resins. Dent Mater 2006; 22: 973-980.10.1016/j.dental.2005.11.020 ↗
17. 17) Tuloglu N, Sen Tunc E, Ozer S, Bayrak S. Shear bond strength of self-adhering flowable composite on dentin with and without application of an adhesive system. J Appl Biomater Funct Mater 2014; 12: 97-101.10.5301/jabfm.5000166 ↗
18. 18) Łagocka R, Skoczyk-Jaworska M, Mazurek-Mochol M. Self-adhesive, bulk-fill bioactive materials as an alternative to silver amalgam in restorative dentistry. Pomeranian J Life Sci 2022; 68: 36-44.10.21164/pomjlifesci.840 ↗
19. 19) Francois P, Fouquet V, Attal JP, Dursun E. Commercially available fluoride-releasing restorative materials: A review and a proposal for classification. Materials (Basel) 2020; 13: 2313.10.3390/ma13102313 ↗
20. 20) Latta MA, Radniecki SM. Bond strength of self-adhesive restorative materials affected by smear layer thickness but not dentin desiccation. J Adhes Dent 2020; 22: 79-84.
21. 21) Sadeghyar A, Lettner S, Watts DC, Schedle A. Alternatives to amalgam: Is pretreatment necessary for effective bonding to dentin? Dent Mater 2022; 38: 1703-1709.10.1016/j.dental.2022.08.011 ↗
22. 22) Pecora N, Yaman P, Dennison J, Herrero A. Comparison of shear bond strength relative to two testing devices. J Prosthet Dent 2002; 88: 511-515.10.1067/mpr.2002.129063 ↗
23. 23) DeHoff PH, Anusavice KJ, Wang Z. Three-dimensional finite element analysis of the shear bond test. Dent Mater 1995; 11: 126-131.10.1016/0109-5641(95)80047-6 ↗
24. 24) Asiri AA, Khan R, Alzahrani SS, Haider S, Khan SUD, Asiri EAM, et al. Comparative analysis of the shear bond strength of flowable self-adhering resin-composites adhesive to dentin with a conventional adhesive. Coatings 2021; 11: 273.10.3390/coatings11030273 ↗
25. 25) Armstrong S, Breschi L, Ozcan M, Pfefferkorn F, Ferrari M, Van Meerbeek B. Academy of Dental Materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (muTBS) approach. Dent Mater 2017; 33: 133-143.10.1016/j.dental.2016.11.015 ↗
26. 26) Mauro SJ, Sundfeld RH, Bedran-Russo AKB, Fraga Briso AL. Bond strength of resin-modified glass ionomer to dentin: The effect of dentin surface treatment. J Minim Interv Dent 2009; 2: 45-53.
27. 27) Garoushi S, Lassila LV, Vallittu PK. The effect of span length of flexural testing on properties of short fiber reinforced composite. J Mater Sci Mater Med 2012; 23: 325-328.10.1007/s10856-011-4480-7 ↗
28. 28) Lohbauer U, Belli R. The mechanical performance of a novel self-adhesive restorative material. J Adhes Dent 2020; 22: 47-58.
29. 29) Brewster J, Roberts HW. 12-Month flexural mechanical properties of conventional and self-adhesive flowable resin composite materials. Dent Mater J 2023; 42: 598-609.10.4012/dmj.2023-011 ↗
30. 30) Rodrigues DS, Buciumeanu M, Martinelli AE, Nascimento RM, Henriques B, Silva FS, et al. Mechanical strength and wear of dental glass-ionomer and resin composites affected by porosity and chemical composition. J Bio Tribo Corros 2015; 1: 24.10.1007/s40735-015-0025-9 ↗
31. 31) U.S. Department of Health and Human Services Federal Panel on Community Water Fluoridation. U.S. Public Health Service recommendation for fluoride concentration in drinking water for the prevention of dental caries. Public Health Rep 2015; 130: 318-331.10.1177/003335491513000408 ↗
32. 32) DenBesten P, Ko HS. Fluoride levels in whole saliva of preschool children after brushing with 0.25 g (pea-sized) as compared to 1.0 g (full-brush) of a fluoride dentifrice. Pediatr Dent 1996; 18: 277-280.
33. 33) Opydo-Szymaczek J, Pawlaczyk-Kamienska T, Borysewicz-Lewicka M. Fluoride intake and salivary fluoride retention after using high-fluoride toothpaste followed by post-brushing water rinsing and conventional (1400-1450 ppm) fluoride toothpastes used without rinsing. Int J Environ Res Public Health 2022; 19: 13235.10.3390/ijerph192013235 ↗
34. 34) Staun Larsen L, Baelum V, Richards A, Nyvad B. Fluoride in saliva and oral mucosa after brushing with 1,450 or 5,000 ppm fluoride toothpaste. Caries Res 2019; 53: 675-681.10.1159/000501264 ↗
35. 35) Reis AF, Giannini M, Pereira PN. Influence of water-storage time on the sorption and solubility behavior of current adhesives and primer/adhesive mixtures. Oper Dent 2007; 32: 53-59.10.2341/06-13 ↗
36. 36) Nicholson JW. Maturation processes in glass-ionomer dental cements. Acta Biomater Odontol Scand 2018; 4: 63-71.10.1080/23337931.2018.1497492 ↗
37. 37) Besnault C, Attal JP, Ruse D, Degrange M. Self-etching adhesives improve the shear bond strength of a resin-modified glass-ionomer cement to dentin. J Adhes Dent 2004; 6: 55-59.
38. 38) Charlton DG, Haveman CW. Dentin surface treatment and bond strength of glass ionomers. Am J Dent 1994; 7: 47-49.
39. 39) Eamsa-ard P, Jaturanont P WS, Lertsatira T, Kulkirativanich J, Eiamputtharak P, Supattarakul P, et al. The shear bond strengths of glass ionomer cement and novel bioactive material to dentin. Proceeding of the RSU International Research Conference 2022 on Science and Technology 2022; 2022: p.126-132.
40. 40) Fritz UB, Finger WJ, Uno S. Resin-modified glass ionomer cements: Bonding to enamel and dentin. Dent Mater 1996; 12: 161-166.10.1016/S0109-5641(96)80015-7 ↗
41. 41) Irie M, Suzuki K. Water storage effect on the marginal seal of resin-modified glass-ionomer restorations. Oper Dent 1999; 24: 272-278.
42. 42) Fano L, Fano V, Ma W, Wang X, Zhu F. Hydrolytic degradation and cracks in resin-modified glass-ionomer cements. J Biomed Mater Res B Appl Biomater 2004; 69: 87-93.10.1002/jbm.b.20037 ↗