The effect of graphene oxide on the mechanical properties of cBN composites fabricated by HTHP method
Source abstract
Abstract
Abstract Conventional cubic boron nitride (cBN) composites suffer from high brittleness and poor machinability. Here, we use graphene to tackle these problems. In this paper, cBN/graphene oxide (GO) composites with the addition of Al-SiC were prepared by high temperature and high pressure sintering method. The fracture toughness of cBN/1.5 wt% GO composites increased by 27.5% compared to that of the monolithic cBN composites. The improvement of fracture toughness is ascribed to crack deflection, graphene interface sliding, and GO pull-out and bridging. The bending strength of the composites improved from 564.2 to 696.9 MPa, which can be attributed to the load bearing of GO and strong bonding between GO and cBN matrix.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Boron and Carbon Nanomaterials Research · Graphene research and applications · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. A roadmap for graphene10.1038/nature11458 ↗
2. Graphene nanoribbon composites10.1021/nn102529n ↗
3. Simultaneous strengthening and toughening of reduced graphene oxide/alumina composites fabricated by molecular-level mixing process10.1016/j.carbon.2014.06.074 ↗
4. Toughening in graphene ceramic composites10.1021/nn200319d ↗
5. Spark plasma sintering of graphene reinforced silicon carbide ceramics10.1016/j.ceramint.2017.04.042 ↗
6. Extraordinary toughening enhancement and flexural strength in Si3N4 composites using graphene sheets10.1016/j.jeurceramsoc.2013.08.039 ↗
7. Effect of Y2O3 additive on properties of cBN composites with Si3N4-Al2O3-Al as binder by high temperature and high pressure sintering10.1016/j.ceramint.2019.07.026 ↗
8. Assessment of the performance of TiB2nanoparticles doped cBN-TiN-Al-Co composites by high temperature high pressure sintering10.1016/j.matchemphys.2019.05.042 ↗
9. Effect of Si/Ti additive on the preparation and properties of cBN-diamond composite sintered by high-temperature and high-pressure10.1016/j.diamond.2019.107513 ↗
10. High pressure sintering of cubic boron nitride compacts with Al and AlN10.1016/j.diamond.2008.07.002 ↗
11. Fabrication of alumina ceramic reinforced with boron nitride nanotubes with improved mechanical properties10.1111/j.1551-2916.2011.04821.x ↗
12. Toughening mechanisms of SiC-bonded CNT bulk nanocomposites prepared by spark plasma sintering10.1016/j.ijrmhm.2017.10.024 ↗
13. Composition, microstructure and mechanical properties of cBN-based composites sintered with AlN- Al- Ni binder10.1016/j.ceramint.2018.06.130 ↗
14. Synthesis of high-performance graphene nanosheets by thermal reduction of graphene oxide10.1016/j.materresbull.2011.06.036 ↗
15. Synthesis and properties of bulk graphene nanoplatelets consolidated by spark plasma sintering10.1016/j.carbon.2012.04.054 ↗
16. Effect of graphene nano-platelet reinforcement on the mechanical properties of hot pressed boron carbide based composite10.1016/j.ceramint.2018.02.225 ↗
17. Perspectives on carbon nanotubes and graphene Raman spectroscopy10.1021/nl904286r ↗
18. Compression behavior of single-layer graphenes10.1021/nn100454w ↗
19. Toughening of zirconia/alumina composites by the addition of graphene platelets10.1016/j.jeurceramsoc.2012.07.007 ↗
20. Enhanced mechanical properties of nanocrystalline boron carbide by nanoporosity and interface phases10.1038/ncomms2047 ↗
21. Enhancing toughness in boron carbide with reduced graphene oxide10.1111/jace.13943 ↗
22. Effect of Ni and graphene on microstructure and toughness of titanium boride ceramic tool material prepared by spark plasma sintering10.1016/j.ceramint.2018.08.017 ↗
23. Enhancing toughness and strength of SiC ceramics with reduced graphene oxide by HP sintering10.1016/j.jeurceramsoc.2018.05.033 ↗