Fatigue behavior and recovery of a van der Waals-layered material, highly oriented pyrolytic graphite, under cyclic interlayer shear loading
Source abstract
Abstract
van der Waals (vdW)-layered materials possess both high stiffness and flexibility owing to strong in-plane bonding and weak interlayer interactions and are characterized by reversible deformation through interlayer slip. These structural features suggest the possibility of a unique fatigue response that is distinct from that of conventional materials. However, a fundamental question remains unanswered: Does fatigue occur in such systems at all? This study aims to elucidate the fundamental fatigue behavior of vdW-layered materials, with a particular focus on their characteristic interlayer slip. Highly oriented pyrolytic graphite (HOPG), a representative vdW-layered material composed of stacked graphene layers, was employed. Microscale cantilever specimens were subjected to one-sided (pulsating) and two-sided (alternating) cyclic shear loading under in situ observation using transmission and scanning electron microscopes. In the one-sided fatigue tests, cyclic softening was observed with increasing cycle number, as indicated by the decreases in the shear modulus and nominal shear stress range, accompanied by the accumulation of plastic deformation. Furthermore, the reduced deformation resistance was partially restored over time. Cyclic softening was also observed in the two-sided fatigue tests; however, unlike in the one-sided case, no accumulation of plastic deformation occurred, and the reduced deformation resistance was fully restored over time. These findings indicate that, while HOPG exhibits a transient decrease in the deformation resistance characteristic of fatigue, it also possesses a self-recovery mechanism enabled by reversible interlayer slip, suggesting that its mechanical properties can be retained semi-permanently. • We investigated the fatigue of van der Waals-layered graphite caused by interlayer slip. • We conducted pulsating and alternating fatigue tests on the micro-graphite cantilever specimens. • Both pulsating and alternating loading caused cyclic softening, reducing deformation resistance with cycles. • Deformation resistance recovered over time without any external energy input.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Graphene research and applications · Fiber-reinforced polymer composites · Graphite, nuclear technology, radiation studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Two-dimensional atomic crystals10.1073/pnas.0502848102 ↗
2. Graphene-like two-dimensional materials10.1021/cr300263a ↗
3. Intrinsic interlayer shear strength of graphite10.1016/j.jmps.2024.105853 ↗
4. Recent advances in the mechanics of 2D materials
5. Bending of multilayer van der Waals materials
6. Bending stiffness and interlayer shear modulus of few-layer graphene
7. Ultrasoft slip-mediated bending in few-layer graphene10.1038/s41563-019-0529-7 ↗
8. Bending deformation and self-restoration of submicron-sized graphite cantilevers10.1016/j.actamat.2022.118381 ↗
9. Analyzing the bending deformation of van der Waals-layered materials by a semi-discrete layer model10.1063/5.0170037 ↗
10. Observation of microscale superlubricity in graphite10.1103/PhysRevLett.108.205503 ↗
11. Elasticity of single-crystalline graphite: inelastic X-ray scattering study10.1103/PhysRevB.75.153408 ↗
12. Bending modes, elastic constants and mechanical stability of graphitic systems10.1016/j.carbon.2010.08.042 ↗
13. Self-retracting motion of graphite microflakes10.1103/PhysRevLett.100.067205 ↗
14. Nano-thick surface-modified layer governs bending deformation of micrographite10.1016/j.carbon.2024.119712 ↗
15. Ultrastiff graphene10.1038/s41699-021-00232-1 ↗
16. Measurement of the elastic properties and intrinsic strength of monolayer graphene
17. Basinski · 1979
18. Pedersen · 1981
19. Basinski · 1992
20. Fatigue of graphene10.1038/s41563-019-0586-y ↗
21. Cui
22. Fatigue and its effect on the mechanical and thermal transport properties of polycrystalline graphene10.1007/s10853-021-05953-8 ↗
23. Low-cycle fatigue failure of MoS2 monolayer10.1016/j.eml.2022.101942 ↗
24. Short-beam shear fatigue life assessment of thermally cycled carbon–aluminium laminates with protective glass interlayers10.1007/s43452-021-00181-y ↗
25. A modified short beam shear specimen for characterization of interfacial strength in nanocomposites10.1016/j.polymertesting.2012.04.011 ↗
26. Low cycle fatigue crack propagation at a notch under pulsating load10.1111/j.1460-2695.1979.tb01351.x ↗
27. Analysis of partially pulsating fatigue process on carbon steel with microstructural observation10.1016/j.msea.2015.10.103 ↗
28. Effect of loading type on fatigue lifetime of sintered-silver die attach10.1109/TDMR.2018.2847638 ↗
29. The use of a Ga + focused ion beam to modify graphene for device applications10.1088/0957-4484/23/25/255305 ↗
30. TEM sample preparation and FIB-induced damage10.1557/mrs2007.63 ↗
31. FIB damage of Cu and possible consequences for miniaturized mechanical tests10.1016/j.msea.2007.01.046 ↗
32. Damage in III–V compounds during focused ion beam milling10.1017/S1431927605050294 ↗
33. Improvements in performance of focused ion beam cross-sectioning: aspects of ion-sample interaction10.1093/jmicro/dfh078 ↗
34. Modifying atomic-scale friction between two graphene sheets: a molecular-force-field study10.1103/PhysRevB.76.155429 ↗
35. Ductile van der Waals materials10.1126/science.abd4527 ↗
36. High-throughput screening of 2D van der Waals crystals with plastic deformability10.1038/s41467-022-35229-x ↗
37. Effect of nanopore on mechanical characteristics of indium selenide membrane10.1007/s40430-025-05397-0 ↗
38. Stretching and breaking of ultrathin MoS 210.1021/nn203879f ↗
39. Rhombohedral stacking-faults in exfoliated highly oriented pyrolytic graphite10.1016/j.cartre.2024.100345 ↗
40. Visualization of Raman spectroscopy for stacking orders: distinguishing Bernal and rhombohedral graphite10.1007/s40042-024-01165-w ↗
41. Stacking order in graphite films controlled by van der Waals technology10.1021/acs.nanolett.9b03014 ↗
42. Measuring the degree of stacking order in graphite by Raman spectroscopy10.1016/j.carbon.2007.11.015 ↗