Physics Dept, School of Distance Education, Universiti Sains Malaysia, 11800 Penang, Malaysia, L. L. Wen, L. S. Chuah, Physics Dept, School of Distance Education, Universiti Sains Malaysia, 11800 Penang, Malaysia, Y. G. Zhang, Physics Dept, School of Distance Education, Universiti Sains Malaysia, 11800 Penang, Malaysia, Y. Yusof, Physics Dept, School of Distance Education, Universiti Sains Malaysia, 11800 Penang, Malaysia, N. M. Ahmed, Physics Dept, School of Distance Education, Universiti Sains Malaysia, 11800 Penang, Malaysia, Z. Hassan, Physics Dept, School of Distance Education, Universiti Sains Malaysia, 11800 Penang, Malaysia

Abstract

In this paper, we investigated growth of GaN and Al0.09Ga0.91N epilayer grown on silicon (111) by using II MBE system. The major characterization tools used for this study were high resolution X-ray diffraction (HRXRD), and micro photoluminescence (PL) spectroscopy. Also reported is our attempt to fabricate and characterize metalsemiconductor-metal photodiode based on these films. The responsivity as a function of wavelength for an MSM GaN/Si(111) detector is a sharp cut-off wavelength at 362 nm. A maximum responsivity of 0.256 A/W was achieved at 358 nm. For Al0.09Ga0.91N film, there is a sharp cut-off wavelength at 340 nm. A maximum responsivity of 0.263 A/W was achieved at 338 nm. In UV spectral region, the detector shows a little decrease from 340 to 200 nm. The responsivity of the MSM drops by nearly an order of magnitude across the cut-off wavelength.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: GaN-based semiconductor devices and materials · Semiconductor Quantum Structures and Devices · Silicon Carbide Semiconductor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. [1] J. I. Pankove: Mater. Res. Soc. Symp. Proc. 162 (1990) 515; https://doi.org/10.1557/PROC-162-51510.1557/PROC-162-515 ↗
2. [2] E. Monroy, E. Munoz, F. J. Sanchez, F. Calle, E. Calleja, B. Beaumout, P. Gibart, J. A. Munoz and F. Cusso: Semicond. Sci. Technol. 13 (1998) 1042; https://doi.org/10.1088/0268-1242/13/9/01310.1088/0268-1242/13/9/013 ↗
3. [3] G. Parish, S. Keller, P. Kozodoy, J. A. Ibbetson, H. Marchand, P. T. Fini, S. B. Fleischer, S. P. DenBaars and U. K. Mishra: Appl. Phys. Lett. 75 (1999) 247; https://doi.org/10.1063/1.12433710.1063/1.124337 ↗
4. [4] E. Monroy, M. Hamilton, D. Walker, P. Kung, F. J. Sanchez and M. Razeghi: Appl. Phys. Lett. 74 (1999) 1171; https://doi.org/10.1063/1.12396010.1063/1.123960 ↗
5. [5] A. Osinsky, S. Gangopadhyay, R. Gaska, B. Williams, M. A. Khan, D. Kuksenkov and H. Temkin: Appl. Phys. Lett. 71 (1997) 2334; https://doi.org/10.1063/1.12002310.1063/1.120023 ↗
6. [6] Q. Chen, J. W. Yang, A. Osinsky, S. Gangopadhyay, B. Lim, M. Z. Anwar, M. Asif Khan, D. Kuksenkov and H. Temkin: Appl. Phys. Lett. 70 (1997) 2277; https://doi.org/10.1063/1.11883710.1063/1.118837 ↗
7. [7] Z. C. Huang, J. C. Chen and D. Wickenden: J. Cryst. Growth 170 (1997) 362; https://doi.org/10.1016/S0022-0248(96)00576-310.1016/S0022-0248(96)00576-3 ↗
8. [8] Y. K. Su, Y. Z. Chiou, F. S. Juang, S. J. Chang and J. K. Sheu: Jpn. J. Appl. Phys. 40 (2001) 2996; https://doi.org/10.1143/JJAP.40.299610.1143/JJAP.40.2996 ↗
9. [9] E. H. Rhoderick and R. H. Williams, Metal-Semiconductor Contacts, 2nd ed. (Oxford University Press, New York, 1988).
10. [10] A. Ohtani, K. S. Stevens, R. Beresford, Appl. Phys. Lett. 65 (1994) 61; https://doi.org/10.1063/1.11307410.1063/1.113074 ↗
11. [11] E. Calleja, M. A. Sanchez-Garcia, F. J. Sanchez, F. Calle, F. B. Naranjo, E. Munoz, S.I. Molina, A. M. Sanchez, F. J. Pacheco, R. Garcia, J. Cryst. Growth 201/202 (1999) 296; https://doi.org/10.1016/S0022-0248(98)01346-310.1016/S0022-0248(98)01346-3 ↗
12. [12] J. Ristic, M. A. Sanchez-Garcia, E. Calleja, A. Perez-Rodriguez, C. Serre, A. RomanoRodriguez, J. R. Morante, V. R., J. Cryst. Growth 263 (2004) 30.
13. [13] A. Reiher, J. Blasing, A. Dadgar, A. Diez, A. Krost, J. Crystal Growth 248 (2003) 563; https://doi.org/10.1016/S0022-0248(02)01880-810.1016/S0022-0248(02)01880-8 ↗
14. [14] X. Zhang, S.J. Chua, P. Li, K.B. Chong, Z.C. Feng, Appl. Lett. 74 (1999) 1984; https://doi.org/10.1063/1.12372110.1063/1.123721 ↗
15. [15] J.T. Torvik, J.I. Pankove, E. Iliopoulos, H. M. Ng and T. D. Moustakas, Appl. Phys. Lett. 72 (1998) 244; https://doi.org/10.1063/1.12069810.1063/1.120698 ↗