Al5Mo thin film anodes for Li-ion batteries were prepared using DC sputtering under different conditions, the latter being specified as deposition at room temperature (S0), deposition at 300°C (S1), and deposition at room temperature followed by thermal annealing at 300°C (S2). The thin films were deposited using an aluminum target tiled with molybdenum discs at a ratio calculated based on the theoretical sputtering yields. The structural and compositional analyses performed with x-ray diffraction (XRD) and energy-dispersive x-ray spectroscopy (EDX) confirmed the Al5Mo compound formation and the Al/Mo elemental ratio, respectively. The compound formation was observed to be evident only for the thin films subjected to heat treatment during or after deposition. Scanning electron micrographs reveal a higher porosity of approximately 23% for sample S0 and a lower porosity of around 18% for sample S1. The chronopotentiometry results show a higher volumetric specific capacity of approximately 197 mAh/cm3 for sample S1. Capacity increments have been observed for all samples upon charge-discharge cycles, whose values after 25 cycles for samples S0, S1, and S2 were 41.2%, 20.4%, and 21.1%, respectively. Open image in new window
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Semiconductor materials and devices · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. J. B. Bates, N. J. Dudney, G. R. Gruzalski, R. A. Zuhr, A. Choudhury, and C. F. Luck, J. Power Sources 43, 103 (1993).10.1016/0378-7753(93)80106-Y ↗
2. J. B. Bates, G. R. Gruzalski, N. J. Dudney, C. F. Luck, and X. H. Yu, Solid State Ionics 70, 619 (1994).10.1016/0167-2738(94)90383-2 ↗
3. N. J. Dudney and Y.-I. Jang, J. Power Sources 119, 300 (2003).10.1016/S0378-7753(03)00162-9 ↗
4. W.-J. Zhang, J. Power Sources 196, 13 (2011).10.1016/j.jpowsour.2010.07.020 ↗
5. M. J. Lindsay, G. X. Wang, and H. K. Liu, J. Power Sources 119, 84 (2003).10.1016/S0378-7753(03)00130-7 ↗
6. M. Wachtler, J. O. Besenhard, and M. Winter, J. Power Sources 94, 189 (2001).10.1016/S0378-7753(00)00585-1 ↗
7. R. Z. Hu, L. Zhang, X. Liu, M. Q. Zeng, and M. Zhu, Electrochem. Comm. 10, 1109 (2008).10.1016/j.elecom.2008.05.012 ↗
8. K. Wang, X. He, J. Ren, L. Wang, C. Jiang, and C. Wan, Electrochim. Acta 52, 1221 (2006).10.1016/j.electacta.2006.07.020 ↗
9. M. Winter, J. O. Besenhard, M. E. Spahr, and P. Novak, J. Adv. Mater. 10, 725 (1998).10.1002/(SICI)1521-4095(199807)10:10<725::AID-ADMA725>3.0.CO;2-Z ↗
10. D. Larcher, S. Beattie, M. Morcrette, K. Edstrom, J. C. Jumas, and J. M. Tarascon, J. Mater. Chem. 17, 3759 (2007).10.1039/b705421c ↗
11. M. M. Thackeray, J. T. Vaughey, and L. M. L. Fransson, J. Mater. Sci. 54, 20 (2002).
12. M. Winter and J. O. Besenhard, Electrochim. Acta 45, 31 (1999).10.1016/S0013-4686(99)00191-7 ↗
13. H. J. Bang, S. Kim, and J. Prakash, J. Power Sources 92, 45 (2001).10.1016/S0378-7753(00)00522-X ↗
14. C. Wang, A. J. Appleby, and F. E. Littl, J. Power Sources 93, 174 (2001).10.1016/S0378-7753(00)00576-0 ↗
15. S. Balaji, S. Shanmugan, D. Mutharasu, and K. Ramanathan, Mater. Sci.-Pol. 28, 583 (2010).
16. S. Balaji, T. Mani Chandran, and D. Mutharasu, Ionics 18, 549 (2012).10.1007/s11581-011-0650-3 ↗