journal article·2016-02

Failure analysis of a leaching reactor made of glass-fiber reinforced plastic

Mari Lindgren, Gunnar Bergman, Markus Kakkonen, Markus Lehtonen, Jarno Jokinen, Markus Wallin, Olli Saarela, Jyrki Vuorinen

Publisher page

Abstract

Abstract This paper reports a failure analysis of a leaching reactor in a zinc plant that suffered from a catastrophic failure after less than two years of operation. During normal operation the bottom of the reactor fell out suddenly, releasing the contents, a high-temperature acidic solution, into the surroundings in an uncontrollable manner. The reactor was made of glass-fiber reinforced plastic. Microscopy, thermal analysis, mechanical testing and finite element analyses were employed to investigate the causes of the failure. There were several contributing factors but the root cause was poor adhesion between the bottom and the joint laminate, which was caused by insufficient grinding during the surface preparation stage of the joint.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical Behavior of Composites · High-Velocity Impact and Material Behavior · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. M. Lahtinen, H. Takala, K. Svens, A. Järvinen, P. Talonen. Atmospheric zinc concentrate leaching technology of Outokumpu, In: T. Fujisawat et al., editors. Proc. of International Symposium on Lead and Zinc processing, October 17–19, 2005, Kyoto, Japan, 803–816.
2. Ruonala M, Svens K, Hammerschmidt J, Saxen B, Tuuppa E. Latest developments in zinc processing, In: Siegmund A, Centono L, Geenen C, Piret N, Richards G, Stephens R, editors. Proc. of Lead-Zinc 2010, TMS (The Minerals, Metals & Materials Society), 29–45.
3. Atmospheric zinc concentrate leaching of Outokumpu technology
4. Hull · 1996
5. Graham J, Johnson T, Kelley D, Optimum material solutions for industrial hydrometallurgical equipment. In: G. Jarjoura ed. Proc of COM2012, Corrosion: Recent Advantages & Sustainability, MetSoc, 93–103.
6. ASTM D5868, Standard Test Method for Lap Shear Adhesion for Fiber Reinforced Plastic (FRP) Bonding
7. ASTM D3762, Standard Test Method for Adhesive-Bonded Surface Durability of Aluminum (Wedge Test)
8. The virtual crack closure technique: history, approach and applications
9. Effect of void content on the strength of composite laminates10.1016/0263-8223(94)90044-2 ↗
10. Incropera · 1996 · 783
11. Effects of two aqueous acid solutions on glass reinforced vinyl ester resin tubes10.1179/1879139511Y.0000000022 ↗
12. Long-term water immersion ageing characteristics of GFRP composites10.1007/s10853-009-3485-9 ↗
13. The effects of mechanical damage in a glass fibre/epoxy composite on the absorption rate10.1016/0961-9526(94)00014-Z ↗
14. Long term environmental effects on physical properties of vinylester composite pipes10.1016/j.polymertesting.2011.10.001 ↗
15. Hygrothermal effects of epoxy resin. Part I. The nature of water in epoxy10.1016/S0032-3861(98)00790-3 ↗
16. Numerical analysis of the stress distribution in single-lap shear tests under elastic assumption — application to the optimisation of the mechanical behaviour10.1016/j.ijadhadh.2011.07.001 ↗
17. A review of finite element analysis of adhesively bonded joints10.1016/j.ijadhadh.2011.01.006 ↗
18. A new method to quantify delamination resistance of fiber reinforced polymers (FRP) under transverse loading10.1007/s10443-004-6205-2 ↗
19. Improvements in mode I interlaminar fracture toughness and in-plane mechanical properties of stitched glass/polyester composites10.1016/j.compscitech.2006.03.032 ↗
20. Mixed mode fracture toughness of GFRP composites10.1016/j.compstruct.2006.04.020 ↗
21. Influence of in-plane fiber orientation on mode I interlaminar fracture toughness of stitched glass/polyester composites10.1016/j.compscitech.2008.02.008 ↗
22. Double cantilever beam mode I testing for vacuum infused repairs of GFRP10.1163/156856103762864642 ↗
23. Tensile creep and deformation modeling of vinyl ester polymer and its nanocomposites10.1177/0731684408090378 ↗