Fracture failure analysis of the sacrificial anode protector in a water injection well
Source abstract
Abstract
Abstract In an injection well, sacrificial anode protectors were installed in order to protect the tubing string. However, one sacrificial anode protector was broken during the lifting process of the tubing string in well workover. The causes for the fracture failure of the sacrificial anode protector were investigated by scanning electron microscope (SEM), energy dispersive spectrometer (EDS), X-ray diffractometry (XRD) and optical microscope (OM). The metallographic structure of the sacrificial anode protector was pearlite plus reticular ferrite and its chemical composition met the requirements of API Spec 5CT. However, the hardness distribution was inhomogeneous and the yield strength was also lower than the required value. In addition, the impact toughness was poor. The failure of the sacrificial anode protector was the combined consequence of material defects and the harsh service environment. In the CO2/H2S environment, the anode was dissolved and the cathode was subjected to hydrogen evolution. Therefore, hydrogen atoms diffused into the metal and accumulated at crystal defects, thus inducing microcracks. Finally, hydrogen embrittlement fracture failure occurred. In the material selection of the cathode of the sacrificial anode protector, a material with good hydrogen resistance is recommended and the high-temperature exposure time should be prolonged. In addition, it is necessary to design an effective service life for the sacrificial anode protector and replace the sacrificial anode protector in time.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Failure analysis on fracture of S13Cr-110 tubing10.1016/j.engfailanal.2018.03.004 ↗
2. Corrosion mechanism and applicability assessment of N80 and 9Cr steels in CO2 auxiliary steam drive10.1007/s11665-018-3847-z ↗
3. Sour corrosion of C110 steel and its influence by galvanic couple and stress10.1021/ie2018492 ↗
4. Stress corrosion crack evaluation of super 13Cr tubing in high-temperature and high-pressure gas wells10.1016/j.engfailanal.2018.09.030 ↗
5. Effect of immersion time on the mechanical properties of S135 drill pipe immersed in H2S solution10.1007/s11665-014-1198-y ↗
6. Effects of heat-stable salts on the corrosion behaviours of 20 steel in the MDEA/H2S/CO2 environment10.1080/1478422X.2019.1591737 ↗
7. Unraveling the effects of CO2 and H2S on the corrosion behavior of electroless Ni-P coating in CO2/H2S/Cl- environments at high temperature and high pressure10.1016/j.corsci.2018.12.022 ↗
8. Electrochemical corrosion behavior of carbon steel under dynamic high pressure H2S/CO2 environment10.1016/j.corsci.2012.08.007 ↗
9. High temperature sweet corrosion and inhibition in the oil and gas industry: Progress, challenges and future perspectives
10. Magnesium alloy anode as a smart corrosivity detector and intelligent sacrificial anode protector for reinforced concrete10.1016/j.corsci.2019.04.027 ↗
11. Effect of anode and size variations on the cathodic protection of mild steel in sea water and sulphuric acid
12. Assessment of sacrificial anode impact by aluminum accumulation in mussel Mytilus edulis: A large-scale laboratory test10.1016/j.marpolbul.2011.09.017 ↗
13. Surface catalysis based on ruthenium dioxide for effective activation of aluminium sacrificial anodes10.1016/S0010-938X(03)00038-6 ↗
14. Application oe sacrificial anode protection in re-injection water well
15. Study and application od tubing protection technique of sacrificial anode in Shanshan oilfield
16. X. Jiang, Nonferrous inclusion in steel, (2011) 263–276.
17. R. Heidersbach, Metallurgy and corrosion control in oil and gas production, (2010)107-114.10.1002/9780470925782 ↗
18. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
19. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
20. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
21. Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testing10.1016/j.corsci.2017.08.032 ↗
22. Effect of plastic deformation and H2S on dynamic fracture toughness of high strength casing steel10.1007/s11595-015-1159-9 ↗
23. Instrumented Charpy impact testing and dynamic fracture toughness of 4145H drilling collar steel
24. Corrosion rule of ductile cast iron pipe in seashore saline soil determined by electrolytic/galvanic accelerated corrosion tests
25. Failure analysis of a carbon steel screw under the service in the presence of hydrogen sulphide10.1016/j.engfailanal.2011.07.001 ↗
26. Failure analysis of P110 tubing string in the ultra-deep oil well10.1016/j.engfailanal.2010.11.013 ↗
27. Effect of microstructure and temperature on the stress corrosion cracking of two microalloyed pipeline steels in H2S environment for gas transport10.1016/j.engfailanal.2019.06.028 ↗
28. The effects of sulfide stress cracking on the mechanical properties and intergranular cracking of P110 casing steel in sour environments10.1007/s12182-013-0286-1 ↗
29. The inhibition effect of the molybdate on hydrogen permeation of 2205 duplex stainless steel10.1016/j.surfcoat.2015.12.077 ↗
30. Hydrogen permeation behaviour of X56 steel in simulated atmospheric environment under loading10.1179/147842209X12559428167689 ↗
31. Effect of the elastic tensile load on the electrochemical corrosion behavior and diffusible hydrogen content of ferritic steel in acidic environment10.1016/j.ijhydene.2017.05.210 ↗
32. Sour gas corrosion—corrosion of steels and other metallic materials in aqueous environments containing H2S10.1016/B978-0-12-409547-2.11546-X ↗
33. Review of recent progress in the study of corrosion products of steels in a hydrogen sulphide environment10.1016/j.corsci.2018.05.002 ↗