Abstract The analysis of multiple cracks in a heat exchanger tubeplate at a petrochemical plant led to experimental replication of in-service damage. High lifting stresses created a first leak that was repaired. Extended branched intergranular cracking developed from the tubeplate surface around the repair weld after few weeks of renewed operation. Chemical analyses failed to detect Na on crack surfaces, while operative conditions also allowed discarding a typical SCC cracking mechanism. Lack of radial interference between tubes and plate, lack of penetration and lack of fusion at tube to tubeplate weld roots were also thought as contributors to cracking. Microstructural analyses revealed martensite clusters in welds and HAZ, and austenite grain boundary precipitates in the tubeplate base material. Thermal cycles were applied to ex-service samples to replicate the conditions for these brittle micro constituents, which were found to be unstable at operating temperatures. Mechanical testing also replicated grain boundary weakness. This inadequate structure was related to welding without proper thermal cycles and heat treatments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. ASME BPVC · 2004
2. An analysis of an incident during the renovation work of a power boiler superheater10.1016/j.engfailanal.2015.07.011 ↗
3. Failure analysis of carbon steel components in a water bath heater and the influence of ethylene glycol concentration10.1016/j.engfailanal.2016.05.015 ↗
4. Thermomechanical fatigue life prediction of 316L compact heat exchanger10.1016/j.engfailanal.2016.06.003 ↗
5. Failure analysis of tube–tubesheet welds in cracked gas heat exchangers10.1016/j.engfailanal.2004.01.003 ↗
6. Failure analysis of tube-to-tubesheet welded joints in a shell-tube heat exchanger10.1016/j.csefa.2016.06.002 ↗
7. ASTM A 336/A 336M – 07 · 2007
8. ASTM A388/A388M - 16a · 2016
9. Appendix A · 2010
10. Mechanical properties of a 2-1/4 Cr-1 Mo steel tubesheet forging10.1007/BF02833318 ↗
11. Influence of long-term ageing on the microstructure and mechanical properties of T24 steel10.1016/j.msea.2016.11.087 ↗
12. Microstructure and mechanical properties of the T23 steel after long-term ageing at elevated temperature10.1080/09603409.2016.1139306 ↗
13. Common causes of historical failures in high pressure tubes
14. Intergranular susceptibility in failures of high pressure tubes
15. The link between equilibrium segregation and precipitation in ternary solutions exhibiting temper embrittlement10.1179/030634576790431390 ↗
16. Temper Embrittlement
17. API RP 934-A · 2008