Effect of extra-large compound calcium-aluminosilicate inclusions on cracking of camshafts
Source abstract
Abstract
Abstract About one-hundred out of three-hundred camshafts were found to crack in varying degrees after finishing final heat treatment of induction-quenching. The cracked camshafts were made from one steel ingot of same furnace number. The failed camshafts are used in truck diesel engine with six cylinders. Stereomicroscope observation showed that several longitudinal and radial cracks were presented on the external surfaces of journals and cams and the side of journals of camshafts. Numerous extra-large elongated compound inclusions of calcium-aluminosilicate (CaO⋅Al2O3⋅SiO2) along the longitudinal of camshaft were found on the fracture surfaces. Fracture surfaces characteristically “woody” in appearance or lamellar and deep groove fracture topography were confirmed to be associated with inclusion distribution along the longitudinal direction of camshaft. Metallographic examination indicated that the camshaft material had a very low purity, especially in the surface region of camshafts, i.e. crack origin regions. The total index of oxide inclusion of the metallographic samples from the smoothed fracture surfaces was evaluated to be K4 = 181 according to DIN standard, much higher than the specified index, K4 ≤ 30. During induction-quenching process, a hoop tensile thermal stress and a hoop tensile transformation stress would develop on the matrix surrounding the compound inclusion of calcium-aluminosilicate due to the significant difference in the thermal expansion coefficients between them and the volume expansion of matrix in the surface region resulting from the transformation of austenite to martensite. When the superimposed stress of both stresses was greater than the tensile strength of matrix material in the surface region, the micro-cracks along the radial of compound inclusion would develop on the matrix surrounding the compound inclusion to lead to cracking of camshaft.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical Failure Analysis and Simulation · Fatigue and fracture mechanics · Mechanical stress and fatigue analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Fracture analysis of a camshaft made from nodular cast iron10.1016/j.engfailanal.2005.11.001 ↗
2. Development of valve trainrig for assessment of cam/follower tribochemistry10.1016/j.triboint.2015.02.026 ↗
3. Failure analysis of an overhead valve train system in urban buses10.1016/j.engfailanal.2018.11.003 ↗
4. Analysis of a cracked diesel engine camshaft10.1007/s11668-012-9584-y ↗
5. Hoag · 2015 · 367
6. DIN 50602-1985 Microscopic examination of special steels using standard diagrams to assess the content of non-metallic inclusions.
7. The effect of sulfide inductions on mechanical properties and failures of steel components10.1007/s11668-015-9940-9 ↗
8. Failure of a fusion welded ball joint as a result of modification in MnS direction10.1007/s11668-008-9164-3 ↗
9. Failure analysis of the oil transport spiral welded pipe10.1016/j.engfailanal.2012.05.008 ↗
10. Defects as root cause of fatigue failure of metallic components. II. Non-metallic inclusions10.1016/j.engfailanal.2019.01.054 ↗
11. The microstructure and fracture of a carburized steel10.1007/BF02661935 ↗
12. Cracking failure of locomotive diesel engine injector nozzles10.1007/s11668-015-9962-3 ↗
13. Crack-inclusion due to mismatched thermal expansion under plane stress condition10.1007/s11012-016-0360-z ↗
14. Zhang · 1991
15. Experimental and analytical investigation of steel bolts failed after isothermal heat treatment10.1007/s11668-015-9938-3 ↗
16. Failure analysis of microcracks and alumina inclusions induced insulator pin’s low stress mode of fracture10.1007/s11668-015-9970-3 ↗