Erosion of alloys used for the stages of electrical submersible pumps
Source abstract
Abstract
Abstract Judicious selection of the material used for the stages of an electric submersible pump (ESP) is crucial for a prolonged service life. Working in high-velocity fluids carrying solid particles, the stage surfaces are subjected to solid particle impingement and thus erosion defects arise. Moreover, subsequent erosion-corrosion synergy brings additional threats to the ESPs operating in corrosive environments. In this report, jet impingement tests were conducted to evaluate the performance of three alloys under erosive and corrosive conditions. The tested materials include two Ni-Resist cast irons — wear-resistant materials commonly used for ESP stages — and one superduplex stainless steel (SDSS) that is famous for high strength and extraordinary corrosion resistance. The erosion rate of each material, along with its dependence on jet impingement angle, is quantified in terms of overall volume loss and localized depth loss. Tap water and salt solution are used as particle carrier in parallel to study the synergy between erosion and corrosion. The erosion mechanism of different phases, as well as its dependence on particle impingement conditions, are discussed. Finally, the applicability of substituting Ni-Resist cast irons with SDSS to cope with highly corrosive conditions is assessed based on the experiment results.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Erosion and Abrasive Machining · Advanced materials and composites · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. R.V. Flatern, Schlumberger Defining Series: Electrical Submersible Pumps (2015). URL https://www.slb.com/-/media/Files/resources/oilfield_review/defining_series/Defining-ESP.pdf.
2. Gahr · 1998 · vol. 31
3. Erosion corrosion of pump impeller of cyclic cooling water system10.1016/j.engfailanal.2005.07.012 ↗
4. Material overview for electric submersible pumps: Part I – metallic and ceramic materials
5. The effects of solidification on the microstructure and mechanical properties of modified ductile Ni-resist iron with a high manganese content10.1016/j.msea.2013.12.070 ↗
6. R. Elliott, Chapter 5 - Some founding considerations, in: R. Elliott (Ed.), Cast Iron Technology, Butterworth-Heinemann, 1988, pp. 165–220. doi:10.1016/B978-0-408-01512-7.50008-2.10.1016/B978-0-408-01512-7.50008-2 ↗
7. Nickel Development Institute, Properties and applications of Ni-resist and ductile Ni-resist alloys (No.11018) (1998). URL https://www.nickelinstitute.org/media/1770/propertiesandapplicationsofni_resistandductileni_resistalloys_11018_pdf.
8. The erosion of carbide-metal composites10.1016/0043-1648(88)90210-4 ↗
9. Corrosion behavior of supermartensitic stainless steel in aerated and CO2-saturated synthetic seawater10.1016/j.msea.2006.04.107 ↗
10. Effect of microstructure on corrosion behavior of superduplex stainless steel at critical environment conditions10.1016/j.scriptamat.2007.07.037 ↗
11. O. Abuzeid, M.A. Zour, A. Aljoboury, Y. Alzafin, Stress Corrosion Cracking of Ductile Ni-Resist Irons and Stainless Steels, in: Environmental and Industrial Corrosion-Practical and Theoretical Aspects, IntechOpen, 2012. doi:10.5772/52318.10.5772/52318 ↗
12. Stress corrosion cracking of stainless steels recommended for building brine recirculation pumps10.1016/j.engfailanal.2010.03.008 ↗
13. Effect of carbon dioxide and temperature on passive film parametersof superduplex stainless steel10.1590/S1516-14392013005000088 ↗
14. Effect of sigma phase on the wear behavior of a super duplex stainless steel10.1016/j.wear.2013.04.010 ↗
15. Duplex stainless steels: brief history and some recent alloys
16. Super duplex stainless steels10.1179/mst.1992.8.8.685 ↗
17. H. Meng, X. Hu, A. Neville, A systematic erosion-corrosion study of two stainless steels in marine conditions via experimental design, Wear 263 (1–6 SPEC. ISS.) (2007) 355–362. doi:10.1016/j.wear.2006.12.007.10.1016/j.wear.2006.12.007 ↗
18. Erosion-corrosion behaviour of lean duplex stainless steels in 3.5% NaCl solution10.1016/j.wear.2012.12.007 ↗
19. Wear models and predictive equations: their form and content10.1016/0043-1648(95)90158-2 ↗
20. The role of abrasive particle size on erosion characteristics of stainless steel10.1016/j.engfailanal.2019.01.020 ↗
21. A comprehensive review of solid particle erosion modeling for oil and gas wells and pipelines applications10.1016/j.jngse.2014.10.001 ↗
22. Analytical and experimental research on erosion wear law of drill pipe in gas drilling10.1016/j.engfailanal.2017.05.023 ↗
23. Some reflections on the past and future of erosion10.1016/0043-1648(95)07188-1 ↗
24. Practical estimation of erosion damage caused by solid particle impact: Part 1: Effects of impact parameters on a predictive equation10.1016/j.wear.2005.01.039 ↗
25. Inspection of internal erosion-corrosion of elbow pipe in the desalination station10.1016/j.engfailanal.2019.04.062 ↗
26. K.S. Tan, J.A. Wharton, R.J. Wood, Solid particle erosion-corrosion behaviour of a novel HVOF nickel aluminium bronze coating for marine applications - Correlation between mass loss and electrochemical measurements, Wear 258 (1–4 SPEC. ISS.) (2005) 629–640. doi:10.1016/j.wear.2004.02.019.10.1016/j.wear.2004.02.019 ↗
27. Slurry erosion surface damage under normal impact for pipeline steels10.1016/j.engfailanal.2018.03.019 ↗
28. Effect of impingement angle on slurry erosion behaviour and mechanisms of 1017 steel and high-chromium white cast iron10.1016/j.wear.2006.11.018 ↗
29. Slurry erosion of steel – Review of tests, mechanisms and materials10.1016/j.wear.2018.05.010 ↗
30. Y. Zhang, B.S. McLaury, S.A. Shirazi, E.F. Rybicki, A two-dimensional mechanistic model for sand erosion prediction including particle impact characteristics, NACE International Corrosion 2010 Conference & Expo (10378) (2010) 1–19.10.5006/C2010-10378 ↗
31. A.A. A276M-17, Standard Specification for Stainless Steel Bars and Shapes (2017). doi:10.1520/A0276_A0276M-17. URL www.astm.org.10.1520/A0276_A0276M-17 ↗
32. Modeling of erodent particle trajectories in slurry flow10.1016/j.wear.2015.04.013 ↗
33. Formation of eutectic carbides in Fe-Cr-Mo-alloy during non-equilibrium crystallization10.1016/j.matdes.2016.01.028 ↗
34. A threshold selection method from gray-level histograms10.1109/TSMC.1979.4310076 ↗
35. A note on a general definition of the coefficient of determination10.1093/biomet/78.3.691 ↗
36. The impact angle dependence of erosion damage caused by solid particle impact10.1016/S0043-1648(96)07430-3 ↗
37. ASTM G119-93, Standard Guide for Determining Synergism Between Wear and Corrosion, ASTM STANDARD 93 (Reapproved) (1994) 1–7. doi:10.1520/G0119-09.2.
38. Jet slurry corrosive wear of high- chromium cast iron and high-carbon steel grinding bali alloys10.5006/1.3584909 ↗
39. Microstructure aspects of a newly developed, low cost, corrosion-resistant white cast iron10.1007/s11661-012-1524-7 ↗
40. Relationships between pitting, stress, and stress corrosion cracking of line pipe steels10.5006/1.3585131 ↗
41. Caustic stress corrosion cracking of a spheroidal graphite cast iron: laboratory investigation10.1179/026708303225009535 ↗
42. 4.13 - Corrosion Fatigue
43. The effect of mechanical properties on erosion10.1016/0043-1648(88)90208-6 ↗
44. An integrated methodology for predicting material wear rates due to erosion10.1016/j.wear.2009.05.001 ↗
45. A numerical investigation of a geometry independent integrated method to predict erosion rates in slurry erosion10.1016/j.wear.2010.12.040 ↗
46. Erosion of surfaces by solid particles10.1016/0043-1648(60)90055-7 ↗