journal article·2019-11

Three-dimensional modeling of creep deformation in magnesium reduction retorts

M. Shahheidari, A. Sadeghi, M.H. Sadeghi

Publisher page

Abstract

Abstract Metallic magnesium is produced through a reduction reaction inside thick-walled tubes called retorts. Retorts operate at 1200 °C with an internal vacuum that causes high temperature creep deformation and short lifespan. This paper predicts retort creep deformation via three-dimensional (3D) finite element simulation using creep model constants obtained by experimental tests. Simulation results were verified by comparing the ovality of cross-sections along the axial length of an experimentally failed retort with
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Materials Engineering and Processing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. The Pidgeon process in China and its future
2. Experimental and numerical studies on a one-step method for the production of Mg in the silicothermic reduction process10.1021/acs.iecr.5b01830 ↗
3. Research Progress on Material and Service Life of the Magnesium-Smelting Reduction Pot
4. Study on the reduction jar used for MgMaking
5. The prevention of production of σ phase in refractory steel for Mg - reduction Jar
6. New heat-resistant alloy and production process used for Mg reduction pot
7. Research on new types of horizontal Mg-reduction jar
8. Study of new horizontal reduction jar in silicothermic process of magnesium metallurgical industry
9. Design of new type of vertical magnesium reduction jar
10. Analysis of high temperature failure and service life of magnesium metallurgy pot [J]
11. Microstructure Analysis of high temperature faited reducing retorts used in magnesium production
12. Damage analysis in Fe-Cr-Ni centrifugally cast alloy tubes for reforming furnaces10.1016/j.engfailanal.2013.09.020 ↗
13. Creep failures of overheated boiler, superheater and reformer tubes10.1016/j.engfailanal.2004.03.001 ↗
14. Failure analysis and creep remaining life of hydrogen reformer outlet pigtail tubes10.1016/j.engfailanal.2007.11.009 ↗
15. Evaluation of creep damage of INCOLOY 800HT pigtails in a refinery steam reformer unit10.1016/j.engfailanal.2014.07.017 ↗
16. A study of creep collapse of a long circular cylindrical shell under uniform external pressure10.2514/8.8243 ↗
17. Creep collapse of long cylindrical shells under high temperature and external pressure
18. The lifetime of a long cylindrical shell under external pressure at elevated temperature10.1016/0029-5493(72)90062-3 ↗
19. Bargmann · 1972 · 327
20. Simplified prediction of creep buckling of cylinders under external pressure. Part 1: finite element validation10.1016/S0997-7538(98)90507-1 ↗
21. Simplified prediction of the creep buckling of cylinders under external pressure. Part 2: experimental verification10.1016/S0997-7538(99)00149-7 ↗
22. A simplified method for predicting creep collapse of a tube under external pressure10.1115/1.2928619 ↗
23. Ioka · 1994
24. Creep collapse of a heat transfer tube subjected to external pressure at high temperatures10.1016/0029-5493(92)90024-P ↗
25. Breitbach · 1989 · 182
26. Stress and creep damage analysis for HTR heat exchangers at very high temperatures10.1016/0308-0161(85)90057-2 ↗
27. Microstructural and failure analysis of welded primary reformer furnace tube made of HP-Nb micro alloyed heat resistant steel10.1016/j.engfailanal.2016.05.023 ↗
28. Metallurgical evaluation of creep-failed superheater tubes10.1016/j.engfailanal.2008.09.012 ↗
29. Failure analysis and metallurgical transitions in SS 304L air pipe caused by local overheating10.1016/j.engfailanal.2015.10.014 ↗
30. Microstructure-based assessment of creep rupture behaviour of cast-forged P91 steel Chandan10.1016/j.msea.2017.04.037 ↗
31. Fracture behaviour of crept P91 welded sample for di ff erent post weld heat treatments condition10.1016/j.engfailanal.2018.08.029 ↗
32. High temperature creep failure in magnesium reduction retorts10.1016/j.engfailanal.2018.08.024 ↗
33. Estimation of Norton-Bailey parameters from creep rupture data10.1179/030634579790434312 ↗
34. An interactive approach to creep behavior modeling10.1016/j.msea.2008.04.090 ↗
35. Berla · 2008 · 488 · 594
36. An assessment of creep deformation and rupture behaviour of 9Cr – 1 . 8W – 0 . 5Mo – VNb (ASME grade 92) steel10.1016/j.msea.2015.05.068 ↗
37. Fundamental models for creep properties of steels and copper10.1007/s12666-015-0762-y ↗
38. A new magnesium reduction jar materials and manufacturing technologies
39. Mathematical modelling on dramatic temperature change of reduction retorts in pidgeon process10.4028/www.scientific.net/AMR.452-453.1215 ↗
40. 2004 · vol. 9
41. Creep-fatigue failure of an aero engine turbine blades10.1016/S1350-6307(01)00011-5 ↗
42. Creep fracture maps for 316 stainless steel10.1007/BF02811696 ↗
43. Crack and cavity nucleation at interfaces during creep10.1007/BF02643772 ↗
44. Numerical study of magnesium (Mg) production by the Pidgeon process: impact of heat transfer on Mg reduction process10.1016/j.ijheatmasstransfer.2012.09.027 ↗
45. Anisotropic creep damage and fracture mechanism of nickel-base single crystal superalloy under multiaxial stress