All ductile iron pipe producers use the annealing process to improve the metal structure. It lasts several hours in a hot air atmosphere, when the surface of pipes is covered by ferric oxide scale, consisting usually of two significantly different layers, being the subject of the research reported here. In the U.S.A., commercially produced pipes are not protected by zinc coatings, because it is believed that ferric oxides are not a solid undercoat for such coatings, while the EN 545:2010 standard used in Europe requires the use of zinc or zinc-aluminum coatings, depending on soil corrosivity. To evaluate which approach has more potential, it is necessary first of all to recognize the structure of ferric oxides after the annealing process and then to understand their role as a base for zinc coatings. The microstructure of oxide scales grown on the external surface of industrial ductile iron pipes was investigated using scanning electron microscopy. In the ductile iron matrix, the concentration of silicon is reported to be much lower than in the layer of oxide scale growing directly on the pipe surface. In several samples, some cracks between the oxide layers were not successfully avoided in spite of using a professional saw with a continuous cooling process. Each time the cracks were horizontal and occurred along two boundaries: between the ductile iron matrix and the first oxide layer or between the two oxide layers rich in silicon and essentially silicon free.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Sægrov · 2015 · 4 · 208
2. Principles for the selection of material and structural solutions for the construction of water supply mains
3. Ductile Iron Pipe Research Association, All pipe materials are not equal: Ductile Iron Pipe vs. Steel Pipe, 2016, p. 11.
4. Janco · 1992 · 96
5. Effect of mould wall thickness on rate of solidification of centrifugal casting
6. Ductile Iron Pipe Research Association, Installation Guide for Ductile Iron Pipe, 2016, p. 134.
7. EN 545:2010, Ductile iron pipes, fittings, accessories and their joints for water application – Requirements and test methods, p. 91.
8. National Research Council, Review of Bureau of Reclamation’s Corrosion Prevention Standards for Ductile Iron Pipe, Washington, DC: The National Academies Press, 2009, p. 172, https://doi.org/10.17226/12593.10.17226/12593 ↗
9. Pont-à-Mousson, Ductile Iron Pipes – Compendium, Nancy, France, 1986, p. 301.
10. Corrosion protection of ductile iron pipe10.5006/MP2005_44_1-24 ↗
11. Corrosion and corrosion control of iron pipe: 75 years of research10.1002/j.1551-8833.2005.tb10915.x ↗
12. Evaluating ductile iron pipe corrosion
13. F. Yilmaz, O. Cevner, B. Mustafa, Ductile iron pipes surface characterization and pinhole formation, in: 5th Int. Ankiros Foundry Congress, 11-13 Nov. 2010, Istanbul, p. 22.
14. L.G. Horn, The design decision model for corrosion control of ductile iron pipelines, 2018, p. 8. www.dipra.org (accessed 21.01.2020).
15. J. Jun, K. A. Unocic, M. Petrova, S.A. Shipilov, T. Carvalhaes, G. Thakur, J. Piburn, B.A. Pint, Methodologies for evaluation of corrosion protection for ductile iron pipe. Technical Report ORNL/TM-2017/144, Oak Ridge, 2019, p. 103, DOI: 10.2172/1528741.10.2172/1528741 ↗
16. An analysis of the elemental composition of micro-samples using EDS technique
17. A. Wassilkowska, New generation of water supply ductile iron pipes: microstructure and properties, Monografie Politechniki Krakowskiej, Kraków (in Polish), 2017, p. 127.
18. Oxidation of silicon containing steel10.1179/1743281212Y.0000000007 ↗
19. Microstructural and microtextural characterization of oxide scale on steel using electron backscatter diffraction10.1111/j.0022-2720.2004.01320.x ↗