journal article·2022-01

Failure analysis of areal gas distribution skirt plate

J.N. Mohapatra, Ravindra Kulkarni, D. Satish Kumar, G. Balachandran

Publisher page

Abstract

Abstract A detailed failure analysis was carried out on a skirt plate used in the reduction shaft of Corex plant at Areal Gas Distribution that failed after seven years of service. The analysis involved composition, hardness, mechanical properties, impact toughness, microstructure and phase analysis in the failed plate, and after solution annealing the plate for different lengths of time. It was found that the plate completely embrittled due to formation of massive Cr23C6 type carbides and σ- phase (FeCr) observed through microstructure and EDX analysis for prolonged service exposure at high temperature (∼ 850°C). The elongation of the steel was reduced to 1-4% and impact energy dropped to 5 Joule due to the embrittlement. The fracture surface showed intergranular brittle failure. After solution annealing treatment, the massive carbides and phases were mostly dissolved resulting in the restoration of the property. Hence it is suggested for solution annealing treatment in the in-service plates to improve their life. In addition, periodic monitoring of the plates through replica test and NDT could help in assessment of health of the plates for preventive measure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal Alloys Wear and Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. A Study on the Failure of AISI 304 Stainless Steel Tubes in a Gas Heater Unit
2. D. H. Herring, Sigma-Phase Embrittlement, Feb. 29 (2012), https://www.industrialheating.com/articles/90371-sigma-phase-embrittlement.
3. Overview of Intermetallic Sigma (σ) Phase Precipitation in Stainless Steels
4. The sigma phase transformation in austenitic stainless steels
5. Effect of composition on embrittlement of austenitic stainless steels
6. Comparative study on sigma phase precipitation of three types of stainless steels: austenitic, super ferritic and duplex10.1179/174328406X109230 ↗
7. Microstructural changes and corrosion resistance of AISI 310S steel exposed to 600–800 °C10.1016/j.matchar.2008.12.005 ↗
8. Study of embrittlement in austenitic stainless steel AISI304H with 15 years in service exposed to high temperature
9. TEM Examination of Precipitation Behaviour of M23C6 and Sigma Phases and Dislocations in SS 310S under Creep Deformation at 800°C10.1017/S1431927615003724 ↗
10. Isothermal and cyclic ageing of 310S austenitic stainless steel10.1007/s11661-017-4073-2 ↗
11. Turbine housing failure due to sigma phase precipitation and embrittlement of niobium-stabilized austenitic steel casting10.1007/s11665-020-04626-y ↗
12. Z. Kubon, S. Stejskalova, L. Kander, Effect of sigma phase on fracture behavior of steels and weld joints of components in power industry working at super critical conditions, Intech Open Book Series, Open access peer-reviewed chapter, December 20, (2017), https://doi:10.5772/intechopen.71569.10.5772/intechopen.71569 ↗
13. A Multi-Purpose Austenitic Heat Resistant Stainless Steel with Oxidation Resistance Under Mildly Cyclic Conditions to 2010°F (1100°C), https://www.sandmeyersteel.com/images/310-Spec-Sheet.pdf.