journal article·2024-07

Two fatigue fracture modes at different temperatures of 10%Cr heat-resistant steel weldment filled with Ni-based alloy

Qunbing Zhang, Lina Ren, Xiaowei Lei, Wenlan Wei, Jianxun Zhang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Advanced Ultra-Supercritical Coal-Fired Power Plant with Post-Combustion Carbon Capture: Analysis of Electricity Penalty and CO2 Emission Reduction10.3390/su13020801 ↗
2. Creep damage in 9–12% Cr steel notched components: Microstructural evolution and stress state dependence10.1016/j.ijpvp.2023.104977 ↗
3. A study on as-welded microstructure and mechanical properties of thick-walled 9Cr3W3Co1CuVNbBN martensitic steel weldment10.1016/j.ijpvp.2023.105077 ↗
4. Microstructure development of modified 9Cr-1Mo steel during laser powder bed fusion and heat treatment
5. Near-threshold fatigue crack growth behavior of 10% Cr martensitic steel welded joint with 9% Cr weld metal in high temperature air10.1016/j.ijfatigue.2020.105650 ↗
6. Numerical and experimental investigation on distribution of residual stress and the influence of heat treatment in multi-pass dissimilar welded rotor joint of alloy 617/10Cr steel10.1016/j.ijpvp.2022.104715 ↗
7. Numerical and experimental investigations on the temperature field in local post weld heat treatment of 9 % Cr heat resistant steel welded pipes10.1016/j.jmatprotec.2021.117232 ↗
8. Microstructure evolution and its effect on the stress rupture behavior of 9%Cr-CrMoV dissimilar welded joint10.1016/j.engfailanal.2023.107071 ↗
9. Coupled effect of temperature and stress on the microstructure and stress rupture behavior of 9% Cr-CrMoV dissimilar welded joints10.1016/j.engfailanal.2021.105945 ↗
10. Effect of nickel-based filler metal types on creep properties of dissimilar metal welds between Inconel 617B and 10% Cr martensitic steel10.1016/j.jmrt.2021.07.131 ↗
11. Evolution of microsegregation-induced precipitations and bending fracture mechanisms of 9% Ni steel weldments filled with nickel-based alloys10.1016/j.jmrt.2023.07.178 ↗
12. Microstructure of 10% Cr martensitic heat-resistant steel welded joints and type IV cracking behavior during creep rupture at 650°C10.1016/j.msea.2015.04.062 ↗
13. The heterogeneous microstructure of laser welded joint and its effect on mechanical properties for dissimilar 9Cr steel and alloy 61710.1016/j.jmrt.2023.07.281 ↗
14. Low-cycle fatigue behaviors of a new type of 10% Cr martensitic steel and welded joint with Ni-based weld metal10.1016/j.ijfatigue.2016.03.003 ↗
15. Assessment of fatigue and electrochemical corrosion characteristics of dissimilar materials weld between alloy 617 and 12 Cr steel10.1016/j.jmapro.2020.02.038 ↗
16. Rupture behavior and fracture mode for Inconel 625–9% Cr steel dissimilar welded joints at high temperature10.1016/j.engfailanal.2021.105412 ↗
17. Creep rupture properties of dissimilar metal weld between Inconel 617B and modified 9%Cr martensitic steel10.1016/j.msea.2019.138185 ↗
18. Two stress rupture modes observed in Alloy 617–9%Cr dissimilar welded joint10.1016/j.matlet.2019.126978 ↗
19. Macrosegregation induced interface structure and its effect on creep failure in dissimilar metal welds between Ni-based alloy and 10% Cr martensitic steel10.1016/j.msea.2021.141847 ↗
20. Low cycle fatigue properties of a 9–12% Cr martensitic steel welded joint with Ni-based weld metal based on a local strain approach10.1016/j.engfailanal.2022.106347 ↗
21. Failure competition behavior of 9Cr/617 dissimilar welded joint during LCF test at elevated temperature10.1016/j.msea.2019.138810 ↗