Evidence of gas permeation in electrostatically painted steel cylinders
Source abstract
Abstract
Abstract The process of gas generation, entrapment and subsequent permeation through coatings applied on the surface of metals for corrosion protection purposes is the cause for the development of a defect known as “fish-scaling”. Particularly, in operations like enamelling or painting of metals, this phenomenon affects strongly the surface quality of the items and the development of further processing operations. In this work, the reasons that promote the development of defects in electrostatically painted steel during the manufacture route of fire extinguishers are analysed. The surface and cross section analyses of the samples conducted by optical and scanning electron microscopy suggest that the degradation of the coating is caused by gas migration from the metal-coating interface to the surface of the cylinders. Water used during cleaning and descaling operations acted as a potential gas source being hydrogen the element responsible for the formation of both, structural defects in the coating and cracks in the steel substrate. The degradation mechanisms of the steel and the coatings are found and explained in terms of manufacturing process of the cylinders.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Causes for fish scaling on enamel steels
2. Effect of “fishscale” defect on the protective properties of enamel coatings
3. An analysis of the microstructure and interfacial chemistry of steel–enamel interface10.1016/S0040-6090(03)00973-8 ↗
4. The effects of a nickel oxide precoat on the gas bubble structures and fish-scaling resistance in vitreous enamels10.1016/j.msea.2003.08.003 ↗
5. Development of cold rolled steel sheet DC01EK for enameling and fish-scaling resistance
6. Failure of vitreous enamelled coatings10.1016/1350-6307(96)00017-9 ↗
7. Failure analysis of enamel-coated carbon steel heating elements of gas-gas heater for fuel gas desulfurization system10.1016/j.engfailanal.2006.02.009 ↗
8. Characterization of organic coatings on metal substrates by electrochemical impedance spectroscopy10.5006/1.3585095 ↗
9. Corrosion protection by organic coatings: electrochemical mechanism and novel methods of investigation10.1016/S0013-4686(00)00348-0 ↗
10. The detection and mapping of defects in organic coatings using local electrochemical impedance methods10.1149/1.1392593 ↗
11. Defect dimension evaluation in organic coated galvanized steel by electrochemical impedance spectroscopy10.1023/A:1020558416074 ↗
12. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
13. Absorption and transport of hydrogen during gas metal arc welding of low alloy steel10.1179/stw.1997.2.4.174 ↗
14. Gedeon SA. Hydrogen assisted cracking of high resistance steel welds, Ph.D thesis Massachusetts Institutue of Technology; 1987.10.21236/ADA196738 ↗
15. Hydrogen-induced intergranular fracture of steel10.1016/S0013-7944(00)00124-7 ↗
16. Investigation of hydrogen embrittlement failure in a steam separator by field metallography10.1016/j.engfailanal.2012.11.001 ↗
17. A comparative study of hydrogen induced cracking behavior in API 5L X60 and X70 pipeline steels10.1016/j.engfailanal.2013.04.028 ↗
18. Failure analysis of a crude oil pipeline10.1016/j.engfailanal.2006.12.001 ↗
19. Surface defects in drying paint films10.1016/0300-9440(80)80019-1 ↗
20. Basic principles and advantages of the electrostatic paint spraying process10.1108/eb020133 ↗
21. Thin films with high surface tension10.1137/S003614459529284X ↗
22. Diffusion and evolution of hydrogen from steel
23. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
24. The fracture of metals