Hardness and failure assessment of a hot extrusion punch during service
Source abstract
Abstract
To explore the evolution of the microstructure, properties, and failure mechanism of a hot extrusion punch during service, a hot extrusion experiment was carried out on a home-designed testing platform, enabling multiple analyses at an elevated temperature of 950℃. The microstructure was evaluated using optical microscopy, scanning electron microscopy, and other analytical methods. The results showed that the punch could continue working 850 times before it failed. The primary failure mode was ascribed to local plastic deformation, accompanied by apparent oxidation and wear at the bottom and working area. The extended analysis also revealed that the ferrite content in the matrix increased in the entire working zone and that the overall microstructure exhibited a fibrous morphology instead of lath features, where the tiny carbide particles were homogeneously distributed. This suggested that significant plastic deformation occurred during service. Moreover, the carbide particles were further fragmented and well dispersed with plastic deformation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgy and Material Forming · Aluminum Alloys Composites Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. A review on thermal fatigue behavior of hot working mould steel[J]
2. Investigation on high temperature wear behavior of a newly developed hot-work tool steel[J]
3. Formation Mechanism of Primary Carbide in H13 Steel During Electroslag Remelting Process[J]
4. Effect of niobium on microstructure of cast AISI H13 hot work tool steel[J]10.1016/S1006-706X(08)60145-4 ↗
5. Influence of cooling rate on phase formation in spray-formed H13 tool steel[J]10.1016/j.msea.2007.05.121 ↗
6. Effect of annealing process on spheroidized microstructureand mechanical properties of H13 steel[J]
7. The Study of the Chemical Composition and Improvement and Development for the H13 Hot Work Mould & Mold Steel[J]
8. Effect of heat treatment on service life of H13 steel bar extruding die [J]
9. Precipitation Behaviors and Strengthening of Carbides in H13 Steel during Quenching [J]
10. Fracture Analysis on Hot Extrusion Mould of 4Cr5MoSiV1 Steel[J]
11. Analysis on H13 Steel Extrusion Die Failure[J]
12. Analysis of wear of a gas nitrided H13 tool steel mould in aluminium extrusion[J]10.1016/j.engfailanal.2012.07.016 ↗
13. General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China, Standardization Administration. GB/T 228.1-2010.Matallic materials Tensile testing Part 1: Method of test at room temperature[S].Beijing: Standards Press of China, 2010.
14. Failure Analysis of 4Cr5MoSoV1 Steel Hot Extrusion Die [J]
15. Failure analysis of hot extrusion die based on dimensional metrology, micro-characterization and numerical simulation — A case study of Ti alloy parts [J]10.1016/j.engfailanal.2016.12.015 ↗
16. Failure Analysis of Hot Extrusion Mold for High-strength Steel [J]
17. A Comparison of wear resistance of two types hot-work mould steels at high temperature [J]