journal article·2011-01

Failure analysis of a stainless steel hydrotreating reactor

W.B. Kan, H.L. Pan

Engineering Failure Analysis· Volume 18· Issue 1
Publisher page

Abstract

Abstract This paper presents an analysis of a failed AISI 316L austenitic stainless steel (SS) hydrotreating reactor that produces flavors and fragrances. Pitting and cracking were observed mainly in the vicinity of the circumferential and longitudinal shell welds on the internal surface of the reactor by dye penetrant testing (DPT). Ultrasonic evaluation revealed the cracks were within near-surface area, therefore remedial grinding was performed to remove them. In situ metallographic investigation revealed that the cracks were predominantly transgranular and multi-branching. Thickness gauge, hydraulic pressure testing, and acoustic emission validated the reusability of the repaired vessel. Analysis of the catalysts showed the source of chloride. SCC (stress corrosion cracking) susceptibility testing of the identical material proved its liability to chloride SCC in the environment of the suspect catalysts. Studies revealed that the failure was caused by chloride SCC. Recommendations are made to prevent the recurrence of the similar failure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Minerals Flotation and Separation Techniques · Materials Engineering and Processing · Marine and Offshore Engineering Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Sedriks · 1979
2. Bafna VK, Haribhakti PU. In situ metallography for the plant health assessment study and failure investigation. In: 4th middle east NDT conference and exhibition. Kingdom of Bahrain; 2007.
3. ASTM D5808-09a:Standard test method for determining chloride in aromatic hydrocarbons and related chemicals by microcoulometry. West Conshohocken, PA: ASTM International; 2009.
4. ASTM D5453-09:Standard test method for determination of total sulfur in light hydrocarbons, spark ignition engine fuel, diesel engine fuel, and engine oil by ultraviolet fluorescence. West Conshohocken, PA: ASTM International; 2009.
5. ASTM G30-97:Standard practice for making and using U-bend stress-corrosion test specimens. West Conshohocken, PA: ASTM International; 2009.
6. Fontana · 1986
7. Failure analysis of a stainless steel pipeline10.1016/j.engfailanal.2007.05.002 ↗
8. The stress corrosion cracking behavior of austenitic stainless steels in boiling magnesium chloride solutions10.1016/j.corsci.2006.12.023 ↗
9. Timmins PF, International ASM. Solutions to hydrogen attack in steels. Materials Park, OH: ASM International; 1997.
10. Hydrogen-induced cracking in two linepipe steels10.1007/BF02431612 ↗
11. Martensite transformation and surface cracking of hydrogen charged and outgassed type 304 stainless steel10.1016/S0921-5093(00)00833-9 ↗
12. Stress corrosion cracking of cold-worked austenitic stainless steels10.1016/0010-938X(82)90055-5 ↗