journal article·2012-01

Failure analysis of perforation in salty water-wall tubes of a power plant

Mohammad Dorri, Davoud Harandizadeh

Publisher page

Abstract

Abstract Perforation of water-wall of saline panels in Shahid-Montazeri power plant led to some systematic serious problems. XRD and XRF investigation along with spectrometric and metallographic analysis proved that perforation is mainly due to caustic corrosion. Moreover; it was concluded that significant amount of copper ions entered into the water circulation line and caused higher corrosion rate. It’s evident that variation in oxygen concentration and base metal decarburization were also effective in corrosion deterioration. Reduction in water-wall over-deposition and regular descaling along with modification of heating rate and replacing lithium hydroxide and ammonia with suitable modifiers, helped to overcome the problem.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Corrosion and its inhibition in SA213-T22 TIG weldments used in power plants under neutral and alkaline environments10.1016/j.msea.2006.06.051 ↗
2. ASM metals handbook, vol. 13. 9th ed.; 1992. p. 986–93.
3. Lessons learned from the examination of tubes pulled from electricité de France steam generators10.1016/S0029-5493(96)01364-7 ↗
4. Port · 1991
5. Boiler tube failures (BTFs) in natural circulation high pressure drum boiler of a power station
6. Nalco Company, Product Data Sheet, Number 2814.
7. Modern power station practice. Chemistry and metallurgy, vol. 5. Central Electricity Generating Board, Pergamon Press.
8. Port Robert · 1991
9. Fontana · 1986
10. Some aspects of metallurgical assessment of boiler tubes—basic principles and case studies10.1016/j.msea.2006.06.026 ↗
11. Failure causes of cracking and bending of boiler superheater tube in power plant
12. Metallurgical investigation of failed boiler water-wall tubes received from a thermal power station10.1016/j.engfailanal.2010.06.004 ↗
13. Malik AU, Andijani I, Mobin M, Al-Muaili F, Al-Hajri M. Corrosion of boiler tubes some case studies. In: 4th SWCC Acquired Experience Symposium, Jeddah; 2005. p. 739–63.
14. A pictorial review of failures in conventional boiler plant10.1016/0308-0161(75)90002-2 ↗
15. Failure analysis of 101-C ammonia plant-heat exchanger10.1016/S1350-6307(03)00016-5 ↗
16. Failure analysis of boiler cold and hot reheater tubes10.1016/j.engfailanal.2006.03.007 ↗
17. Lessons learned from the examination of tubes pulled from electricité de France steam generators10.1016/S0029-5493(96)01364-7 ↗