journal article·2014-11

Erosive failure of steel pipeline by solid pulverized particles

Eva Zdravecká, Ján Slota, Jana Tkáčová

Publisher page

Abstract

Abstract In the power industry, abrasion and erosion wear are important cost generating factors during the transport of pulverized coal. The causes of failures during the transport of pulverized fuel are due to cyclic loading and corrosion resulting in erosive wear, plastic deformation and fatigue. Due to damage of target surface it is important to pay attention to investigate the problems of erosive failures by solid particles impingement. The practical problem solving low life-time of the piping system is presented. To solve the problems of real erosion wear the experimental erosive wear tests were applied. The erosion tests were carried out by the stream of SiO2 sand particles with an average size 0.8 mm at an impact velocity of 50 m/s, under impact angles 15°, 45° and 90°. To validate the applied simulation model, the simulation results were compared to measured data from real field application and they demonstrate good conformity with prediction of all erosion models considered over a range of conditions, including particle impact angle, impact speed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · Particle Dynamics in Fluid Flows · Coal Combustion and Slurry Processing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Modelling of pipe bend erosion by dilute particle suspensions10.1016/j.compchemeng.2012.02.006 ↗
2. Influence of microstructure on erosion resistance of steels10.1016/j.wear.2009.08.004 ↗
3. Erosion caused by impact of solid particles10.1016/S0161-9160(13)70071-1 ↗
4. The mechanism of erosion of ductile metals
5. The impact angle dependence of erosion damage caused by solid particle impact10.1016/S0043-1648(96)07430-3 ↗
6. Solid particle erosion behaviour of metallic materials at room and elevated temperatures10.1016/S0301-679X(96)00064-3 ↗
7. Hutchings · 1992
8. Failure analysis of overhead power line yoke connector10.1016/j.engfailanal.2013.04.024 ↗
9. Causes of failure and repairing options for dies and molds: a review10.1016/j.engfailanal.2013.09.006 ↗
10. A comprehensive procedure to estimate erosion in elbows for gas/liquid/sand multiphase flow10.1115/1.2131885 ↗
11. Kmec J, Sobotová L, Dobrovič J, Bičejová L, Gombár M. Categories of hydroerosion factors. RAM Verlag. 153p. ISBN 978-3-942303-11-8.
12. Analysis of a boiler pipe rupture10.1016/j.engfailanal.2004.10.015 ↗
13. The final report of operational tests of the MO 21 piping system oriented on the structure of the applied materials. Košice. SjF TU, Košice 1997, p. 26.
14. Fatigue crack growth in micro-alloyed steels with polyhedral and non-polyhedral microstructure
15. A study of erosion phenomena: Part I10.1016/0043-1648(63)90003-6 ↗
16. Erosive wear of metallic materials and HVOF coatings
17. fa US Steel Slovakia, .
18. Kleis · 2008