Failure of a pressure vessel for rail transport of fluid carbon dioxide
Source abstract
Abstract
Abstract In 1976, a pressure vessel of a tank wagon burst during gravity shunting. The pressure vessel was filled with cold fluid carbon dioxide and failed by cleavage fracture explosively. Big parts of the vessel were flung up to 300 m, a building was destroyed, and rails as well as the superstructure of the gravity shunting yard were damaged. The initiation sites of the fracture and the orientations of crack propagation were determined by means of the patterns on the fracture surfaces of the broken parts. The initiation sites were located in the heat-affected zone (HAZ) of welds, close to transitions of cross-sections and the starting and end points, respectively, of the welds. The primary initiation of crack propagation was almost certainly on the left side, close to the weld of the fixed bearing connecting the vessel with the carriage. The results of metallographic investigations indicated the development of cold weld cracks during welding. Mechanical behavior assessments on specimens extracted from the failed vessel indicated sufficient strength and ductility in tensile loading. The values of the notched-bar impact energy or toughness were within the limits according to industry rules and standards, except for one metal sheet of the vessel that was welded to the left fixed bearing. During shunting, two tank wagons were inappropriately braked, and began to roll too quickly. One rail brake used for deceleration of the wagons caused impulsive noises and vibrations, resulting in high impulsive loading of the first wagon. The cold weld cracks in the heat-affected zones near the fixed bearing of the pressure vessel were initiation points for unstable crack growth. As the result of very low notched-bar impact toughness, crack propagation was not arrested and unstable cleavage fracture occurred. Due to a second similar accident, happened one year before, a program was started to assess characteristic values of pressure vessel materials and the influence of weld parameters by the manufacturer, the inspecting authority, and BAM. The scientific findings led to modifications of industry rules and standards with regard to using ISO-V specimens and to higher required values for notched-bar impact energy for fine grain structural steels.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Material Properties and Failure Mechanisms · Mechanical Failure Analysis and Simulation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. “BAM test report 1.2/11123”, 20.Juli 1977.10.1017/S0312897000014338 ↗
2. Martens A. Results of the investigations of fractured iron bottles for storage of hydrogen gas (in German). Mittheilungen aus den königlich-technischen Versuchsanstalten zu Berlin, No 1; 1896. p. 2–36
3. Regulation for train operation DV 408 (“Fahrdienstvorschrift”) in German, Deutsche Bahn.
4. Böllinghaus T, Bauer M. INVESTIGATION OF IRON CONTAINERS FOR STORAGE OF HYDROGEN GAS, Translation of Adolf Martenś Spectacular Failure Investigation Report published in 1896, EFA, Special Issue “A Tribute to A. Martens”; 2014.10.1016/j.engfailanal.2014.03.018 ↗
5. 1975
6. 1951
7. 1975
8. DIN 50121 Folding tests on welds (“Faltversuch an Schweißverbindungen”) in German, Berlin: Beuth Verlag.
9. 1975
10. Investigations of the MV Kurdistan casualty10.1016/S1350-6307(96)00030-1 ↗
11. Valluri SR, Taplin DMR, Ram Rao P, Knott JF, Dubey R. Fractography and mechanism of hydrogen cracking – the fisheye concept, Advances in Fracture Research. Proceeding of 6th International Conference on Fracture (ICF 6), New Delhi; 1984. p. 2459–66.10.1016/B978-1-4832-8440-8.50254-4 ↗
12. VdTÜV 12-298 Fine grain structural steel BH51S (“Feinkornbaustahl”), Essen: Vereinigung der Technischen Überwachungs-Vereine e.V.; April 1968.
13. 1961
14. SEW 089-70 Weldable fine grain structural steels (“Schweißbare Feinkornbaustähle”), Düsseldorf: Verlag Stahleisen GmbH; 1970.
15. “BAM-Bericht, Begründung für die Neufestsetzung der Kerbschlagzähigkeit hochfester Feinkornbaustähle für Tanks für den Transport gefährlicher Güter”, BAM, Berlin; 12.1.1983.
16. BAM internal investigations on materials of pressure vessels for transportation of fluid carbon dioxide, BAM, Berlin; 1982.
17. 1983
18. AD-Merkblatt W10 Materials for low temperatures (“Werkstoffe für tiefe Temperaturen”) in German, Essen: Verband der Technischen Überwachungs-Vereine e.V; 1972.
19. AD-Merkblatt W10 Materials for low temperatures (“Werkstoffe für tiefe Temperaturen”) in German, Berlin: Verband der Technischen Überwachungs-Vereine e.V; 2007.
20. 1993