journal article·2024-08Open access

Root cause analysis of coining tool failure with proposed solution to extend its service life

Miroslava Ťavodová, Pavel Beňo, Jana Luptáková, Dana Stančeková, Nataša Náprstková, Katarina Monkova

Abstract

• Root causes analysis of the coining tool failure served as a tool for revealing the causes of damage and early decommissioning of the punch. • The cause of crack initiation was plastic deformation during pressing, hardening during martensitic transformation, and improper chroming process. • The cracks appeared outside the relief of the coining die, and also in the core of its working part. • Changes in production allowed for a 148-fold increase in the number of minted coins produced by a single minting tool. The article deals with a root cause analysis of coining tool failure after its untimely discarding and the design to extend its service life by innovating the manufacturing process. The analysis was performed on the coining die which had to be put out of service due to the insufficient quality of minted stainless coins. The purity of steel and the microstructure of the material of the semi-finished goods were evaluated. Furthermore, an analysis of the coining die failure under the surface and in the core was performed as well as the state of the chromium layer failure on the coining die relief. Based on the results of the analysis, a new experimental coining die was designed and produced according to an innovative manufacturing process. The pressing of the relief was carried out in a vacuum furnace and relief was coated with a TiAlN by the PVD method. New processes introduced in the production of coining die prevented the failure of die punches, extended the time of operation, thereby increasing quality of the coin production.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced machining processes and optimization · Engineering Diagnostics and Reliability · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. The research of options for the innovation heat treatment of the tools for coinage in order to increase their lifetime10.21062/ujep/x.2016/a/1213-2489/MT/16/1/274 ↗
2. Kalincová, D., Kaštan, R. Increasing the service life of the relief of punches by chrome plating. Acta facultatis technicae. 2011, Vol. XVI, No. 2.
3. Mori, H. et al. Surface Improvement of Coining Dies with DLC Films, Procedia Engineering, 81, 2014, 1933-1938, ISSN 1877-7058, https://doi.org/10.1016/j.proeng.2014.10.259.10.1016/j.proeng.2014.10.259 ↗
4. Die wear in stamping of advanced high strength steels – Investigations on the effects of substrate material and hard-coatings10.1016/j.triboint.2012.02.016 ↗
5. Pelcastre, L. et al. Investigations into the damage mechanisms of form fixture hardening tools, Engineering Failure Analysis, Volume 25, 2012, Pages 219-226, ISSN 1350-6307, https://doi.org/10.1016/j.engfailanal.2012.05.014.10.1016/j.engfailanal.2012.05.014 ↗
6. Fatigue life prediction model of WC-Co cold forging dies based on experimental and numerical studies10.1016/j.engfailanal.2020.104910 ↗
7. ISO 4967:2013 Steel - Determination of content of non-metallic inclusions - Micrographic method using standard diagrams.
8. EN · 2007 · 10247
9. ASTM E45 Determining the Inclusion Content of Steel.
10. SS111116:2019 Jernkontoret’s inclusion chart II for quantitative assessment of the content of non-metallic inclusions in metals and alloys.
11. Kazakov, A., Zhitenev, A., Ryaboshuk, S. Interpretation and Classification of Non-Metallic Inclusions 2016 Materials Per-formance and Characterization 510.1520/MPC20160040 ↗
12. (3) August 2016, DOI: 10.1520/MPC20160040.10.1520/MPC20160040 ↗
13. Computer Simulations of Mechanical Properties of Steel Dies10.1080/10426910902806202 ↗
14. Evaluation of the potential of tool materials for the cold forming of advanced high strength steels10.1016/j.wear.2013.01.001 ↗
15. Coating surface roughness measurement made on coining dies10.21062/ujep/x.2014/a/1213-2489/MT/14/3/309 ↗
16. Degradation Processes in the Contact Layers of Forming Tools
17. Fitrullah, M. et al. The Improvement of Product Quality and Production Capacity of Metal Coin Dies by Tempering Treatment and PVD TiN Coating in IsodurTM Steel. Advanced Materials Research, vol. 1112, Trans Tech Publications, Ltd., July 2015, pp. 323–328. Crossref, doi:10.4028/www.scientific.net/amr.1112.323.10.4028/www.scientific.net/AMR.1112.323 ↗
18. Determination of a hardening behaviour law for a cold forging TiN-coated tool steel10.1016/S0257-8972(00)00558-2 ↗
19. Böhler steel https://www.bohler.cz/cs/products/k455/.
20. Jakubéczyová, D. et al. Testing of PVD Hard Coatings Applied to Coining Dies. Materials Science Forum, vol. 818, Trans Tech Publications, Ltd., May 2015, pp. 27–31. Crossref, doi:10.4028/www.scientific.net/msf.818.27.10.4028/www.scientific.net/MSF.818.27 ↗
21. Analysis of Integrity of Surface of Hardened Chromium-Nickel Steel after Finishing Grinding10.21062/ujep/186.2018/a/1213-2489/MT/18/5/833 ↗
22. Quality of chrome layers of coining dies and its impact on their reliability and lifetime in operation
23. Modern Coating of Coins and Coinage
24. Mechanical damage of hard chromium coatings on 416 stainless steel10.1016/j.engfailanal.2016.04.011 ↗
25. Single layer and multilayer wear resistant coatings of (Ti, Al)N: a review10.1016/S0921-5093(03)00473-8 ↗
26. Impact of fracture toughness on surface properties of PVD coated cold work tool steel10.1016/j.surfcoat.2015.07.021 ↗
27. Industrial applications of PACVD hard coatings
28. Brezinová, J. et al. Selected Properties of Hardfacing Layers Created by PTA Technology January 2021 Metals - 11(1):134 DOI: 10.3390/met11010134.10.3390/met11010134 ↗
29. Emamverdian, A. A. et al. Current failure mechanisms and treatment methods of hot forging tools (dies) - a review, Engineering Failure Analysis, Volume 129, 2021, 105678, ISSN 1350-6307.10.1016/j.engfailanal.2021.105678 ↗
30. Weonwoong, K., Eungsun, B., Bon H. K. Damage cause analysis of coating failure of pot roll for hot-dip aluminizing, Engineering Failure Analysis, Volume 154, 2023, 107692, ISSN 1350-6307.10.1016/j.engfailanal.2023.107692 ↗
31. Jurko · 2006
32. Environmentally induced changes in fatigue life and durability of marine structures and vessels10.1016/j.prostr.2022.12.100 ↗
33. Characterization of thin PVD coatings deposited on PM high speed steel
34. Wear-resistant diffusion coatings on steels for punching and coining dies10.1007/BF00776898 ↗
35. González-Velázquez, J.L., Entezari, E. On the assessment of non-metallic inclusions by part 13 of API 579 -1/ASME FFS-1 2016, Procedia Structural Integrity, Volume 33, 2021, 221-228, https://doi.org/10.1016/j.prostr.2021.10.027.10.1016/j.prostr.2021.10.027 ↗
36. Surface Characterization and Performance Evaluation of Nitrogen Implanted Coinage Dies10.3390/pr10030479 ↗
37. The effect of risk volume on the fatigue life of stainless steels subjected to high-frequency loading10.1016/j.prostr.2023.10.081 ↗
38. Investigation of the effect of shape of inclusions on homogenized properties by using peridynamics10.1016/j.prostr.2020.11.124 ↗
39. An investigation into the role of non-metallic inclusions in cleavage fracture of medium carbon pearlitic steels for high-speed railway wheel10.1016/j.engfailanal.2021.105860 ↗
40. A novel methodology for fatigue assessment of high strength steels with non-metallic inclusions10.1016/j.prostr.2022.03.123 ↗
41. Defects as a root cause of fatigue failure of metallic components. II: Non-metallic inclusions
42. Entezari, E. et al., An experimental and statistical study on the characteristics of non-metallic inclusions that serve as hydrogen-induced crack nucleation sites in pipeline steel, Engineering Failure Analysis, Volume 154, 2023, 107695, ISSN 1350-6307, https://doi.org/10.1016/j.engfailanal.2023.107695.10.1016/j.engfailanal.2023.107695 ↗
43. Holubář, P., Computer simulation of the growth of PVD coatings and a new series of three-layer coatings [online]. 2008 http://www.mmspektrum.com/clanek/pocitacova-simulace-rustu-pvd-povlaku-a-nova-rada-trojvrstvych-povlaku.htm.
44. Khattak, M. A., Failure Investigation of Welded 430 Stainless Steel Plates for Conveyor Belts. Engineering Failure Analysis, 104754. 2020. doi:10.1016/j.engfailanal.2020.104754.10.1016/j.engfailanal.2020.104754 ↗
45. Experimental investigation on the effect of tensile pre-strain on ratcheting behavior of 430 Stainless Steel under fully-reversed loading condition10.1016/j.engfailanal.2010.12.008 ↗
46. Material Data Sheet 1.4016 (X6Cr17) chrome-extension://efaidnbmnnnibpcajpcglclefindmkaj/https://d2zo35mdb530wx.cloudfront.net/_legacy/UCPthyssenkruppBAMXUK/assets.files/material-data-sheets/stainless-steel/stainless-steel-1.4016-430.pdf.
47. VIRGAMET https://virgamet.com/x6cr17-1-4016-aisi-430-z8c17-uns-s43000-x8cr17-430s17-stainless-steel.
48. Defects as a root cause of fatigue failure of metallic components. I: Basic aspects10.1016/j.engfailanal.2019.01.055 ↗
49. Failure Investigation of Products and Components in Metal Forming Industry: Root Cause Analysis and Process-Based Approach10.1007/s11668-020-00801-4 ↗
50. Pantazopoulos · Failure Mechanisms in Alloys. Metals · 2020 · 10 · 117
51. Applying fracture mechanics to fatigue strength determination – some basic considerations10.1016/j.ijfatigue.2019.05.009 ↗
52. ISO 6508-1:2023 Metallic materials — Rockwell hardness test — Part 1: Test method.