journal article·2025-10

Impact of chemical composition on hydrogen-induced ductility loss and tensile properties of Cu–Al–Ni–Fe–Mn cast alloys

Junichiro Yamabe, Takafumi Yano, Shinya Honda, Kojiro Fujiyama

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Matsunaga · 2024
2. Nagumo · 2023
3. Review of the hydrogen embrittlement and interactions between hydrogen and microstructural interfaces in metallic alloys: grain boundary, twin boundary, and nano-precipitate10.1016/j.ijhydene.2024.05.257 ↗
4. Hydrogen trapping and embrittlement in metals – a review10.1016/j.ijhydene.2024.04.076 ↗
5. Hydrogen effects on plasticity10.1016/S1572-4859(09)01504-6 ↗
6. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
7. The role of hydrogen and other interstitials in the mechanical behavior of metals10.1007/s13632-016-0319-4 ↗
8. Influence of hydrogen-enhanced plasticity and decohesion mechanisms of hydrogen embrittlement on the fracture resistance of steel10.1016/j.engfailanal.2021.105312 ↗
9. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
10. Effect of multiple hydrogen embrittlement mechanisms on crack propagation behavior of FCC metals: competition vs. synergy10.1016/j.ijplas.2021.103023 ↗
11. Hydrogen-related failure of steels – a new aspect10.1179/026708304225019687 ↗
12. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
13. On the physical differences between tensile testing of type 304 and 316 austenitic stainless steels with internal hydrogen and in external hydrogen10.1016/j.ijhydene.2010.06.018 ↗
14. Hydrogen embrittlement susceptibility of a high strength steel X8010.1016/j.msea.2010.07.027 ↗
15. Hydrogen uptake in austenitic stainless steels by exposure to gaseous hydrogen and its effect on tensile deformation10.1016/j.corsci.2011.04.022 ↗
16. Comparison of hydrogen embrittlement in three pipeline steels in high-pressure gaseous hydrogen environments10.1016/j.corsci.2012.01.028 ↗
17. Hydrogen embrittlement properties of stainless and low alloy steels in high pressure gaseous hydrogen environment
18. Surface coating with a high resistance to hydrogen entry under high-pressure hydrogen-gas environment10.1016/j.ijhydene.2013.05.152 ↗
19. Effects of hydrogen on tensile properties and fracture surface morphologies of Type 316L stainless steel10.1016/j.ijhydene.2013.12.099 ↗
20. Criteria for determining hydrogen compatibility and the mechanisms for hydrogen-assisted surface crack growth in austenitic stainless steels10.1016/j.engfracmech.2015.12.023 ↗
21. Effect of strain rate on hydrogen embrittlement susceptibility of twinning-induced plasticity steel pre-charged with high-pressure hydrogen gas10.1016/j.ijhydene.2016.06.259 ↗
22. Hydrogen diffusivity and tensile-ductility loss of solution-treated austenitic stainless steels with external and internal hydrogen10.1016/j.ijhydene.2017.04.055 ↗
23. Comprehensive understanding of ductility loss mechanisms in various steels with external and internal hydrogen10.1007/s11661-017-4323-3 ↗
24. Elucidating the variables affecting accelerated fatigue crack growth of steels in hydrogen gas with low oxygen concentrations10.1016/j.actamat.2013.07.001 ↗
25. Hydrogen accelerated fatigue crack growth of friction stir welded X52 steel pipe10.1016/j.ijhydene.2016.10.153 ↗
26. Hydrogen trapping and fatigue crack growth property of low-carbon steel in hydrogen-gas environment10.1016/j.ijfatigue.2017.04.010 ↗
27. Hydrogen-affected fatigue crack propagation at various loading frequencies and gaseous hydrogen pressures in commercially pure iron10.1016/j.ijfatigue.2018.12.009 ↗
28. Assessment of resistance to fatigue crack growth of natural gas line pipe steels carrying gas mixed with hydrogen10.1016/j.ijhydene.2019.02.216 ↗
29. Hydrogen enhanced fatigue crack growth rates in a ferritic Fe-3 wt% Si alloy and an X70 pipeline steel10.1016/j.engfracmech.2019.106641 ↗
30. H. Kobayashi, T. Yamada, H. Kobayashi, S. Matsuoka, Criteria for selecting materials to be used for hydrogen refueling station equipment, ASME PVP2016-64033, 2016.10.1115/PVP2016-64033 ↗
31. Determination of hydrogen compatibility for solution-treated austenitic stainless steels based on a newly proposed nickel-equivalent equation10.1016/j.ijhydene.2016.06.193 ↗
32. J. Nakamura, T. Omura, Y. Tomio, H. Hirata, M. Terunuma, E. Dan, T. Osuki, Mechanical properties of high nitrogen – high strength stainless steels in high pressure gaseous hydrogen environment, ASME PVP2013-97365, 2013, doi:10.1115/PVP2013-97365.10.1115/PVP2013-97365 ↗
33. Mechanical properties and room-temperature creep deformation of hydrogen-charged low-Mo austenitic stainless steels for high-pressure hydrogen use10.2320/jinstmet.JC201403 ↗
34. Development of methods for evaluating hydrogen compatibility and suitability10.1016/j.ijhydene.2014.03.234 ↗
35. C. San Marchi, J. Yamabe, M. Schwarz, H. Matsunaga, S. Zickler, S. Matsuoka, H. Kobayashi, Global harmonization of fatigue life testing in gaseous hydrogen, ASME PVP2018-84898, 2018, doi: 10.1115/PVP2018-84898.10.1115/PVP2018-84898 ↗
36. Slow strain rate tensile and fatigue properties of Cr–Mo and carbon steels in a 115 MPa hydrogen gas atmosphere10.1016/j.ijhydene.2015.02.098 ↗
37. Test method to establish hydrogen compatibility of materials in high pressure hydrogen gas environments for fuel cell vehicles10.2355/isijinternational.ISIJINT-2020-358 ↗
38. Qualification of chromium–molybdenum steel based on the safety factor multiplier method in CHMC1-201410.1016/j.ijhydene.2014.10.114 ↗
39. Pressure cycle testing of Cr-Mo steel pressure vessels subjected to gaseous hydrogen
40. High-strength copper-based alloy with excellent resistance to hydrogen embrittlement10.1016/j.ijhydene.2016.05.156 ↗
41. Material performance of age-hardened beryllium-copper alloy, CDA-C17200, in a high-pressure, gaseous hydrogen environment10.1016/j.ijhydene.2017.04.270 ↗
42. Influence of high-pressure hydrogen on the tensile and fatigue properties of a high-strength Cu-Al-Ni-Fe alloy10.1016/j.ijhydene.2010.07.093 ↗
43. Effect of hydrogen charging on the mechanical properties of high-strength copper-base alloys, austenitic stainless steel AISI 321, inconel 625 and ferritic steel 1.4511
44. Determination of hydrogen compatibility for Cu-Al-Ni-Fe-Mn cast alloys prepared by varying Al and Ni contents
45. Effect of casting defect on the tensile strength of aluminum die casting materials10.1299/kikaia.68.567 ↗
46. Reclassification of spheroidal graphite ductile cast irons grades according to design needs10.1007/s40962-020-00454-x ↗
47. Analysis of ductile cast iron tensile tests to relate ductility variation to casting defects and material microstructure10.1016/j.msea.2008.09.082 ↗
48. The effects of defects on tensile properties of cast ADC12 aluminum alloy10.1007/s11661-015-3134-7 ↗
49. The fatal defects in cast Al-Si alloys due to Sn addition
50. Specific application method for determining the strength and fracture toughness of metal materials10.1016/j.tafmec.2023.103822 ↗
51. Comparative study of hydrogen-induced intergranular fracture behavior in Ni and Cu–Ni alloy at ambient and cryogenic temperatures
52. Murakami · 2019
53. The penny-shaped crack and the plane strain crack in an infinite body of power-law material10.1115/1.3157742 ↗
54. Fully plastic solutions and large scale yielding estimates for plate stress crack problem10.1115/1.3443380 ↗
55. The fracture toughness of a nickel-aluminum bronze10.1007/BF00566247 ↗
56. Microstructure, mechanical properties, and brittle fracture of a cast nickel-aluminum-bronze (NAB) UNS C9580010.1016/j.engfailanal.2021.105606 ↗
57. Ohji · 2006
58. Effects of hydrogen and casting defects on the fatigue behavior of Cu-Al-Ni-Fe-Mn cast alloy