journal article·2026-07

Failure analysis of cracking of 316L Medium-Pressure superheated steam Piping in a natural gas purification plant

Zhiming Yu, Shaomu Wen, Rui Fan, Ganghua Huang, Hongfa Huang, Jin Yan

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Mechanical Failure Analysis and Simulation · High Temperature Alloys and Creep · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. The research progress and prospect of data mining methods on corrosion prediction of oil and gas pipelines10.1016/j.engfailanal.2022.106951 ↗
2. Key technologies for corrosion control in high-sulfur gas field: Review and prospect
3. Corrosion control and monitoring/detection of natural gas purification plant in sour gas field
4. Discussion on energy saving technology of steam and condensate system in natural gas purification plant
5. Selection and Analysis of Material for Boiler Pipes in a Steam Plant10.1016/j.proeng.2016.06.659 ↗
6. Change in the Structural and Mechanical State of Heat-Resistant 15CrMoV5-10 Steel of TPP Steam Pipelines under the Influence of Operational Factors10.3390/ma18143421 ↗
7. Research trends on stress corrosion cracking (SCC) in 316L stainless steel: a bibliometric review
8. Failure analysis on abnormal leakage of TP321 stainless steel pipe in hydrogen-eliminated system of nuclear power plant10.1016/j.engfailanal.2018.02.021 ↗
9. Effect of Long-Term Pre-oxidation on the Corrosion Rate of 316L Stainless Steel in a High-Temperature Water Environment10.1007/s11665-022-06878-2 ↗
10. Adaptation of the point defect model to simulate oxidation kinetics of 316L stainless steel in the pressurised water reactor environment10.1016/j.corsci.2021.109454 ↗
11. The stress corrosion cracking of type 316 stainless steel in oxygenated and chlorinated high temperature water10.1016/0010-938X(85)90010-1 ↗
12. Numerical modeling of stress corrosion cracking in steel structures with phase field method10.1016/j.engfailanal.2023.107921 ↗
13. Is duplex stainless steel more corrosion resistant than 316L in aqueous acid chloride-containing environments at temperatures higher than 100℃10.1080/1478422X.2018.1507335 ↗
14. Effects of temperature and pressure on stress corrosion cracking behavior of 310S stainless steel in chloride solution10.3901/CJME.2016.0420.056 ↗
15. Failure Analysis of 316 Stainless Steel Corrosion Fatigue Test Fixture10.1007/s11668-025-02115-9 ↗
16. Investigation of intergranular stress corrosion cracking in a failed 347H stainless steel furnace tube10.1016/j.engfailanal.2022.106835 ↗
17. Intergranular stress corrosion cracking in simulated BWR water of 316L stainless steels manufactured with different procedures10.1016/j.corsci.2021.109344 ↗
18. Effect of temperature on the electrochemical pitting corrosion behavior of 316L stainless steel in chloride-containing MDEA solution10.1016/j.jngse.2020.103718 ↗
19. Multi-phase-field modeling of localized corrosion involving galvanic pitting and mechano-electrochemical coupling10.1016/j.corsci.2020.108900 ↗
20. Effects of chloride and oxygen on stress corrosion cracking of cold worked 316/316L austenitic stainless steel in high temperature water10.1016/j.corsci.2016.04.035 ↗
21. Role of dissolved oxygen on the corrosion behavior of 316L stainless steel10.1016/j.matdes.2025.115017 ↗
22. Failure analysis of 316L stainless steel bellows serving in steam tube10.1016/j.ijpvp.2022.104718 ↗
23. Corrosion crack failure analysis of 316L hydraulic control pipeline in high temperature aerobic steam environment of heavy oil thermal recovery well10.1016/j.engfailanal.2022.106297 ↗
24. Failure investigation of an AISI 316L pipe of the flare system in an off-shore oil platform10.1016/j.engfailanal.2024.108939 ↗
25. Stress corrosion cracking failure of a SS 316L high pressure heater tube10.1016/j.engfailanal.2018.03.013 ↗
26. Failure Analysis of 316L Stainless Steel Dechlorination System Tube: a Case Study of Chloride-Induced stress Corrosion Cracking10.1007/s11668-025-02251-2 ↗
27. Failure analysis of stress corrosion cracking of 316L stainless steel bend pipe in the atmospheric tower10.1016/j.engfailanal.2025.109519 ↗
28. Failure analysis of austenitic stainless steel pipes in amine liquid regeneration unit of a desulfurizer10.1016/j.engfailanal.2015.07.028 ↗
29. Corrosion of 316L stainless steel in high temperature water and steam: Mechanisms of corrosion10.1016/j.jnucmat.2024.155180 ↗
30. Degradation of the protective layer on stainless steel by chlorine variation under high-temperature conditions
31. Localized corrosion and stress corrosion cracking of stainless steels in halides other than chlorides solutions: a review10.1515/corrrev-2019-0061 ↗
32. Effects of temperature and pressure on stress corrosion cracking behavior of 310S stainless steel in chloride solution10.3901/CJME.2016.0420.056 ↗
33. EPRI, PWR Secondary Water Chemistry Guidelines, Revision 7, Report 3002000505, Electric Power Research Institute, Palo Alto, CA, 2013.
34. GB/T 20801.1 [S], Pressure piping code-Part 1: Industrial piping (2025).
35. Fracture toughness of type 316LN stainless steel welded joints10.1016/j.msea.2016.12.128 ↗
36. Metallurgical failure investigation of small bore piping (SBP) in a diesel hydrotreating unit (DHT) of an oil refinery10.1515/pm-2024-0046 ↗
37. Probing intergranular mixed transgranular stress corrosion cracking under the high constant load10.1038/s41598-022-16390-1 ↗
38. The failure Mechanism of the 316 SS Heat Exchanger Tube in the Geothermal Water Environment10.3390/ma15228103 ↗
39. Analysis
40. Integrity Assessment of stress Corrosion Cracking Susceptibility of Duplex UNS S32205 and Austenitic UNS S31653 Stainless Steel Reinforcements10.3390/met13121932 ↗
41. Focused review on factors affecting martensitic stainless steels and super martensitic stainless steel passive film in the oil and gas field10.1007/s10008-024-05984-6 ↗
42. Effect of Organizational Evolution on the stress Corrosion Cracking of the Cr-Co-Ni-Mo Series of Ultra-High Strength Stainless Steel10.3390/ma15020497 ↗
43. Effect of Thermo-Mechanical Processing on Initiation and Propagation of stress Corrosion Cracking in 304L Austenitic Stainless Steel10.3390/met13081458 ↗
44. Microstructural changes in AISI 304L stainless steel due to surface machining: effect on its susceptibility to chloride stress corrosion cracking10.1016/j.jnucmat.2010.05.028 ↗
45. Influence of the machined surface roughness on the pitting behavior of 304 stainless steel10.1002/maco.202213574 ↗
46. Analysis of Oxide Wedging during Environment Assisted Crack Growth10.5006/1.3581914 ↗