Combined effects of phase transformation–induced PFZ and stress corrosion cracking on the failure of an Inconel 625 boiler tube
Source abstract
Abstract
This study investigates the failure mechanism of an Inconel 625 alloy boiler tube that had been in service for approximately 18 months before failure. Numerous through-thickness cracks were observed in the weld heat-affected zone (HAZ). Microstructural analysis revealed that long-term exposure at elevated temperature induced phase transformations, which in turn altered the microstructure. Fine γ″ and Ni 2 (Cr,Mo) precipitates formed within the matrix and contributed to matrix strengthening, whereas a large number of Cr-rich carbides were observed along the grain boundaries. These boundary precipitates produced precipitation-free zones adjacent to the grain boundaries and created conditions similar to those associated with stress relaxation cracking. In addition, chloride was detected in the corrosion oxides present along both the main cracks and secondary branch cracks. The results indicate a failure mechanism in which precipitation-free zones formation caused by phase transformation acts in combination with stress corrosion cracking.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Special Metals Corporation, INCONEL alloy 625, Technical Bulletin, https://www.specialmetals.com/documents/technical-bulletins/inconel/inconel-alloy-625.pdf (accessed 2026-03-09).
2. S. Floreen, G.E. Fuchs, W.J. Yang, The metallurgy of alloy 625, in: E.A. Loria (Ed.), Superalloys 718, 625, 706 and Various Derivatives, The Minerals, Metals & Materials Society, 1994, pp. 13–37. DOI: 10.7449/1994/Superalloys_1994_13_37.10.7449/1994/Superalloys_1994_13_37 ↗
3. Studies on the oxidation behavior of Inconel 625 between 873 and 1523 K10.1007/BF01046827 ↗
4. Sub-scale depletion and enrichment processes during high temperature oxidation of the nickel base alloy 625 in the temperature range 900–1000 °C10.1007/s11085-010-9225-3 ↗
5. Microstructural evolution of Inconel 625 alloy exposed to isothermal oxidation in air at 800–1000 °C
6. M. Köhler, Effect of the elevated-temperature precipitation in alloy 625 on properties and microstructure, in: E.A. Loria (Ed.), Superalloys 718, 625 and Various Derivatives, The Minerals, Metals & Materials Society, 1991, pp. 363–374. DOI: 10.7449/1991/Superalloys_1991_363_374.10.7449/1991/Superalloys_1991_363_374 ↗
7. Precipitation of an intermetallic phase with Pt2Mo-type structure in alloy 62510.1007/s11661-999-0194-6 ↗
8. Precipitation behavior of Ni-based superalloy alloy 625 for A-USC power plants10.2355/isijinternational.ISIJINT-2022-169 ↗
9. Sensitization of as rolled and stable annealed alloy 62510.1007/s00501-013-0225-x ↗
10. M. Köhler, U. Heubner, Time-temperature-sensitization and time-temperature-precipitation behavior of alloy 625 (UNS N06625), in: CORROSION/96, Paper No. NACE-96427, NACE International, 1996.10.5006/C1996-96427 ↗
11. F. Cortial, J.-M. Corrieu, C. Vernot-Loier, Heat treatments of weld alloy 625: influence on the microstructure, mechanical properties and corrosion resistance, in: E.A. Loria (Ed.), Superalloys 718, 625, 706 and Various Derivatives, The Minerals, Metals & Materials Society, 1994, pp. 859–870. DOI: 10.7449/1994/Superalloys_1994_859_870.10.7449/1994/Superalloys_1994_859_870 ↗
12. Effect of precipitation on post-heat-treated Inconel 625 alloy after friction stir welding10.1016/j.matdes.2009.12.020 ↗
13. Stress relaxation cracking susceptibility evaluation in 347H stainless steel welds10.1007/s40194-024-01678-9 ↗
14. Stress relaxation cracking in 347H stainless steel arc welds: susceptibility evaluation of heat-affected zone10.3390/met14050494 ↗
15. Corrosion of alloy 625 in aqueous solutions containing chloride and oxygen10.5006/1.3284802 ↗
16. Stress corrosion cracking of alloy 625 in pH 2 aqueous solution at high temperature and pressure10.5006/1.3560116 ↗
17. C. Wu, V. de Andrade, Z. Liu, W. Zhao, A. Lewis, A.L. Marie, C. Wang, A. Davydov, A. Telang, A. Yawny, C. Korte, In situ monitoring of stress corrosion at the alloy 625|NaCl interface, Surface Science and Technology 2 (2024) Article 3. DOI: 10.1007/s44251-024-00034-9.10.1007/s44251-024-00034-9 ↗
18. J. Dong, Z. Bi, N. Wang, X. Xie, Z. Wang, Structure control of a new-type high-Cr superalloy, in: Superalloys 2008, The Minerals, Metals & Materials Society, 2008, pp. 41–50. DOI: 10.7449/2008/Superalloys_2008_41_50.10.7449/2008/Superalloys_2008_41_50 ↗
19. Effect of prior plastic deformation on the α-Cr precipitation in a binary Ni–Cr alloy10.1007/s11661-020-06026-2 ↗
20. MetalTek International, Alloy Grade UNS: 50Cr–50Ni–Cb (50/50Nb) – Nickel Based Alloy (UNS R20501), https://www.metaltek.com/alloy/specialty-alloys-heat-resistant-stainless-steel-mtek-50-50nb/ (accessed 2026-03-09).
21. Precipitation of sigma phase in duplex stainless steel and recent development on its detection by electrochemical potentiokinetic reactivation: a review10.1016/j.corcom.2021.08.001 ↗
22. Sigma-phase in duplex-stainless steels10.1515/ijmr-2004-0120 ↗
23. A recent review on the failure analysis of boiler tube10.21776/jrm.v15i2.1392 ↗
24. A review of underlying reasons for intergranular cracking for a variety of failure scenarios