journal article·2026-09

Failure analysis of multi-stage cold-drawn electrode wire rods: Role of deformation-induced martensite

K.K Rakesha, Sujata Panda, H.K. Mehtani, D.Satish Kumar

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Mechanical Failure Analysis and Simulation · Mechanical stress and fatigue analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Wear of laying head pipes in a wire rod mill10.1007/s11668-013-9701-6 ↗
2. American Welding Society. AWS A5.18/A5.18M: Specification for Carbon Steel Electrodes and Rods for Gas Shielded Arc Welding. 8th ed. Miami (FL): American Welding Society; 2021.
3. Metallurgical investigation of welding wire rod grade during processing10.1016/j.engfailanal.2020.104884 ↗
4. Metallurgical investigation of wire breakage of tyre bead grade10.1016/j.csefa.2015.09.003 ↗
5. Analysis of causes of defects appearance in wire drawing10.4028/www.scientific.net/DDF.405.217 ↗
6. W.T. Becker, R.J. Shipley. Failure Analysis and Prevention. ASM Handbook, Materials Park (OH): ASM International; 11, 2002. Doi: 10.31399/asm.hb.v11.9781627081801.10.31399/asm.hb.v11.9781627081801 ↗
7. Failures during the production and usage of steel wires10.1016/j.jmatprotec.2005.07.007 ↗
8. Influence of flaws of wire rod surface, inclusions and voids on wire breaks in superfine wire drawing10.1299/jsmea.46.365 ↗
9. Reasons for breakage of welding rod and wire10.4028/www.scientific.net/MSF.946.247 ↗
10. Cause analysis of V-shaped crack pairs on drawn welding wire surface of ER70S-6 steel10.1051/metal/2022070 ↗
11. Deformation-induced martensite: a new paradigm for exceptional steels10.1002/adma.201601526 ↗
12. Atomic-scale mechanisms of deformation-induced cementite decomposition in pearlite10.1016/j.actamat.2011.03.022 ↗
13. Improved etching technique for the determination of percent martensite in high-strength dual-phase steels10.1016/0026-0800(79)90041-7 ↗
14. M.J. Santofimia Navarro, C. Kwakernaak, W.G. Sloof, L. Zhao, J. Sietsma. Experimental study of the distribution of alloying elements after the formation of epitaxial ferrite upon cooling in a low-carbon steel. Mater Charact. 61(2010) 937–942. Doi: 10.1016/j.matchar.2010.06.006.10.1016/j.matchar.2010.06.006 ↗
15. Quantitative measurement of cementite dissociation in drawn pearlitic steel10.1016/j.msea.2011.03.051 ↗
16. Microstructure evolution in pearlitic steels during wire drawing10.1016/S1359-6454(02)00281-1 ↗
17. Temperature rise in wire drawing
18. S. van der Zwaag. Kinetics of phase transformations in steels. In: D. V. Edmonds, E. Pereloma, editors. Phase transformations in steels, volume 1: fundamentals and diffusion controlled transformations. Woodhead Publishing; 2012. p. 126–152. Doi: 10.1533/9780857096104.1.126.10.1533/9780857096104.1.126 ↗
19. I. Alanis-Fuerte, P. Garnica, E. López Martínez, H. J. Vergara Hernández. Effect of cold-rolling and heating rate on austenite formation in a low–carbon steel. ISIJ Int. 62(2022) 227–236. Doi: 10.2355/isijinternational.ISIJINT-2021-294.10.2355/isijinternational.ISIJINT-2021-294 ↗
20. Static strain aging of eutectoid carbon steel wires10.2355/isijinternational1966.16.417 ↗
21. The strain induced cementite dissolution in carbon steel — experimental facts and theoretical approach10.4028/www.scientific.net/SSP.94.45 ↗
22. A. Phelippeau, S. Pommier, I. Zakharchenko, R. Levy-Tubiana, T. Tsakalakos, M. Clavel, M. Croft, Z. Zhong, C. Prioul. Cold drawn steel wires—processing, residual stresses and ductility. Part II: Synchrotron and neutron diffraction. Fatigue Fract Eng Mater Struct. 29(2006) 255–265. Doi: 10.1111/j.1460-2695.2005.00987.x.10.1111/j.1460-2695.2005.00987.x ↗
23. Decomposition of cementite in pearlitic steel due to plastic deformation10.1016/S0921-5093(02)00358-1 ↗
24. Cementite decomposition in heavily drawn pearlite steel wire10.1016/S1359-6462(00)00690-4 ↗
25. Segregation stabilizes nanocrystalline bulk steel with near theoretical strength10.1103/PhysRevLett.113.106104 ↗
26. Nanostructuring and dissolution of cementite in pearlitic steels during severe plastic deformation
27. The role of phase hardness differential on the non-uniform elongation of a ferrite-martensite dual phase steel10.1007/s11661-021-06361-y ↗
28. Microvoid formation of ferrite-martensite dual-phase steel via tensile deformation after severe plastic shear-deformation10.2355/isijinternational.ISIJINT-2023-012 ↗
29. Schwartz AJ, Kumar M, Adams BL, Field DP, editors. Electron backscatter diffraction in materials science. 2nd ed. New York: Springer; 2009.10.1007/978-0-387-88136-2 ↗
30. Influence of degree of cold-drawing on the mechanical properties of low carbon steel
32. Crack initiation during wire drawing of low carbon, manganese steel wire rods containing ferrite, pearlite, and martensite10.1179/mst.1994.10.11.971 ↗
33. The effect of martensite particle size on tensile fracture of surface-carburised AISI 8620 steel with dual-phase core microstructure10.1016/S0261-3069(02)00065-1 ↗